Microstructure evolution of the rolled tungsten during the current-assisted annealing treatment
Source abstract
Abstract
Current-assisted annealing treatment (CAAT) is a promising method for adjusting the microstructure of metals. It was employed to heat treat the tungsten (W) with a rolling deformation of 90% to clarify its microstructure evolution under the action of current. The grain morphologies before and after heat treatment were observed by metallographic microscopy. Compared to traditional heat treatment, the CAATed W is easier to achieve full recrystallization with finer and more uniform grains. This indicates that the current increases the nucleation rate of recrystallization. The Johnson-Mehl-Avrami-Kolmogorov (JMAK) model was applied to describe the increase rate of recrystallization fraction. It can be calculated that the apparent activation energy of recrystallization under current is only 352.9 kJ/mol. Combined with electron backscatter diffraction (EBSD) characterization, the rolled W prefers to align along the 〈100〉 // ND orientation with the prolonging of current action time. In essence, the acceleration of recrystallization and the tendency of grain orientation are both related to the atomic migration enhanced by current. The electric current can generate an additional driving force for atomic migration, especially in regions with high electrical resistivity, where this driving force becomes more pronounced, leading to intensified atomic migration.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. In situ oxide dispersion strengthened tungsten alloys with high compressive strength and high strain-to-failure10.1016/j.actamat.2016.09.034 ↗
2. Cold rolled tungsten (W) plates and foils: evolution of the microstructure10.1016/j.ijrmhm.2016.06.020 ↗
3. Recent progress in R&D on tungsten alloys for divertor structural and plasma facing materials10.1016/j.jnucmat.2013.02.074 ↗
4. Recent progress in research on tungsten materials for nuclear fusion applications in Europe10.1016/j.jnucmat.2012.08.018 ↗
5. Solution softening mechanism of iridium and rhenium in tungsten at room temperature10.1016/0263-4368(91)90028-M ↗
6. Interfacial fracture behavior of tungsten wire/tungsten matrix composites with copper-coated interfaces10.1016/j.msea.2009.10.046 ↗
7. In situ synchrotron tomography estimation of toughening effect by semi-ductile fibre reinforcement in a tungsten-fibre-reinforced tungsten composite system10.1016/j.actamat.2013.07.035 ↗
8. Fracture toughness investigations of tungsten alloys and SPD tungsten alloys10.1016/j.jnucmat.2007.03.079 ↗
9. Grain size engineering of bcc refractory metals: top-down and bottom-up—application to tungsten10.1016/j.msea.2007.02.099 ↗
10. Refinement of tungsten microstructure by severe plastic deformation
11. Microstructures and recrystallization behavior of severely hot-deformed tungsten10.1016/j.msea.2008.03.051 ↗
12. Deviations from Matthiessen’s rule of the electrical resistivity of dislocations in aluminum10.1143/JPSJ.36.698 ↗
13. The microstructure and property variations of metals induced by electric current treatment: a review10.1016/j.matchar.2018.08.058 ↗
14. Application of high-density electropulsing to improve the performance of metallic materials: mechanisms, microstructure and properties10.3390/ma11020185 ↗
15. Electromigration in metals10.1088/0034-4885/52/3/002 ↗
16. Overview no. 49: on the mechanisms for the electroplastic effect in metals10.1016/0001-6160(86)90001-5 ↗
17. Additional results on the electroplastic effect in metals10.1016/0036-9748(79)90311-9 ↗
18. A study of the electroplastic effect in metals10.1016/0036-9748(78)90026-1 ↗
19. Enhanced recovery and recrystallization of metals due to an applied current10.1016/j.scriptamat.2014.07.004 ↗
20. The effect of electric field and pressure on the synthesis and consolidation of materials: a review of the spark plasma sintering method10.1007/s10853-006-6555-2 ↗
21. Effect of electric current on recrystallization kinetics in interstitial free steel and AZ31 magnesium alloy10.1016/j.matchar.2017.09.021 ↗
22. Effect of electric current on crystal orientation and its contribution to densification during spark plasma sintering10.1016/j.matlet.2018.07.001 ↗
23. Characteristics of microstructure evolution during FAST joining of the tungsten foil laminate10.3390/met11060886 ↗
24. The influence of powder characteristics on densification behavior and microstructure evolution of W-Cr-Zr alloy consolidated by field-assisted sintering technology10.1016/j.ijrmhm.2022.105939 ↗
25. Effect of electric current on densification behavior of conductive ceramic powders consolidated by spark plasma sintering10.1016/j.actamat.2017.11.010 ↗
26. First principles calculation of lattice thermal conductivity of metals considering phonon-phonon and phonon-electron scattering10.1063/1.4953366 ↗
27. The critical point of average grain size in phonon thermal conductivity of fine-grained undoped lead telluride10.2320/matertrans.MT-M2020069 ↗
28. Mechanical property and thermal conductivity of pentadiamond: a comprehensive molecular dynamics study10.1016/j.commatsci.2021.111039 ↗
29. Current-induced marker motion in gold wires10.1016/0022-3697(61)90138-X ↗
30. Electromigration in integrated circuit conductors10.1088/0022-3727/32/17/201 ↗
31. Recrystallization kinetics of 50% hot-rolled 2% Y2O3 dispersed tungsten10.1016/j.fusengdes.2019.04.017 ↗
32. Study on austenitization kinetics of SA508 Gr. 3 steel based on isoconversional method10.3390/met6010008 ↗
33. On grain growth and phase precipitation behaviors during W-Cr-Zr alloy densification using field-assisted sintering technology10.1016/j.ijrmhm.2021.105552 ↗
34. The Johnson-Mehl-Avrami-Kohnogorov model: a brief review10.1007/BF03185527 ↗
35. Microstructure and annealing behavior of three rolled pure tungsten plates with different thickness reduction10.1016/j.fusengdes.2021.112863 ↗
36. A study of the batch annealing of cold-rolled HSLA steels containing niobium or titanium10.1007/s11661-015-2949-6 ↗
37. Recrystallization kinetics of warm-rolled tungsten in the temperature range 1150–1350° C10.1016/j.jnucmat.2014.08.037 ↗
38. The conductivity of lattices of spheres-ii. the body centred and face centred cubic lattices10.1098/rspa.1978.0129 ↗
39. Deviations from Matthiessen’s rule of the electrical resistivity of dislocations in aluminum10.1143/JPSJ.36.698 ↗
40. Nucleation and growth during recrystallization10.1590/S1516-14392005000300002 ↗
41. Grain growth10.1179/mst.1990.6.11.1136 ↗