journal article·2012-01

Bulk WC–Al2O3 composites prepared by spark plasma sintering

Donghai Zheng, Xiaoqiang Li, Xuan Ai, Chao Yang, Yuanyuan Li

Publisher page

Abstract

Abstract WC and WC–Al 2 O 3 materials without metallic binder addition were densified by spark plasma sintering in the range of 1800–1900 °C. The densification behavior, phase constitution, microstructure and mechanical properties of pure WC and WC–Al 2 O 3 composite were investigated. The addition of Al 2 O 3 facilitates sintering and increases the fracture toughness of the composites to a certain extent. An interesting phenomenon is found that a proper content of Al 2 O 3 additive helps to limit the formation of W 2 C phase in sintered WC materials. The pure WC specimen possesses a hardness (HV 10 ) of 25.71 GPa, fracture toughness of 4.54 MPa·m 1/2 , and transverse fracture strength of 862 MPa, while those of WC-6.8 vol.% Al 2 O 3 composites are 24.48 GPa, 6.01 MPa·m 1/2 , and 1245 MPa respectively. The higher fracture toughness and transverse fracture strength of WC-6.8 vol.% Al 2 O 3 are thought to result from the reduction of W 2 C phase, the crack-bridging by Al 2 O 3 particles and the local change in fracture mode from intergranular to transgranular.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Properties of ultra-fine grain binderless cemented carbide ‘RCCFN’10.1016/0263-4368(95)92676-B ↗
2. Consolidation and properties of binderless sub-micron tungsten carbide by field-activated sintering10.1016/j.ijrmhm.2004.08.003 ↗
3. One step synthesis and densification of ultra-fine WC by high-frequency induction combustion10.1016/j.ijrmhm.2005.04.004 ↗
4. Binder-free WC bulk synthesized by spark plasma sintering10.1016/j.jallcom.2008.12.151 ↗
5. Microstructures of binderless tungsten carbides sintered by spark plasma sintering process10.1016/S0921-5093(03)00151-5 ↗
6. Bulk ultrafine binderless WC prepared by spark plasma sintering10.1016/j.scriptamat.2005.10.014 ↗
7. Consolidation of binderless WC–TiC by high frequency induction heating sintering10.1016/j.ijrmhm.2007.01.006 ↗
8. Binderless WC and WC–VC materials obtained by pulsed electric current sintering10.1016/j.ijrmhm.2007.01.002 ↗
9. Sintering of binderless WC–Mo2C hard materials by rapid sintering process10.1016/j.ceramint.2007.03.029 ↗
10. Pressureless sintering and tribological properties of WC–ZrO2 composites10.1016/j.jeurceramsoc.2004.05.021 ↗
11. Processing of ultrafine ZrO2 toughened WC composites10.1016/j.jeurceramsoc.2009.07.013 ↗
12. Fabrication of nanocrystalline WC and nanocomposite WC–MgO refractory materials at room temperature10.1016/S0925-8388(99)00508-3 ↗
13. Fabrication and characterizations of new nanocomposite WC/Al2O3 materials by room temperature ball milling and subsequent consolidation10.1016/j.jallcom.2004.08.064 ↗
14. A critical-evaluation of indentation techniques for measuring fracture toughness. 1. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
15. Elastic properties of ceramic–metal particulate composites10.1016/j.msea.2004.10.009 ↗
16. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
17. Microstructural characterization of Al2O3–SiC nanocomposites10.1016/S0955-2219(97)00103-9 ↗