Effects of filler materials on the microstructural characteristics and mechanical properties of laser-welded lap joints of TZM alloys
Source abstract
Abstract
The poor weldability of molybdenum (Mo) alloys has always been the main problem that impedes their application as large-sized structural components. Two types of laser-welded lap joints, namely LW-Ti and LW-Nb joints, were prepared using titanium (Ti) and niobium (Nb) as filler materials to investigate the alterations in microstructures and mechanical properties of TZM (Mo-0.5Ti-0.08Zr-0.02C) alloy joints. The results indicate that both Ti and Nb have excellent metallurgical compatibility with Mo, resulting in well-formed joints. Due to solid-solution strengthening, the microhardness of the fusion zone (FZ) significantly increases from 269.9 HV to 397.1 HV for LW-Ti joints and reaches 389.6 HV for LW-Nb joints. Furthermore, the shear strength of LW-Ti joints is approximately 2.05 times that of LW-Nb joints, measuring at 110.97 MPa. Fractures in LW-Ti joints primarily occur at the base metal (BM) and display lamellar ductile fracture characteristics, while fractures in LW-Nb joints mainly occur at the FZ and exhibit coarse brittle intergranular fractures. The mechanical properties of LW-Nb joints are compromised due to the larger maximum pore diameter (300 μm) in the FZ compared to LW-Ti joints (50 μm), which can be attributed to the higher viscosity of liquid niobium. Additionally, the average grain size in the FZ of LW-Nb joints (86.37 μm) is larger than that in LW-Ti joints (53.28 μm). The reduction in grain size observed in LW-Ti joints also increases the grain boundary area, decreases oxygen concentration along the grain boundaries, and enhances binding strength at Mo grain boundaries. Given Ti`s stronger affinity for oxygen compared to Mo, the abundant formation of second-phase TiO 2 particles within LW-Ti joints hinders the specific formation of MoO 2 along grain boundaries. Consequently, the proposed welding technology was employed to weld a large-scale cylinder-flange component made from Mo alloy, which is expected to greatly facilitate the widespread utilization of welded structures made from Mo alloys.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Traditional and emerging applications of molybdenum metal and its alloys[J]
2. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility[J]10.1038/nmat3544 ↗
3. Fracture and ductile-to-brittle transition characteristics of molybdenum by impact and static bend tests[J]10.2320/matertrans1989.36.504 ↗
4. Effects of titanium and carbon on cohesion property and brittleness of grain boundary of molybdenum[J]10.1016/j.ssc.2022.114963 ↗
5. Oxygen content effect on mechanical properties and microstructure of TZM alloy[J]
6. Microstructure and mechanical properties of molybdenum-titanium-zirconium-carbon alloy TZM processed via laser powder-bed fusion[J]10.1016/j.ijrmhm.2020.105369 ↗
7. Microstructure evolution and formation mechanism of γ-TiAl/Ni-based superalloy laser-welded joint with Ti/V/cu filler metals[J]10.1016/j.matlet.2022.133647 ↗
8. Microstructure development of molybdenum during rotary friction welding[J]10.1016/j.matchar.2019.03.024 ↗
9. Microstructural characterization and mechanical properties of Ti3Al-Nb/ Ni-based superalloy laser-welded joints with different type of V/cu composite interlayers [J]10.1016/j.optlastec.2022.108736 ↗
10. Microstructure transformation and pore formation mechanism of Mo-14Re alloy weld by vacuum electron beam welding[J]10.1016/j.vacuum.2023.112594 ↗
11. Microstructure evolution and embrittlement of electron beam welded TZM alloy joint[J]10.1016/j.msea.2017.05.076 ↗
12. Stress relief and purification mechanisms for grain boundaries of electron beam welded TZM alloy joint with zirconium addition[J]10.1016/j.jmatprotec.2017.08.031 ↗
13. Analysis of microstructure and mechanical strength of lap joints of TZM alloy welded by a fiber laser[J]10.1016/j.jmapro.2019.02.015 ↗
14. Characterization of Armour steel welds using austenitic and ferritic filler metals[J]10.1007/s12666-021-02464-7 ↗
15. A state of the art review of fillet welded joints[J]10.3390/ma15248743 ↗
16. Influence of processing window on laser welding-brazing of Al to press-hardened 22MnB5 steel[J]10.1016/j.optlastec.2020.106566 ↗
17. The influence of laser power on microstructure and properties of laser welding-brazing of Al alloys to Al-Si coated 22MnB5 steel[J]10.1016/j.optlastec.2023.109318 ↗
18. The effect of molybdenum content on the microstructural evolution and tensile properties of as-cast Ti-Mo alloys[J]
19. Microstructural and mechanical properties of Ti-Mo alloys designed by the cluster plus glue atom model for biomedical application[J]10.1007/s00170-020-06208-7 ↗
20. Effects of minor Zr addition on the microstructure and mechanical properties of laser welded dissimilar joint of titanium and molybdenum[J]10.1016/j.msea.2018.10.037 ↗
21. Effects of titanium on grain boundary strength in molybdenum laser weld bead and formation and strengthening mechanisms of brazing layer[J]10.1016/j.matdes.2019.107681 ↗
22. Ductile Nb alloys with reduced density and cost[J]10.1016/j.jallcom.2019.151685 ↗
23. A new approach to understand the deformation behavior and strengthening mechanism of molybdenum alloy: from single crystal to polycrystal[J]10.1016/j.ijrmhm.2021.105715 ↗
24. Effect of niobium on the mechanical strength of the laser beam welding joints of molybdenum[J]10.1016/j.ijrmhm.2023.106207 ↗
25. Mechanism of Zn coating on the wettability, spreadability, and microstructure of Al/steel with the laser welding–brazing method[J]10.1007/s11661-020-05637-z ↗
26. Interface characterization and mechanical properties of dual beam laser welding-brazing Al/steel dissimilar metals[J]10.1016/j.jmapro.2019.03.005 ↗
27. Numerical study of keyhole dynamics and keyhole-induced porosity formation in remote laser welding of Al alloys[J]10.1016/j.ijheatmasstransfer.2016.12.019 ↗
28. Numerical study of keyhole instability and porosity formation mechanism in laser welding of aluminum alloy and steel[J]10.1016/j.jmatprotec.2017.10.011 ↗
29. Effect of heat input on porosity defects in a fiber laser welded socket-joint made of powder metallurgy molybdenum alloy[J]10.3390/ma12091433 ↗
30. Non-contact measurements of surface tension and viscosity of niobium, zirconium, and titanium using an electrostatic levitation furnace[J]10.1023/A:1015459222027 ↗
31. Regulation of performance of laser-welded socket joint of Mo–14Re ultra-high-temperature heat pipe by introducing Ti into both weld and heat affected zone[J]10.1016/j.jmrt.2022.11.162 ↗
32. Enhanced mechanical performance of fusion zone in laser beam welding joint of molybdenum alloy due to solid carburizing[J]10.1016/j.matdes.2019.107957 ↗
33. Interdiffusion in the β Mo–Ti solid solution at high temperatures[J]
34. Laser beam oscillating welding of 5A06 aluminum alloys: microstructure, porosity and mechanical properties[J]10.1016/j.optlastec.2018.09.036 ↗
35. Mitigation of porosity defects in fiber laser welding under low vacuum[J]10.1016/j.jmatprotec.2019.116385 ↗