Microstructural evolution of W-10Re alloys due to thermal cycling at high temperatures and its impact on surface degradation
Source abstract
Abstract
Abstract This paper features four microstructurally different tungsten 10 wt% rhenium (W10Re) alloys tested by thermal cycling at high temperatures in a conventional electron beam welding machine. The sample surfaces undergo minimum temperatures of 1700–1750 °C with 3.000–180.000 additional temperature jumps of 170–200 °C. The used materials show microstructural changes as well as surface damage related to the exposure time and the number of applied temperature jumps. The loaded surfaces show formation of slip bands, grain boundary bulging, pitting, thermal grooving as well as crack formation after the cyclic thermal loading. An initial columnar grain structure reduced pitting of grains at the surface by influencing the preferential crack direction, while on the other hand increasing surface swelling. Introducing HfC into the W10Re matrix led to a smaller final grain size after recrystallization as well as decreasing surface swelling and pitting. A larger initial grain size has shown increased surface degradation and large amounts of swelling. The changes in microstructure were characterized by classical metallographic means including light optical microscopy and hardness testing. The surface damage was investigated in detail by using laser scanning microscopy. Differences in surface damage mechanisms were characterized by electron back scatter diffraction and scanning electron images. The combination of temperature measurements with finite element modeling enabled to calculate the temperatures and loading conditions of the samples.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. The heat dissipation in the anode of an X-ray tube
2. Behling · 2015
3. A “spinning target X-ray generator” and its input limit
4. Höhere Belastung von Drehanodenröhren durch Verwendung von legierten Anoden
5. Höhere Belastung von Drehanodenröhren durch Verwendung von legierten Anoden10.1055/s-0029-1227099 ↗
6. Limitations in the determination of total filtration of x-ray tube assemblies10.1088/0031-9155/33/2/006 ↗
7. Measurement of the x-ray tube anodes’ surface profile and its effects on the x-ray spectra10.1118/1.3056464 ↗
8. Monte Carlo simulation of the effects of anode surface roughness on x-ray spectra10.1118/1.3495541 ↗
9. Simulation of the effect of anode surface roughness on diagnostic x-ray spectra10.1088/0031-9155/47/22/305 ↗
10. Quantifying the effect of anode surface roughness on diagnostic x-ray spectra using Monte Carlo simulation10.1118/1.3284212 ↗
11. Solution softening mechanism of iridium and rhenium in tungsten at room temperature10.1016/0263-4368(91)90028-M ↗
12. Effect of rhenium on the dislocation core structure in tungsten10.1103/PhysRevLett.104.195503 ↗
13. Solute-induced solid-solution softening and hardening in bcc tungsten10.1016/j.actamat.2017.09.019 ↗
14. Ductilisation of tungsten (W) through cold-rolling: R-curve behaviour10.1016/j.ijrmhm.2016.03.006 ↗
15. Lassner · 1999
16. The alloys of rhenium with molybdenum or with tungsten and having good high temperature properties
17. Mechanical properties of dilute tungsten-rhenium alloys
18. Superplasticity in Tungsten-Rhenium Alloys
19. Yielding and fracture in tungsten and tungsten-rhenium alloys10.1016/0022-5088(69)90047-2 ↗
20. Thermal expansion coefficient of WRe alloys from first principles10.1103/PhysRevB.96.035148 ↗
21. Temperature dependence of thermal conductivity in W and W-re alloys from 300 to 1000 K10.1016/S0167-577X(02)01403-9 ↗
22. Tungsten and CFC degradation under combined high cycle transient and steady state heat loads10.1016/j.fusengdes.2012.02.106 ↗
23. Wirtz · 2017
24. Wirtz · 2013 · 130
25. Performance of the different tungsten grades under fusion relevant power loads10.1016/S0022-3115(00)00668-1 ↗
26. Podgoršak · 201610.1007/978-3-319-25382-4 ↗
27. Energy spectra and angular distributions of charged particles backscattered from solid targets10.1088/0022-3727/41/5/055505 ↗
28. Finite Element Analysis of X-Ray Targets
29. Metallographische Praparation von Wolfram und Wolframlegierungen zur Gefugeuntersuchung mittels licht-und rasterelektronenmikroskopischer Methoden
30. A step-by-step analysis of the polishing process for tungsten specimens10.3139/147.110215 ↗
31. Jaffe · 1961
32. Impact of combined transient plasma/heat loads on tungsten performance below and above recrystallization temperature10.1088/0029-5515/55/12/123004 ↗
33. Thermal fatigue mechanism of recrystallized tungsten under cyclic heat loads via electron beam facility10.1016/j.ijrmhm.2016.07.022 ↗
34. Experimental and simulated grain boundary groove profiles in tungsten10.1080/09500830050134345 ↗
35. Effect of faceting on the thermal grain-boundary grooving of tungsten
36. Theory of thermal grooving10.1063/1.1722742 ↗
37. Thermal Grooving by Surface Diffusion: a Review of Classical Thermo-Kinetics Approach, Hittite
38. The surface energy of metals10.1016/S0039-6028(98)00363-X ↗
39. Surface damage and structure evolution of recrystallized tungsten exposed to ELM-like transient loads10.1088/0029-5515/56/3/036021 ↗
40. Tungsten surface morphology control and its thermal fatigue behavior under cyclic heat loading
41. Schijve · 2009
42. Thermal shock response of deformed and recrystallised tungsten10.1016/j.fusengdes.2013.05.077 ↗
43. Effect of rhenium addition on fracture toughness of tungsten at elevated temperatures10.1007/BF00356341 ↗
44. Performance of different tungsten grades under transient thermal loads10.1088/0029-5515/51/7/073017 ↗
45. Grimvall · 1999
46. Rollett · 2004
47. Behavior and microstructural changes in different tungsten-based materials under pulsed plasma loading10.1016/j.nme.2016.06.004 ↗
48. On the Zener drag10.1016/0001-6160(85)90214-7 ↗
49. Study of the pores inside tungsten coating after thermal cycling for fusion device10.1088/0031-8949/T167/1/014060 ↗
50. Tailoring columnar microstructure of axial suspension plasma sprayed TBCs for superior thermal shock performance10.1016/j.matdes.2018.02.011 ↗
51. Micro-engineered first wall tungsten armor for high average power laser fusion energy systems10.1016/j.jnucmat.2005.08.012 ↗
52. E. Lenz, X-Ray Anode Having An Electron Incident Surrface Scored by Microslits. US Patent, US7079625B2, 2006.
53. J. Freudenberger, Focal Track of a Rotating Anode Having a Microstructure. US Patent, US20130170624A1, 2013.
54. Thermal shock performance of CVD tungsten coating at elevated temperatures10.1016/j.jnucmat.2014.07.021 ↗
55. Influence of surface morphology and microstructure on performance of CVD tungsten coating under fusion transient thermal loads10.1016/j.apsusc.2016.08.060 ↗
56. Effects of transition metals on the grain boundary cohesion in tungsten10.1016/j.scriptamat.2012.01.002 ↗
57. Effect of Hf additions on phase stability and mechanical properties of binary W-Hf alloys: a first-principles study10.1016/j.fusengdes.2018.10.007 ↗
58. Scheiber · 2016
59. S. Foldes, Tungsten Hafnium Oxygen Alloys. US Patent, US3434811A, 1969.
60. Mechanical Properties of solid solution and carbide strenghtened arc melted tungsten alloys
61. Fabricating high performance tungsten alloys through zirconium micro-alloying and nano-sized yttria dispersion strengthening10.1016/j.jnucmat.2014.03.029 ↗
62. On the diffusion of scandium and hafnium in tungsten10.1016/S0921-4526(98)00441-4 ↗
63. High temperature diffusion of hafnium in tungsten and a tungsten-hafnium carbide alloy10.1016/0956-716X(94)90256-9 ↗