Fatigue performance improvement of electrical discharge machined hardmetals by means of combined thermal annealing and surface modification routes
Source abstract
Abstract
Electrical discharge machining (EDM) provides an effective means of shaping hardmetals. However, it is also known that surface integrity of these materials may be affected by EDM, degrading their tribomechanical characteristics. This work focuses on assessing the use of two different surface modification routes: thermomechanical treatments (shot blasting, polishing and final high temperature annealing) and/or physical vapor deposition of hard coatings, for improving the fracture and fatigue strength of an EDM-shaped fine-grained hardmetal grade. In doing so, an optimal EDM's surface finish variant and a diamond ground and polished one are used. Mechanical behavior is evaluated under four-point bending and fatigue characterization is given in terms of fatigue limit following the staircase method. Experimental results indicate that both approaches markedly decrease the lessening effect of EDM on the mechanical strength of hardmetals, although a complete fracture and fatigue strength retention is only achieved by combining both of them. The improved mechanical behavior is rationalized on the basis of the beneficial changes induced by surface modification on the effective residual stress field at the surface of EDM-shaped hardmetals, as assessed by a linear elastic fracture mechanics analysis combined with fractographic examination.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Physical and chemical nature of cemented carbides
2. Study of the effect of machining parameters on the machining characteristics in electrical discharge machining of tungsten carbide10.1016/S0924-0136(01)00992-X ↗
3. Analysis of the influence of EDM parameters on surface quality, MRR and EW of WC-Co10.1016/j.jmatprotec.2004.04.346 ↗
4. Influence of the composition of WC-based cermets on manufacturability by wire-EDM10.1016/S1526-6125(07)00007-2 ↗
5. Summary report on the CIRP cooperative research on spark-erosion machining of cemented carbides (die-sinking)10.1016/S0007-8506(16)30040-3 ↗
6. Machining of WC-Co composites10.1080/10426918908956301 ↗
7. Development of the cylindrical wire electrical discharge machining process, part 1: concept, design and material removal rate10.1115/1.1475321 ↗
8. Development of the cylindrical wire electrical discharge machining process, part 2: surface integrity and roundness10.1115/1.1475989 ↗
9. Cracking behaviour of sintered carbides during EDM
10. Analysis of electro discharge machining of cemented carbides10.1016/S0007-8506(07)60906-8 ↗
11. Influence of electrical discharge machining on the sliding contact response of cemented carbides10.1016/S0263-4368(00)00045-7 ↗
12. Nanoindentation characterization of surface layers of electrical discharge machined WC-Co10.1016/S0921-5093(02)00395-7 ↗
13. Surface integrity effects on the fracture resistance of electrical-discharge-machined WC-Co cemented carbides10.1111/j.1551-2916.2004.01687.x ↗
14. Fracture and fatigue behavior of electrical-discharge machined cemented carbides10.1016/j.ijrmhm.2005.04.007 ↗
15. Influence of electrical discharge machining on the reciprocating sliding friction and wear response of WC-Co cemented carbides10.1016/j.ijrmhm.2008.09.002 ↗
16. Surface finishing: impact on tribological characteristics of WC-Co hardmetals10.1016/j.triboint.2009.04.029 ↗
17. Techniques for improved surface integrity of electrodischarge machined ceramic composites10.1179/026708400101517396 ↗
18. Surface integrity in electro-discharge machining, ultrasonic machining, and diamond saw cutting of ceramic composites10.1016/S0272-8842(00)00024-9 ↗
19. Mechanical surface treatments of electro-discharge machined (EDMed) ceramic composite for improved strength and realiability10.1016/S0955-2219(01)00296-5 ↗
20. Mechanical strength improvement of electrical discharge machined cemented carbides through PVD (TiN, TiAlN) coatings10.1016/S0040-6090(03)01062-9 ↗
21. Improvement of fatigue life of electrical discharge machined AISI D2 tool steel by TiN coating10.1016/S0921-5093(01)01268-0 ↗
22. The influence of sample preparation on Palmqvist's method for toughness testing of cemented carbides
23. Fracture toughness evaluation of hardmetals: influence of testing procedure10.1016/S0263-4368(00)00044-5 ↗
24. TiN coating on an electrical discharge machined WC-Co hardmetal: surface integrity effects on indentation adhesion response10.1007/s10853-006-0005-z ↗
25. Adhesion and abrasive wear resistance of TiN deposited on electrical discharge machined WC-Co cemented carbides10.1016/j.wear.2007.11.016 ↗
26. Failure of materials in mechanical design
27. On the fatigue crack growth behavior of WC-Co cemented carbides: kinetics description, microstructural effects and fatigue sensitivity10.1016/S1359-6454(02)00071-X ↗
28. An empirical stress-intensity factor equation for the surface crack10.1016/0013-7944(81)90116-8 ↗
29. Monolithic and composite ceramic machining flaw-microstructure-strength effects: model evaluation10.1016/S0955-2219(01)00488-5 ↗
30. Diamond coatings on electrical-discharge machined hardmetals10.1016/S0925-9635(02)00226-1 ↗
31. Residual stress in cemented carbide following a coating process and after ion implantation post-treatment of the coating10.1016/S0257-8972(98)00670-7 ↗
32. X-ray diffraction characterization of pre-treated cemented carbides for optimizing adhesion strength of sputtered hard coatings10.1016/S0257-8972(01)01282-8 ↗
33. Influence of the residual stress state on cohesive damage of PVD-coated carbide cutting tools10.1002/adem.200800063 ↗
34. Mechanical failure of thin brittle coatings10.1016/1350-6307(95)00014-H ↗
35. Fatigue mechanics of WC-Co cemented carbides10.1016/S0263-4368(01)00032-4 ↗