Abstract
Abstract Crack-free pure W bulks have been fabricated by SHS assisted hot-shock consolidation (HSC). The tungsten powders were preheated by the heat released through a SHS (self-propagating high-temperature synthesis) reaction before shock wave loading. The duration of preheating was less than 3 min and the preheating temperature was controlled in the range of 700 ~ 1300 °C by adjusting the mass of the SHS mixture. The highest relative density of compacted samples can reach 96.7% T.D. (theoretical density) at 1300 °C under the shock pressure of 3.14GPa. The grain sizes of all compacted samples are nearly the same as the initial powder size of 2 μm. The hardness and modulus of the consolidated pure W bulks were measured using nanoindentation test; and the microstructure was investigated using light microscopy (LM) and scanning electron microscopy (SEM). It is found that the shock pressure plays a more important role than preheating temperature, after the pressure exceeding the crush strength of tungsten powder during the sintering process. At the preheating temperature of 1300 °C, the increase in shock pressure leads to obvious surface melting. For HSC of pure tungsten, the void collapse and surface melting are the main sintering mechanisms. The former one contributes to the densification behavior of powders, and the later one is responsible for the inter-particle bonding; and both of which are dominated by the shock pressure. The advantage of preheating for eliminating the cracks is also demonstrated by the experimental results.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Smith · 1993 · 580
2. Grain size engineering of bcc refractory metals: top-down and bottom-up - application to tungsten10.1016/j.msea.2007.02.099 ↗
3. Development of tungsten armor and bonding to copper for plasma-interactive components10.1016/S0022-3115(98)00358-4 ↗
4. Performance of plasma-facing materials under intense thermal loads in tokamaks and stellarators10.13182/FST04-A550 ↗
5. Annealing behaviour and transient high-heat loading performance of different grade fine-grained tungsten10.1088/0031-8949/2011/T145/014055 ↗
6. Mechanical behavior and dynamic failure of high-strength ultrafine grained tungsten under uniaxial compression
7. Microstructure and mechanical properties of super-strong nanocrystalline tungsten processed by high-pressure torsion10.1016/j.actamat.2006.05.005 ↗
8. Nanoengineering opens a new era for tungsten as well10.1007/s11837-006-0081-1 ↗
9. Microwave Sintering: A New Approach to Fine-grain Tungsten-I
10. Fabrication of high temperature oxides dispersion strengthened tungsten composites by spark plasma sintering process10.1016/j.ijrmhm.2009.03.003 ↗
11. The modeling of electric-current-assisted sintering to produce bulk nanocrystalline tungsten10.1007/s11837-006-0218-2 ↗
12. Fabrication and Characterization of ultra-fine grained tungsten by resistance sintering under ultra-high pressure10.1016/j.msea.2008.11.012 ↗
13. Energy deposition and microstructural modification in dynamically consolidated metal powders10.1063/1.332860 ↗
14. Dynamic compaction of aluminum nanocrystals10.1016/1359-6454(96)83816-X ↗
15. Behavior of explosive compacted/consolidated of nanometric copper powders10.1016/j.jallcom.2008.08.120 ↗
16. Fabrication of bulk nanostructured silver material from nanopowders using shockwave consolidation technique10.1016/j.msea.2007.10.008 ↗
17. Explosive compaction and low-temperature sintering of alumina nanopowders10.1007/s10573-008-0108-8 ↗
18. Dynamic consolidation of W-Cu nanocomposites from W-CuO powder mixture10.1016/j.msea.2010.05.077 ↗
19. Prummer · 2006 · 48
20. Hot explosive consolidation of W–Ti alloys10.1007/BF02671254 ↗
21. Shock synthesis and densification of tungsten based heavy alloys10.1016/j.jmatprotec.2004.07.060 ↗
22. Development of high-temperature shock compression system for consolidating powders by the use of underwater shock-wave assembly10.1016/S0921-4526(97)00368-2 ↗
23. An improved high-temperature shock compression and recovery system using underwater shock wave for dynamic compaction of powders10.1016/S0924-0136(98)00281-7 ↗
24. High temperature shock consolidation of hard ceramic powders10.1016/S0921-4526(97)00364-5 ↗
25. High-temperature shock consolidation of diamond powders using converging underwater shock wave10.1016/S1359-6462(98)00311-X ↗
26. Optimization of the experimental conditions for high-temperature shock consolidation10.1016/S0734-743X(99)00034-2 ↗
27. Shock compression of reactive powder mixtures10.1179/174328009X461050 ↗
28. Dynamic Compression of Porous Tungsten10.1063/1.1658272 ↗
29. Hugoniot evaluation of the preheated metal from its principal Hugoniot10.1063/1.2178388 ↗