Preparation of ultrafine tungsten powders by in-situ hydrogen reduction of nano-needle violet tungsten oxide
Source abstract
Abstract
Abstract Ultrafine tungsten powders with a grain size below 0.5 μm are key raw materials for fabricating ultrafine cemented carbides. Conventional hydrogen reduction technique has been utilized to prepare the ultrafine tungsten powders. In the present work, highly pure nano-needles of violet tungsten oxide (WO2.72) were reduced by dry hydrogen. Nucleation and growth of the metallic tungsten in the early stage of hydrogen reduction have been studied by XRD, FESEM and HRTEM. Mechanism of formation of nano-size tungsten powders is proposed and a concept of in-situ hydrogen of the nano-needle WO2.72 is presented. Empirical relations between an average diameter of nano-needle WO2.72 and an average particle size of the resultant tungsten powders in both stage of nucleation and industrial conduction have been established. These empirical relations could be a reasonable guidance for suitably choosing the raw materials of nano-needle WO2.72 to prepare ultrafine tungsten powders. It has been determined that the BET special surface areas of the in-situ hydrogen-reduced tungsten powders with the average particle size of 0.2 μm and 0.3 μm, which were produced from the raw nano-needle WO2.72 powders with the average diameter of 60 nm and 80 nm, are 6.03 m2/g and 4.65 m2/g, and the oxygen contents are 0.35% and 0.29%, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
References (17)
Show source-provided references
1. Wu · 2003
2. Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide — a review10.1016/j.ijrmhm.2008.07.011 ↗
3. Production and characterization of hydrogen- reduced submicron tungsten powders. Part I: State of the art in research, production and characterization of raw materials and tungsten powders10.1016/0263-4368(91)90017-I ↗
4. Production and characterization of hydrogen- reduced submicron tungsten powders. Part II: controlled decomposition of APT and hydrogen reduction of the oxides10.1016/0263-4368(91)90031-I ↗
5. Influence of tungsten oxides’ characteristics on fineness, homogeneity and looseness of reduced ultrafine tungsten powder
6. Wu · 2003
7. The preparation of tungsten powder from violet W18O49
8. Barin · 1995
9. Thermodynamics of the tungsten–oxygen system
10. Hydrogen reduction of tungsten trioxide and ammonium para-tungstate under high pressure10.2320/matertrans1960.15.75 ↗
11. Dynamic study on the morphology of hydrogen reduced tungsten oxide
12. Morphological changes occurring during reduction of WO310.1007/BF00566566 ↗
13. Morphology evolution of the product prepared by hydrogen reduction of Tungsten oxides
14. Mechanism of technical reduction of tungsten: Part 2. Hydrogen reduction of tungsten blue oxide to tungsten powder
15. Growth and morphology of W18O49 crystals produced by microwave decomposition of ammonium paratungstate10.1016/S0022-0248(96)00669-0 ↗
16. Surface-energy-anisotropy-induced orientation effects on Rayleigh instabilities in sapphire10.1016/j.susc.2005.11.038 ↗
17. Wu · 2003