Structure analysis of the constitutional phases in liquid phase sintered W–Mo–Ni–Fe heavy alloys
Source abstract
Abstract
Abstract The crystal structures of constitutional phases in two different tungsten heavy alloys processed via different conditions were examined. The compositions of these two alloys were W–11.9Mo–17.0Ni–7.7Fe and W–29.6Mo–17.0Ni–7.7Fe (at.%), which were liquid phase sintered at 1500 °C for 5 or 240 min, and followed by either furnace-cooling or water-quenching. Increase in isothermal hold caused increased concentration of Mo but decreased concentration of W in the matrix phase, which did not affect the lattice parameter of the matrix phase to a significant extent. Quenching the specimen in water caused increase in the concentrations of both W and Mo in the matrix phase, and, consequently, increases in the lattice parameter of the matrix phase. A tungsten heavy alloy with a high alloying concentration of Mo was prone to induce the precipitation of an intermetallic phase during cooling, which was enhanced by increasing the isothermal hold at the liquid phase sintering temperature and decreasing the cooling rate. The structure of this intermetallic phase is analogous to that of MoNi, and can be designated as (WxMo1−x)(FeyNi1−y). The composition of this intermetallic phase varied with the composition of the alloy and its cooling rate subsequent to sintering. For a furnace-cooling condition, the atomic ratio of W to Mo (x/1−x) in this intermetallic phase was about 0.47 times the atomic ratio of W to Mo of the original alloy composition. Such a proportional constant decreased to about 0.30 when the specimen was water-quenched.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. On a new intermetallic phase in the nickel–tungsten system10.1007/BF02644589 ↗
2. Interfacial embrittlement in liquid-phase sintered tungsten heavy alloys10.1007/BF02658336 ↗
3. Segregation to interphase boundaries in liquid-phase sintered tungsten heavy alloys10.1007/BF02643782 ↗
4. Some structural characteristics of the binder phase of W–Ni–Fe alloys
5. Interphase boundary precipitation in liquid phase sintered W–Ni–Fe and W–Ni–Cu alloys10.1007/BF02644702 ↗
6. Precipitation at tungsten/tungsten interfaces in tungsten–nickel–iron alloys10.1179/pom.1986.29.1.45 ↗
7. Sintering atmosphere effects on tensile properties of heavy alloys10.1007/BF02645474 ↗
8. Rhenium alloying of tungsten heavy alloys
9. Matrix composition effect on the tensile properties of tungsten–molybdenum heavy alloys10.1007/BF02698261 ↗
10. Grain growth in liquid-phase-sintered W–Mo–Ni–Fe alloys10.1016/0022-5088(91)90022-V ↗
11. Microstructural evolution on the sintered properties of W–8pctMo–7pctNi–3pctFe alloy10.1023/A:1004812910331 ↗
12. Interfacial reaction-controlled reprecipitation of W atoms in liquid matrix phase during the sintering of W–8PctMo–7pctNi–3pctFe10.1007/s11661-998-0195-x ↗
13. Segregation of molybdenum atoms to the liquid–solid interfaces in liquid phase sintering of W–8PctMo–7pctNi–3pctFe
14. Variables on the precipitation of an intermetallic phase for liquid phase sintered W–Mo–Ni–Fe heavy alloys10.1016/S0263-4368(02)00072-0 ↗
15. Precipitation of an intermetallic phase in Mo-alloyed tungsten heavy alloys10.2320/matertrans.44.358 ↗
16. Williams · 1996
17. Nash · 1991
18. X-ray diffraction studies of the δ phase, Mo–Ni10.1107/S0365110X60001400 ↗
19. The crystal structure of the δ phase, Mo–Ni10.1107/S0365110X63002668 ↗
20. Electron microscopy study of the δ-NiMo phase in a binary Ni–Mo alloy10.1016/0167-577X(95)00006-2 ↗
21. Lin KH, Hsu CS, Lin ST. Precipitation mechanism of a MoNi type intermetallic phase in W–27.0at.%Mo–35.6at.%Ni–17.6at.%Fe. Int J Refr Metals Hard Mater (Accepted)10.1016/S0263-4368(03)00008-8 ↗
22. Nagender Naidu · 1991
23. Villars · 1995 · vol. 1
24. Villars · 1995 · vol. 2
25. Villars · 1995 · vol. 8
26. Villars · 1995 · vol. 10