Characteristics of tungsten coatings deposited by molten salt electro-deposition and thermal fatigue properties of electrodeposited tungsten coatings
Source abstract
Abstract
Abstract Tungsten coatings were obtained on a tungsten substrate by molten salt electrodeposition (MSE) at 50 mA/cm2 for 60 min in a NaCl-KCl-NaF-WO3 (0.3385:0.3385:0.25:0.0 73mol) melt at 800 °C. The MSE tungsten coatings have rough rectangular pyramid surface and special columnar grains structure. Thermal fatigue tests have shown that the damage factor of MSE tungsten coatings was smaller than that of rolled tungsten under the same thermal loads and MSE tungsten coatings displayed better thermal fatigue properties compared to that of rolled tungsten, which was attributed to high purity, special columnar grains and rectangular pyramid surface morphology.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Recrystallization and composition dependent thermal fatigue response of different tungsten grades10.1016/j.ijrmhm.2017.11.039 ↗
2. Concentration dependent hydrogen diffusion in tungsten10.1016/j.jnucmat.2016.06.044 ↗
3. Transient heat load challenges for plasma-facing materials during long-term operation10.1016/j.nme.2016.12.024 ↗
4. Transient high heat load tests on pure ultra-fine grained tungsten fabricated by resistance sintering under ultra-high pressure10.1016/j.fusengdes.2009.08.003 ↗
5. Physics of ELM power fluxes to plasma facing components and implications for ITER10.1016/j.jnucmat.2009.01.198 ↗
6. Preparation of tungsten coatings on graphite by electro-deposition via Na2WO4-WO3 molten salt system10.1016/j.fusengdes.2014.05.027 ↗
7. Effects of NaPO3 concentration in Na2WO4-WO3 system on pulse electro-deposition tungsten coating from oxide molten slat10.1016/j.jnucmat.2014.07.029 ↗
8. Electrodeposition of tungsten in ZnBr2-NaBr and ZnCl2-NaC1 melts10.1149/1.2085673 ↗
9. ChemInform abstract: electrodeposition of tungsten and related Voltammetric study in a basic ZnCl2-NaCl (40-60 Mol%) melt10.1149/1.1344541 ↗
10. Electrodeposition of metallic tungsten in ZnCl2-NaCl-KCl-WCl4 melt at 250°C10.1149/1.1921130 ↗
11. Electrodeposition of metallic tungsten films in ZnCl2-NaCl-KCl-KF-WO3 melt at 250°C10.1016/j.electacta.2007.04.082 ↗
12. Electrodeposition of tungsten from ZnCl2-NaCl-KCl-KF-WO3 melt and investigation on tungsten species in the melt10.1016/j.electacta.2009.10.021 ↗
13. Study of solubility of WO3 in the NaCl-KCl-NaF-WO3 molten salt10.4028/www.scientific.net/AMR.908.167 ↗
14. Effect of WO3 content on the liquidus temperature of NaCl-KCl-NaF-WO3 molten salt system10.4028/www.scientific.net/AMR.909.54 ↗
15. Electrochemical behavior of tungsten in (NaCl–KCl–NaF–WO3) molten salt10.1007/s12598-013-0156-4 ↗
16. Lassner · 1999 · 85
17. Kinetic and thermodynamic theories of nucleation
18. Linke · Nucl. Fusion · 2011 · 51 · 610.1088/0029-5515/51/7/073017 ↗
19. Thermal fatigue mechanism of recrystallized tungsten under cyclic heat loads via electron beam facility10.1016/j.ijrmhm.2016.07.022 ↗
20. Material properties and their influence on the behaviour of tungsten as plasma facing material10.1088/1741-4326/aa6938 ↗
21. Transient heat load challenges for plasma-facing materials during long-term operation10.1016/j.nme.2016.12.024 ↗
22. Influence of surface morphology and microstructure on performanceof CVD tungsten coating under fusion transient thermal loads10.1016/j.apsusc.2016.08.060 ↗
23. Comparison of the thermal shock performance of different tungsten grades and the influence of microstructure on the damage behavior
24. Development of micro-engineered textured tungsten surfaces for high heat flux applications10.1016/j.jnucmat.2013.05.004 ↗
25. The thermal properties of high purity and fully dense tungsten produced by chemical vapor deposition10.1016/j.jnucmat.2014.11.095 ↗
26. Li · 2017
27. The influence of carbon and oxygen in the grain boundary on the brittle-ductile transition temperature of tungsten bi-crystals10.1016/0036-9748(84)90318-1 ↗
28. Surface topography of CVD-W coatings on graphite substrate with a PVD-Si intermediate layer after thermal fatigue testing10.1016/j.ijrmhm.2016.03.003 ↗