Annealing behaviour of sub-stoichiometric Ti(C,N)–W mechanical alloy powders
Source abstract
Abstract
Abstract The annealing behaviour of Ti(C 0.5 N 0.05 )–40 wt.% W and Ti(C 0.5 N 0.5 ) 0.6 –40 wt.% W mechanically alloyed powders was investigated using XRD, TEM, SEM and DTA techniques. It was observed that the reaction start and finish temperatures between constituents were lower in the system that had higher residual lattice strains after milling. The compositions of the intermetallic compounds and solution phases formed were dependent of the milling conditions and the annealing temperature. Thermal alloying was observed during annealing of Ti(C 0.5 N 0.05 )–40 wt.% W mechanically alloyed products, whereas de-mixing of W-rich phases from the metastable solid solution occurred during annealing of the Ti(C 0.5 N 0.5 ) 0.6 –40 wt.% W milled powders.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Transformation and alloying mechanisms in sub-stoichiometric titanium carbonitrides–tungsten high energy ball milled powders10.1016/j.ijrmhm.2010.12.009 ↗
2. An investigation on the solid state sintering of mechanically alloyed nano-structured 90W–Ni–Fe tungsten heavy alloy10.1016/j.ijrmhm.2007.05.011 ↗
3. Effects of tungsten and aluminium additions on the formation of molybdenum disilicide by mechanically-induced self-propagation reaction10.1016/j.jallcom.2009.09.189 ↗
4. Decarburization of TiC in Ni activated sintered W–xTiC (x=0, 5, 10, 15wt%) composites and the effects of heat treatment on the microstructural and physical properties10.1016/j.ijrmhm.2010.02.004 ↗
5. Synthesis of AlN–TiN nanostructured composite powder by reactive ball milling and subsequent thermal treatment10.1016/j.jallcom.2010.07.037 ↗
6. Fabrication of W–20wt% Ti alloy by pressureless sintering at low temperature10.1016/j.ijrmhm.2010.04.004 ↗
7. The effect of annealing temperature an structure and magneticproperties of nanocomposite Nd10Fe84–xWxB6 (0<x<33at.%) magnets10.1016/j.jmatprotec.2005.04.064 ↗
8. Preparation of W–15wt% Ti prealloyed powders10.1016/j.ijrmhm.2009.03.004 ↗
9. Synthesis of Ti(, M1, M2)(CN)–Ni nanocrystalline powders10.1016/j.ijrmhm.2005.05.002 ↗
10. Structural evolution and grain growth kinetics of the Fe–28Al elemental powder during mechanical alloying and annealing10.1016/j.intermet.2006.12.005 ↗
11. Processing of Cr2Nb precursor through powder metallurgy route10.1016/j.powtec.2009.09.012 ↗
12. Annealing behaviour of mechanically alloyed nanocrystalline NiAl intermetallic under oxidizing and non-oxidizing conditions10.1016/j.jallcom.2009.05.070 ↗
13. Phase transformations in Fe–Ni system at mechanical alloying and consequent annealing of elemental powder mixtures10.1016/S0921-4526(01)00473-2 ↗
14. A W — In solid solution synthesized by mechanical alloying10.1016/j.msea.2006.12.068 ↗
15. The effect of heat treatment on the microstructure and magnetic properties of mechanically alloyed Fe–45%Ni nanostructured powders10.1016/j.jallcom.2010.09.159 ↗
16. Effect of ball milling and post-annealing on magnetic properties of Ni49.8Mn28.5Ga21.7 alloy powders10.1016/j.intermet.2008.08.002 ↗
17. Nanocrystalline Fe–Nb–(B, Ge) alloys from ball milling: microstructure, thermal stability and magnetic properties10.1016/j.intermet.2007.04.008 ↗
18. Magnetic behavior of nanocrystalline Cu–Ni–Co alloys prepared by mechanical alloying and isothermal annealing10.1016/j.jallcom.2007.02.139 ↗
19. Thermal analysis on the curie temperature of nanocrystalline Ni produced by ball milling
20. Influence of milling parameters on the manufacturing of Fe–TiCN composite powders10.1016/j.jmatprotec.2005.02.154 ↗
21. Influence of milling time on the processing of Fe–TiCN composites10.1016/j.msea.2006.05.051 ↗
22. New production of TiCxN1−x-based cermets by one step mechanically induced self-sustaining reaction: powder synthesis and pressureless sintering10.1016/j.jeurceramsoc.2008.02.007 ↗
23. Limits of the Mg–Al γ-phase range by ball-milling10.1016/j.intermet.2007.05.001 ↗
24. Nanocrystallie CoCrFeNiCuAl high-entropy solid solution synthesized by mechanical alloying10.1016/j.jallcom.2009.05.144 ↗
25. Amorphisation of Cr–10Co mixture by mechanical alloying10.1016/j.jnoncrysol.2010.01.015 ↗
26. Mechanical alloying, fine structure and thermal decomposition of nanocrystalline FCC–Fe60Cu4010.1016/S0921-4526(00)00531-7 ↗
27. Vacuum sintering of WC–8wt% Co hardmetals from WC powders with different dispersity10.1016/j.ijrmhm.2010.10.010 ↗
28. XRD analysis and microstructure of milled and sintered V, W, C, and Co powders10.1016/j.ijrmhm.2010.08.008 ↗
29. Formation of titanium nitride produced from nanocrystalline titanium powder under nitrogen atmosphere10.1016/j.ijrmhm.2010.05.008 ↗
30. Mechanism of mechanical alloying10.1007/BF02644161 ↗
31. Massalski · 1990 · 3497
32. Morphological and structural evolutions of non-equilibrium titanium-nitride alloy powders produced by reactive ball milling10.1557/JMR.1992.0888 ↗
33. Amorphization reaction during mechanical alloying: influence of milling conditions10.1007/BF00576540 ↗
34. Investigation of the ternary phase diagram of mechanically alloyed FeCuAg10.1088/0953-8984/9/15/016 ↗
35. Mechanochemical synthesis of metastable solid solutions: phase composition and microstructure evolution10.1007/BF02758016 ↗
36. Mechanically alloyed Mo-Si-B alloys with a continuous α-Mo matrix and improved mechanical properties10.1016/j.intermet.2008.04.015 ↗
37. Microstructure and crystal structure of an equimolar Mg–Ti alloy processed by Simoloyer high energy ball mill10.1016/j.powtec.2010.01.014 ↗
38. Mechanical alloying of Fe100−x−yNbxBy (x=5, 10; y=10, 15): from pure powder mixture to amorphous phase10.1016/j.intermet.2008.06.006 ↗