Wear mechanism of thermally transformed CVD Al2O3 layer
Source abstract
Abstract
Abstract Wear mechanism of the thermally transformed CVD α-Al2O3 that was produced from as-deposited κ-Al2O3 by different heat-treatment processes have been investigated. For alloy steel turning, the wear of the transformed α-Al2O3 produced by a heat-treatment through a cooling process after κ-Al2O3 deposition was uneven, that is, small chippings and flakings of the layer occurred on the wear surface, although its wear resistance was higher than that of as-deposited α-Al2O3 and as-deposited κ-Al2O3. On the other hand, the transformed α-Al2O3 produced by the heat-treatment without a cooling process but in connection to κ-Al2O3 deposition showed an excellent wear resistance without uneven wear. For the α-Al2O3 transformed without a cooling process, crack generation during the cooling is inhibited by the microcracks that have been generated before the cooling by a phase transformation of κ → α. Wear resistance is improved because the cooling cracks with a wide width, which will act as starting points of the uneven wear, decrease.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Lindstrom J, Jonsson B, Ohlsson F. US Patent 3,837,896; 1974.
2. Funk · J Electrochem Soc · 1976 · 123 · 28510.1149/1.2132804 ↗
3. Lindstrom · J Electrochem Soc · 1976 · 123 · 55510.1149/1.2132876 ↗
4. Park · J Electrochem Soc · 1983 · 130 · 160710.1149/1.2120043 ↗
5. Lux · Thin Solid Films · 1986 · 138 · 4910.1016/0040-6090(86)90214-2 ↗
6. Colombier · J Mater Sci · 1989 · 24 · 46210.1007/BF01107428 ↗
7. Skogsmo J, Liu P, Chatfield C, Norden H. In: Bildstein H, Ortner HM, editors. Proceedings of the 12th international plansee seminar, Metallwerk Plansee, Reutte, Austria, vol. 3. 1989. p. 129.
8. Layyous · Surf Coat Technol · 1992 · 56 · 8910.1016/0257-8972(92)90200-T ↗
9. Halvarsson · Surf Coat Technol · 1993 · 61 · 17710.1016/0257-8972(93)90222-A ↗
10. Soderlund · J Mater Res · 1994 · 9 · 168310.1557/JMR.1994.1683 ↗
11. Halvarsson · Surf Coat Technol · 1994 · 68/69 · 26610.1016/0257-8972(94)90172-4 ↗
12. Fredriksson · Thin Solid Films · 1995 · 263 · 2810.1016/0040-6090(95)06546-6 ↗
13. Halvarsson · Surf Coat Technol · 1996 · 80 · 8010.1016/0257-8972(95)02690-8 ↗
14. Vuorinen · Thin Solid Films · 1992 · 214 · 13210.1016/0040-6090(92)90761-Y ↗
15. Skogsmo · Surf Coat Technol · 1992 · 54–55 · 186
16. Fredriksson · Surf Coat Technol · 1993 · 56 · 16510.1016/0257-8972(93)90022-G ↗
17. Lindulf · Thin Solid Films · 1994 · 253 · 31110.1016/0040-6090(94)90340-9 ↗
18. Hansson · Surf Coat Technol · 1995 · 76–77 · 25610.1016/0257-8972(95)02580-4 ↗
19. Larsson · Surf Coat Technol · 1997 · 94–95 · 7610.1016/S0257-8972(97)00479-9 ↗
20. Larsson · Int J Refract Metals Hard Mater · 1998 · 16 · 36910.1016/S0263-4368(98)00042-0 ↗
21. Larsson · Surf Coat Technol · 1999 · 111 · 19110.1016/S0257-8972(98)00734-8 ↗
22. Ljungberg B, Lenander A. US Patent 5,487,625; 1996.
23. Karino · J Jpn Soc Precis Eng · 1995 · 61 · 77310.2493/jjspe.61.773 ↗