journal article·2022-02

Microstructure and mechanical behavior of porous tungsten skeletons synthesized by selected laser melting

Kai Zhou, Wenge Chen, Yana Yang, Rong Li, Longlong Dong, Yong-Qing Fu

Publisher page

Abstract

Because of its high ductile-brittle transition temperature, tungsten (W) is normally alloyed with other metal elements in order to obtain high fracture strength, excellent thermal and electrical properties for industrial applications. For tungsten samples sintered using the conventional powder metallurgy methods, bonding among tungsten particles is normally through sintered necking process, thus without providing a good metallurgical bonding strength. In this paper, we proposed to apply additive manufacture methodology to synthesize two types of porous tungsten skeleton structures, honeycomb (65% porosity) and square skeleton (80% porosity), using a selective laser melting (SLM) method. Results showed that for both these skeleton structures, grains in the XY plane showed an equiaxed crystal appearance, whereas those in the YZ/XZ plane showed columnar patterns parallel to the Z axis. The measured porosities for these two types of skeletons were 52 vol% and 68 vol%, and their compressive strength values were 256 MPa and 149 MPa, respectively. Both their compressive strengths and hardness showed anisotropic behaviors, with their highest values along the direction of Z axis. Results also showed that fracture morphology and mechanisms of these skeletons under compression were quite different when they were compressed along different directions, mainly due to the formed columnar crystals of the skeletons along the Z axis. Fracture morphology along the Z axis showed transgranular fracture and tearing features, whereas those along X axis showed only intergranular fracture features.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Additive manufacturing of pure tungsten by means of selective laser beam melting with substrate preheating temperatures up to 1000 C10.1016/j.nme.2019.02.034 ↗
2. Additive manufacturing of high density pure tungsten by electron beam melting
3. Infiltration sintering of WCu alloys from copper-coated tungsten composite powders for superior mechanical properties and arc-ablation resistance10.1016/j.jallcom.2017.08.164 ↗
4. Improved pseudo-ductile behavior of powder metallurgical tungsten short fiber-reinforced tungsten (Wf/W)10.1016/j.nme.2018.05.001 ↗
5. Assessment of mechanical properties of SPS-produced tungsten including effect of neutron irradiation10.1016/j.ijrmhm.2020.105207 ↗
6. Microstructure and mechanical properties of dispersion strengthened tungsten by HIP treatment followed by thermal annealing10.1016/j.rinma.2020.100116 ↗
7. Experimental study on the high-damping properties of metallic lattice structures obtained from SLM10.1016/j.precisioneng.2021.02.010 ↗
8. Effect of processing parameters on the densification, microstructure and crystallographic texture during the laser powder bed fusion of pure tungsten10.1016/j.ijrmhm.2018.10.004 ↗
9. Crack suppression via in-situ oxidation in additively manufactured W-Ta alloy
10. SLM lattice structures: properties, performance, applications and challenges10.1016/j.matdes.2019.108137 ↗
11. Cracking in laser additively manufactured W: initiation mechanism and a suppression approach by alloying10.1016/j.matdes.2018.12.010 ↗
12. Effects of processing parameters on the densification, microstructure and mechanical properties of pure tungsten fabricated by optimized selective laser melting: from single and multiple scan tracks to bulk parts10.1016/j.ijrmhm.2021.105490 ↗
13. Pure tungsten and oxide dispersion strengthened tungsten manufactured by selective laser melting: microstructure and cracking mechanism
14. Selective laser melting additive manufacturing of pure tungsten: role of volumetric energy density on densification, microstructure and mechanical properties10.1016/j.ijrmhm.2019.105025 ↗
15. High-density tungsten fabricated by selective laser melting: densification, microstructure, mechanical and thermal performance10.1016/j.optlastec.2019.03.018 ↗
16. Analysis of laser-induced microcracking in tungsten under additive manufacturing conditions: experiment and simulation10.1016/j.actamat.2020.04.060 ↗
17. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
18. Tensile and compression properties of variously arranged porous Ti-6Al-4V additively manufactured structures via SLM10.1016/j.prostr.2018.12.025 ↗
19. Review on residual stress in selective laser melting additive manufacturing of alloy parts10.1016/j.optlastec.2020.106283 ↗
20. Microstructure and mechanical behavior of porous Ti-6Al-4V parts obtained by selective laser melting10.1016/j.jmbbm.2013.05.011 ↗
21. Osteogenesis of 3D printed porous Ti6Al4V implants with different pore sizes10.1016/j.jmbbm.2018.04.010 ↗
22. Balling phenomena in selective laser melted tungsten10.1016/j.jmatprotec.2015.02.032 ↗
23. An experimental and numerical study of the high cycle multiaxial fatigue strength of titanium lattice structures produced by Selective Laser Melting (SLM)10.1016/j.ijfatigue.2020.105623 ↗
24. Fabrication and compression property of tungsten skeleton for tungsten-copper composite
25. The thermoviscoplastic response of polycrystalline tungsten in compression10.1016/S0921-5093(99)00517-1 ↗
26. Microstructure and mechanical deformation behavior of selective laser melted Ti6Al4V ELI alloy porous structures10.1016/j.matlet.2020.128366 ↗
27. Effect of crystallographic textures on thermal anisotropy of selective laser melted Cu-2.4Ni-0.7Si alloy
28. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗