Abstract A TiN/MT-TiCN/α-Al2O3/TiN coating is deposited on a WC–6Co hardmetal substrate by chemical vapor deposition (CVD). The influence of the post-treatments after the CVD process on the performances of the inserts in the tuning of grey cast iron EN-GJL-250 and the related characteristics are investigated. Conventional brushing, polishing and wet-blasting are employed for the comparison. The results demonstrate that the coated inserts post-treated by wet-blasting followed by polishing exhibit in a cost effective way the lowest surface roughness, the best combination of cooling micro-crack healing effect and surface finish state, a moderate compressive stress state, and > 100 N adhesion strength. As a result, in the wet cutting condition, the lowest roughness and the smallest work hardening value of the workpieces compared at a fixed time parameter in their middle-later cutting lifetime and the longest tool life are attained. Crater wear developed from adhesive wear is the main reason for the tool failure. The same tool life conclusion is reached in the dry cutting condition.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. The history of hard CVD coatings for tool applications at the University of Technology Vienna10.1016/j.ijrmhm.2013.01.012 ↗
2. Evolution of conventional hard coatings for its use on cutting tools10.1016/j.ijrmhm.2016.05.009 ↗
3. Nanostructured coatings for tooling applications10.1016/j.ijrmhm.2016.06.017 ↗
4. The history of the technological progress of hardmetals10.1016/j.ijrmhm.2014.04.016 ↗
5. Tribological properties of Al2O3 hard coatings modified by mechanical blasting and polishing post-treatment10.1016/j.wear.2012.04.022 ↗
6. Investigation of cemented carbides with alternative binders after CVD coating10.1016/j.ijrmhm.2016.07.005 ↗
7. Oxidation resistance and thermal stability of Ti(C,N) and Ti(C,N,O) coatings deposited by chemical vapor deposition10.1016/j.ijrmhm.2015.08.006 ↗
8. Investigation of the origin of compressive residual stress in CVD TiB2 hard coatings using synchrotron X-ray nanodiffraction10.1016/j.surfcoat.2014.09.050 ↗
9. In-situ high temperature stress analysis of Ti(C,N) coatings on functionally graded cemented carbides by energy dispersive synchrotron X-ray diffraction10.1016/j.ijrmhm.2015.12.001 ↗
10. Micro-blasting effect on fracture resistance of PVD-AlTiN coated cemented carbide cutting tools10.1016/j.surfcoat.2016.07.094 ↗
11. Influence of different post-treatments on tungsten carbide-cobalt inserts10.1016/j.matlet.2008.07.043 ↗
12. Shot peening of brittle materials-status and outlook10.4028/www.scientific.net/MSF.638-642.799 ↗
13. Improvement of PVD coated inserts cutting performance, through appropriate mechanical treatments of substrate and coating surface10.1016/S0257-8972(01)01485-2 ↗
14. Micro shot blasting of machine tools for improving surface finish and reducing cutting forces in manufacturing10.1016/j.matdes.2004.02.013 ↗
15. Effect of PVD films wet micro-blasting by various Al2O3 grain sizes on the wear behaviour of coated tools10.1016/j.surfcoat.2011.03.046 ↗
16. Residual stress gradients in α-Al2O3 hard coatings determined by pencil-beam X-ray nanodiffraction: the influence of blasting media10.1016/j.surfcoat.2014.12.028 ↗
17. Influence of micro-blasting on the microstructure and residual stresses of CVD κ-Al2O3 coatings10.1016/j.surfcoat.2009.06.021 ↗
18. Evolutional history of coating technologies for cemented carbide inserts-chemical vapor deposition and physical vapor deposition
19. Application of the whole powder pattern decomposition procedure in the residual stress analysis of layers and coatings10.1016/j.tsf.2015.05.071 ↗
20. Evaluating mechanical properties and crack resistance of CrN, CrTiN, CrAlN and CrTiAlN coatings by nanoindentation and scratch tests10.1016/j.surfcoat.2015.11.040 ↗
21. Dry-blasting of α- and κ-Al2O3 CVD hard coatings: friction behavior and thermal stress relaxation10.1007/s11249-013-0201-3 ↗
22. The evaluation of the measured adhesion strength of biocompatible thin films by fuzzy logic expert system and international standards
23. Substrate surface finish effects on scratch resistance and failure mechanisms of TiN-coated hardmetals10.1016/j.surfcoat.2015.01.038 ↗
24. Fine platelet-like grained WC–Co cemented carbides: preparation, characterization, properties and application in PVD coating substrates10.1016/j.ijrmhm.2017.01.015 ↗
25. Wear and tool life of tungsten carbide, PCBN and PCD cutting tools10.1016/j.ijmachtools.2005.07.015 ↗
26. Progress in high temperature nanomechanical testing of coatings for optimizing their performance in high speed machining10.1016/j.surfcoat.2014.02.062 ↗
27. Evaluation of machinability by cutting environments in high-speed milling of difficult-to-cut materials10.1016/S0924-0136(01)00529-5 ↗
28. Wear performance of laser precoating treated cemented carbide milling tools10.1016/j.wear.2010.02.009 ↗
29. Wear model in turning of hardened steel with PCBN tool10.1016/j.ijrmhm.2014.06.019 ↗
30. Cutting performance and wear characteristics of Ti(C,N)-based cermet tool in machining hardened steel10.1016/j.ijrmhm.2015.06.006 ↗
31. Cutting temperature effect on PCBN and CVD coated carbide tools in hard turning of D2 tool steel10.1016/j.ijrmhm.2014.11.001 ↗
32. Influence of laser substrate pretreatment on anti-adhesive wear properties of WC/Co-based TiAlN coatings against AISI 316 stainless steel10.1016/j.ijrmhm.2016.03.004 ↗
33. Effect of machining parameters on surface integrity in high speed milling of super alloy GH 4169/Inconel 71810.1080/10426914.2014.994769 ↗
34. Microhardness and surface integrity in turning process of duplex stainless steel (DSS) for different cutting conditions10.1007/s11665-013-0832-4 ↗
35. Influence of chemical composition and microstructure of gray cast iron on wear of heavy duty diesel engines cylinder liners10.1016/j.wear.2007.01.091 ↗
36. Hybrid learning for tool wear monitoring10.1007/s001700050161 ↗
37. Initial tool wear behavior during machining of titanium metal matrix composite (TiMMCS)10.1016/j.ijrmhm.2016.07.021 ↗
38. Fatigue failure of coated carbide tool and its influence on cutting performance in face milling SKD11 hardened steel10.1016/j.ijrmhm.2017.01.001 ↗