This study examines the three-body abrasive-wear performance of WC/Fe surface composites subjected to different matrices, including high‑chromium cast iron (HCCI) and cast steel. These findings indicate that a composite zone can be formed between the matrix and WC preforms, accompanied by a substantial precipitation of carbides. A well-bonded semi-coherent interface forms between Fe 6W 6C and Fe, and the orientation relationship of Fe (110)BCC//Fe 6W 6C(111) FCC is the N W (Nishiyama Wassermann) orientation relationship. The partial density of states indicates that the highest average layout number of W W bonds at the interface is 0.53, which corresponds to the highest bonding strength at an average bond length of 2.83 Å. Compared with high‑manganese steel (HMS) and high‑carbon steel (HCS) specimens, the HCCI specimen exhibits the lowest weight loss of 0.075 g. Furthermore, its surface roughness is low (3.337 μm), and its wear resistance is 24.09 % and 15.59 % greater than those of the HMS and HCS specimens, respectively.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Processing and properties of particulate reinforced steel matrix composites10.1016/S0921-5093(97)00710-7 ↗
2. W–Cu composites with excellent comprehensive properties10.1016/j.compositesb.2022.109664 ↗
3. Cemented carbide phase diagrams: a review10.1016/j.ijrmhm.2011.02.004 ↗
4. Mechanical properties of WC-based hardmetals bonded with iron alloys - a review10.1080/02670836.2016.1186929 ↗
5. WC-Fe metal-matrix composite coatings fabricated by laser wire cladding10.1016/j.jmatprotec.2021.117438 ↗
6. Synthesis, microstructure, and mechanical properties of WC–TiC–Co ceramic composites10.1016/j.jeurceramsoc.2011.06.013 ↗
7. Three-body abrasive wear behavior of CC/high-Cr WCI composite and its interfacial characteristics10.1016/j.wear.2009.09.001 ↗
8. Abrasive wear resistance of WC-based composites, produced with Co or Ni-rich binders10.1016/j.wear.2021.203924 ↗
9. Preparation and microstructural characterization of a high-Cr white cast iron reinforced with WC particles10.3390/ma13112596 ↗
10. Effects of WC particles on microstructure and mechanical properties of 316L steel obtained by laser melting deposition10.1016/j.ceramint.2022.03.324 ↗
11. Impact wear resistance of WC/Hadfield steel composite and its interfacial characteristics10.1016/j.wear.2005.04.010 ↗
12. Microstructure and abrasive wear study of (Ti,W)C-reinforced high-manganese austenitic steel matrix composite10.1016/j.matlet.2008.05.049 ↗
13. Effect of tungsten on microstructure and properties of high chromium cast iron10.1016/j.matdes.2012.02.048 ↗
14. Characterization of iron-matrix composites reinforced by in situ TiC and ex situ WC fabricated by casting10.3390/met11060862 ↗
15. A study on a cast steel reinforced with WC–metal matrix composite10.3390/ma15186199 ↗
16. Interface structure and wear behavior of Cr26 ferrous matrix surface composites reinforced with CTCP10.1007/s11249-014-0303-6 ↗
17. Interfacial bonding and abrasive wear behaviours of the iron matrix composites10.1080/02670836.2022.2068244 ↗
18. Effects of Ni60WC25 powder content on the microstructure and wear properties of WCp reinforced surface metal matrix composites10.1007/s12666-018-1372-2 ↗
19. Wear performance of Ni-WC composites and heat-damage behaviour of WC particle during vacuum-induction melting process10.1016/j.wear.2024.205294 ↗
20. Electronic structure, anisotropic elastic and thermal properties of the η phase Fe 6 W 6 C10.1016/j.commatsci.2015.06.037 ↗
21. Investigation on WC/TiC interface relationship in wear-resistant coating by first-principles10.1016/j.surfcoat.2016.08.025 ↗
22. Adhesion at cerium doped metal-ceramic α-Fe/WC interface: a first-principles calculation10.1016/j.jre.2018.11.009 ↗
23. Microstructure and abrasive wear properties of WC/Fe matrix composites under different preform wall thicknesses
24. First-principles simulation : ideas, illustrations and the CASTEP code10.1088/0953-8984/14/11/301 ↗
25. Relaxation of crystals with the quasi-Newton method10.1006/jcph.1996.5612 ↗
26. Core-rim microstructure and properties of WC/Ni composites10.1016/j.ijrmhm.2018.09.007 ↗
27. Microstructure and wear of Ni-WC hardfacing used for steel-body PDC bits10.1016/j.ijrmhm.2021.105683 ↗
28. Interface structure and wear behavior of Cr26 ferrous matrix surface composites reinforced with CTCP10.1007/s11249-014-0303-6 ↗
29. Effect of WC mass fraction on the microstructure and frictional wear properties of WC/Fe matrix composites10.1016/j.ijrmhm.2023.106265 ↗
30. Deformation behaviors and cyclic strength assessment of AZ31B magnesium alloy based on steady ratcheting effect10.1016/j.msea.2018.03.023 ↗
31. Microstructural and wear properties of WC-12Co cemented carbide fabricated by direct energy deposition10.1016/j.wear.2023.204653 ↗
32. Characterization of iron-based surface multilayer-structured tungsten carbide composite layers by EBSD and FIB/TEM10.1016/j.surfcoat.2020.126365 ↗
33. Effect of isothermal temperature on growth behavior of nanostructured bainite in laser cladded coatings10.3390/ma10070800 ↗
34. A novel iron matrix composite fabricated by two-step in situ reaction: microstructure, formation mechanism and mechanical properties10.1016/j.jallcom.2020.157442 ↗
35. Evolution of microstructure and mechanical properties of aluminum matrix composites reinforced with dual-phase heterostructures10.1016/j.msea.2024.146500 ↗
36. Interfacial structure of WC-Fe metal-matrix composite (WC/Fe3W3C and Fe/Fe3W3C) stability, electronic and mechanical properties from first-principles calculations
37. Interface microstructure and abrasive wear properties of WC-iron matrix composites with Ni, Mo, Fe added to the preforms10.1016/j.jmrt.2023.04.007 ↗
38. Interfacial characterization and erosive wear performance of zirconia toughened alumina ceramics particles reinforced high chromium white cast irons composites10.1016/j.triboint.2021.107262 ↗
39. Three-body dry abrasive wear properties of 15–5 precipitation hardening stainless steel produced by laser powder bed fusion process
40. Two-body and three-body abrasion: a critical discussion10.1016/S0043-1648(97)00188-9 ↗
41. Effects of chromium additions on the three-body abrasive wear behavior of Fe-3.0 wt% B alloy10.1016/j.wear.2017.02.042 ↗