Investigation of binderless WC–TiC–Cr3C2 hard materials prepared by spark plasma sintering (SPS)
Source abstract
Abstract
Abstract Binderless TiC–WC–Cr 3 C 2 hard materials with different compositions were prepared by FAST (field-assisted sintering technique) and by SPS from mixtures of TiC, WC and Cr 3 C 2 . The effect of the microstructure on the properties was evaluated in as-densified materials and materials heat treated at 1900 °C. The mechanical properties were determined and the microstructures were characterised using X-ray diffraction and scanning electron microscopy. A cubic (Ti, W, Cr)C phase was found to form during sintering. Hardness values of up to 23 GPa were observed. For the TiC-rich materials annealing did not have a significant effect on the hardness, but in the case of the WC-rich materials it resulted in a reduction in the hardness due to pore formation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Sintering study of nanocrystalline tungsten carbide powders10.1016/S0965-9773(98)00116-0 ↗
2. Growth behavior of rounded (Ti, W)C and faceted WC grains in a Co matrix during liquid phase sintering10.1016/j.actamat.2005.06.021 ↗
3. Microstructures of binderless tungsten carbides sintered by spark plasma sintering process10.1016/S0921-5093(03)00151-5 ↗
4. Microstructure and abrasive wear of binderless carbides10.1111/j.1151-2916.2000.tb01580.x ↗
5. Consolidation of binderless WC–TiC by high frequency induction heating sintering10.1016/j.ijrmhm.2007.01.006 ↗
6. Sintering behaviour of ultra-fine titanium diboride powder prepared by self-propagating high-temperature synthesis (SHS) technique10.1016/j.msea.2006.11.083 ↗
7. Binderless WC and WC–VC materials obtained by pulsed electric current sintering10.1016/j.ijrmhm.2007.01.002 ↗
8. Spark plasma sintering and deformation of Ti–TiB2 composites10.1016/j.msea.2007.01.161 ↗
9. The synthesis and consolidation of hard materials by spark plasma sintering10.1016/j.ijrmhm.2008.09.011 ↗
10. Bulk ultrafine binderless WC prepared by spark plasma sintering10.1016/j.scriptamat.2005.10.014 ↗
11. Brooks · 1998
12. Zur Kenntnis des Systems Wolframkarbid-Titankarbid-Chromkarbid
13. Data collection of properties of hard materials
14. Evaluation of KIC of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
15. Sintering, consolidation, reaction and crystal growth by the spark plasma system (SPS)10.1016/S0921-5093(00)00773-5 ↗
16. Kosolapova · 1986
17. Microstructure and properties of hot-pressed (Hf, Ti)C10.1016/j.ijrmhm.2006.08.004 ↗
18. Transition metal carbides, nitrides, and carbonitrides
19. Indentation hardness and fracture toughness in single crystal TiC0.9610.1016/0921-5093(95)10152-7 ↗