journal article·2004-01

M6C formation during sintering of cemented carbides containing (Ti,W)C

A. Petersson, B. Jansson, J. Qvick, J. Zackrisson

Publisher page

Abstract

Abstract The temporary formation of M 6 C during sintering of cemented carbides containing the cubic carbide (Ti,W)C is shown in samples exposed to interrupted sintering cycles. The M 6 C, revealed by magnetic-saturation measurements, X-ray diffraction and microscopy, is formed during the initial stage of sintering, but is dissolved as sintering proceeds. The overall carbon content does not change much between the sintering temperatures. It is believed that the initially nearly stoichiometric (Ti,W)C releases carbon due to its equilibrium carbon content decreasing with increasing temperature, which makes dissolution possible. The temporary M 6 C would not normally be detected, since sample characterisation is in practice employed only after sintering.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. A study of the effect of carbon content on the structure and properties of sintered WC–Co alloys
2. Phase equilibria and the sintering of cemented carbides
3. Charakterisierung der Bindephase von WC–Co Hartmetallen über magnetische Eigenschaften
4. The Thermo-Calc databank system10.1016/0364-5916(85)90021-5 ↗
5. Development of a database for cemented carbides: thermodynamic modeling and experiments10.1007/s11669-001-0028-8 ↗
6. Mechanism of solid-state dissolution of WC in Co-based solutions10.1016/S1359-6454(02)00011-3 ↗
7. Sarin VK. Morphology of eta phase in cemented WC–Co alloys. In: Hausner HH, Taubenblat PV, editors. Modern developments in powder metallurgy, vol. 10. Ferrous and Non-ferrous P/M Materials, Princeton, New Jersey, 1977. p. 553–65
8. Solid state sintering of cemented carbides––an experimental study
9. Role of the binder phase in cemented tungsten carbide–cobalt alloys
10. Microstructure evolution in the cemented carbides WC–Co I. Effect of the C/W ratio on the morphology and defects of the WC grains10.1002/1521-396X(200209)193:2<271::AID-PSSA271>3.0.CO;2-O ↗
11. W content in Co binder during sintering of WC–Co10.1016/S1359-6454(97)00459-X ↗