Analysis of contact state and fracture mode of WC-10Co/B318 steel joint fabricated by resistance welding
Source abstract
Abstract
The dissimilar joining of B318 steel and two shapes (spherical and cylindrical) of WC-10Co pellets was performed using resistance welding for application in bimetal band saw blades. The study investigates the effects of pellet shape on joint characteristics and contact state by analyzing the welding process, dynamic resistance, temperature field, macroscopic and microscopic joint morphology, and fracture mode. The results indicated that the shear force of joints with different shapes initially increases before decreasing as the welding current rises. The welding range for the spherical joint is narrower than that for the cylindrical joint, and no reaction layer is formed at the joint. In contrast, the cylindrical joint exhibits a shear force of 1175.3N at 750 A, representing the highest value among the two shapes across various welding currents. Under this parameter, the thickness of the formed reaction layer of the cylindrical joint is moderate, with no severe element loss, and fractures occur in the steel`s heat-affected zone (HAZ). High-speed photography results showed that spherical joints generate heat faster than cylindrical joints. Numerical simulation results indicated that the peak temperature in spherical joints is higher than in cylindrical joints. These differences can be attributed to variations in pellet curvatures of different shapes, leading to different contact states of the workpieces during welding. This affected the heat generation process, the amount of joint deformation, and the elemental migration and metallurgical reactions at the joint interface. Comparing all aspects, the welding performance of the cylindrical joint proves superior to that of the spherical joint.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Mechanically enhancing a brazed joint of WC-co/3Cr13 by utilizing a nanoporous cu lamina interlayer prepared by chemical dealloying10.1016/j.matlet.2023.135530 ↗
2. Dissimilar joining of cemented carbide to low-carbon steel via combustion welding: effect of process parameters on the interfacial microstructure and joint strength10.1016/j.jmapro.2022.03.043 ↗
3. Microstructure and mechanical behavior of dissimilar AISI 304L/WC-co cermet rotary friction welds10.1016/j.msea.2019.04.081 ↗
4. Experiments and numerical simulations on joint formation and material flow during resistance upset welding of WC-10Co and B318 steel10.1016/j.jmatprotec.2021.117164 ↗
5. Microstructural evolution and mechanical properties of diffusion bonding WC-co cemented carbide to steel using co and composite Ni/co interlayers10.1016/j.ijrmhm.2021.105736 ↗
6. Microstructure and properties of WC–co cemented carbide/40Cr steel joints brazed at low–temperature with ag–cu–in–Ti filler alloy10.1016/j.ijrmhm.2022.106092 ↗
7. WC-Co/316L stainless steel joining by laser powder bed fusion for multi-material cutting tools manufacturing10.1016/j.ijrmhm.2023.106140 ↗
8. Influence of braze type on microstructure and mechanical behavior of WC-co/steel dissimilar joints10.1016/j.jmapro.2018.10.015 ↗
9. Microstructure transformation and crack sensitivity of WC-co/steel joint welded by electron beam10.1016/j.vacuum.2016.12.038 ↗
10. Effects of groove shape on microstructure and properties of resistance spot welding joints in WC-10Co/B318 steel10.1016/j.ijrmhm.2021.105693 ↗
11. Characterization and stress relaxation of the functionally graded WC–Co/Ni component/stainless steel joint10.1016/j.jallcom.2012.12.152 ↗
12. Microstructural evolution during low-temperature brazing of WC-co cemented carbide to AISI 4140 steel using a silver-based filler alloy10.1016/j.ijrmhm.2023.106354 ↗
13. Dissimilar vacuum brazing of cemented carbide to steel using double-layer filler metals10.1016/j.jmapro.2019.09.015 ↗
14. Effect of brazing current on microstructure and mechanical behavior of WC-Co/AISI 1020 steel TIG brazed joint10.1016/j.ijrmhm.2016.11.004 ↗
15. WC particulate reinforced joint by ultrasonic-associated brazing of WC-co/35CrMo10.1016/j.jmatprotec.2016.06.037 ↗
16. Rapid diffusion bonding of WC-co cemented carbide to 40Cr steel with Ni interlayer: effect of surface roughness and interlayer thickness10.1016/j.ceramint.2016.07.145 ↗
17. Interfacial microstructure and mechanical strength of WC–co/90MnCrV8 cold work tool steel diffusion bonded joint with cu/Ni electroplated interlayer10.1016/j.matdes.2010.01.050 ↗
18. Effect of interlayer thickness on the microstructure and strength of WC-co/invar/316L steel joints prepared by fibre laser welding10.1016/j.jmatprotec.2017.12.030 ↗
19. Fiber laser welding of WC-co to carbon steel using Fe-Ni invar as interlayer10.1016/j.ijrmhm.2015.12.006 ↗
20. Investigation on microstructure of electron beam welded WC-co/40Cr joints10.1016/j.vacuum.2017.12.012 ↗
21. Electron beam hybrid welding-brazing of WC-Co/40Cr dissimilar materials10.1016/j.ceramint.2019.01.088 ↗
22. G.Q. Chen, B.G. Zhang, Z.Z. Wu, W. Mao, J.C. Feng, Electron beam welding–brazing of hard alloy to steel with Ni-Fe intermediate, Int. J. Refract. Met. Hard Mater. 40 (2013) 58–63.10.1016/j.ijrmhm.2013.03.002 ↗
23. Characterization of WC/12Co cermet–steel dissimilar friction stir welds10.1016/j.jmapro.2017.11.012 ↗
24. Effect of a Ni interlayer on microstructure and mechanical properties of WC-12Co cermet/SC45 steel friction stir welds10.1016/j.jmapro.2019.02.032 ↗
25. Effects of Ni coating thickness on the microstructure and mechanical properties of resistance-welded WC-co/B318 steel joints10.1016/j.ceramint.2021.05.289 ↗
26. Effects of welding current on the microstructure and mechanical behavior of resistance-welded WC-co/B318 steel joints10.1016/j.ceramint.2021.03.056 ↗
27. Microstructure and mechanical property of WC-10Co/RM80 steel dissimilar resistance spot welding joint10.1016/j.msea.2020.139008 ↗
28. Monitoring the evolution of resistance-welded WC-10Co/B318 steel joint based on welding time10.1016/j.ijrmhm.2023.106221 ↗
29. Effect of holding time and interlayer’s thickness on the crack initiation and propagation and the dissolving behavior of the heat-treated facet WC grains10.1016/j.ijrmhm.2017.11.006 ↗
30. Microstructure and properties of WC-co/3Cr13 joints brazed using Ni electroplated interlayer10.1016/j.ijrmhm.2012.02.018 ↗
31. Influence of brazing technology on the microstructure and properties of YG20C cemented carbide and 16Mn steel joints10.1007/s40194-016-0374-0 ↗
32. Investigation on diffusion bonding of functionally graded WC-co/Ni composite and stainless steel10.1016/j.matdes.2012.11.006 ↗
33. Dissimilar welding of WC-co cemented carbide to Ni42Fe50.9C0.6Mn3.5Nb3 invar alloy by laser-tungsten inert gas hybrid welding10.1016/j.matdes.2010.06.006 ↗
34. WC particulate reinforced joint by ultrasonic-associated brazing of WC-co/35CrMo10.1016/j.jmatprotec.2016.06.037 ↗
35. Effect of brazing temperature and holding time on joint properties of induction brazed WC-co/carbon steel using ag-based alloy10.1016/j.jmatprotec.2015.09.044 ↗
36. Vacuum brazing of WC-8Co cemented carbides to carbon steel using pure cu and ag-28Cu as filler metal10.1007/s11665-016-2424-6 ↗
37. La2O3 addition for improving the brazed joints of WC-co/1Cr1310.1016/j.jmatprotec.2018.11.045 ↗
38. Effects of NbC additions on the microstructure and properties of nonuniform structure WC-co cemented carbides10.1016/j.msea.2017.01.077 ↗
39. Effect of groove shape on laser welding-brazing Al to steel10.1016/j.jmatprotec.2017.10.025 ↗
40. Predicting the influence of groove angle on heat transfer and fluid flow for new gas metal arc welding processes10.1016/j.ijheatmasstransfer.2011.08.046 ↗
41. A study of dynamic resistance during small scale resistance spot welding of thin Ni sheets10.1088/0022-3727/37/14/017 ↗
42. Fiber laser welding of WC-co and carbon steel dissimilar materials