In situ synthesized Ti5Si3/Ti–Mo lightweight structural composites
Source abstract
Abstract
Abstract Ti–Si and Ti–Mo alloys are considered to be potential high-temperature structural materials, thus it is interesting to develop new materials from Ti–Mo–Si ternary system by utilizing the strengthening mechanisms of both binary systems. In the present work, a series of composites in which Ti solid solution (partially substituted by Mo) matrix is reinforced by the eutectic cell Ti 5 Si 3 + Ti have been in situ synthesized by using non-consumable vacuum arc melting. The composites exhibit the hypoeutectic microstructure consisting of primary α- or β-(Ti, Mo) solid solution and the fine eutectic cell. Besides the strengthening effect of Ti 5 Si 3 compound, Mo element plays an important role in the composites through solid solution hardening, phase transformation hardening and fine grain hardening. All the above factors result in the significant improvement of mechanical properties, i.e. the yield strength increases from 768.54 MPa to 1450.62 MPa when Mo content changes from 0 to 10 at.%. Although some brittle characteristics can be found on the fractured surfaces of the Mo-added samples, relatively high plasticity is obtained in all the in situ Ti 5 Si 3 /Ti–Mo composites, which guarantees the application of these composites as structural materials.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Microstructure and properties of a laser fabricated burn-resistant Ti alloy10.1016/j.matdes.2003.10.004 ↗
2. The phase relationships in the La–Ti–Sn ternary system at 473K10.1016/j.jallcom.2007.04.294 ↗
3. A review on particulate-reinforced titanium matrix composites
4. Processing-structure–property aspects of particulate- and whisker-reinforced titanium matrix composites10.1016/j.compscitech.2007.07.016 ↗
5. The 473K isothermal section of the Cu–Ti–Sn ternary system10.1016/j.jallcom.2009.02.074 ↗
6. Corrosion resistance, mechanical properties, corrosion fatigue strength and cytocompatibility of new Ti alloys without Al and V10.1016/S0142-9612(97)00235-4 ↗
7. Evolution of the microstructure and hardness of the Ti–Si alloys during high temperature heat-treatment10.1016/j.jallcom.2009.01.017 ↗
8. Influence of tin on the structure and properties of as-cast Ti-rich Ti–Si alloys10.1016/S0925-8388(02)00971-4 ↗
9. Microstructure and compressive properties of in situ synthesized Ti–Si alloy composites reinforced with La2O3 particles10.1016/j.msea.2009.07.024 ↗
10. High volume intermetallics reinforced Ti-based composites in situ synthesized from Ti–Si–Sn ternary system10.1016/j.msea.2011.01.104 ↗
11. Microstructure and elastic modulus of Ti–Nb–Si ternary alloys for biomedical applications10.1016/j.scriptamat.2005.11.001 ↗
12. Deformation induced martensite and superelasticity in a β-metastable titanium alloy10.1016/S0921-5093(00)00921-7 ↗
13. Aging response of the Ti–Nb system biomaterials with β-stabilizing elements10.1016/j.matdes.2010.05.047 ↗
14. Microstructures and properties of titanium alloys Ti–Mo for dental use10.1016/S1003-6326(06)60308-7 ↗
15. Martensitic transformations in Ti–Mo alloys10.1007/BF00772735 ↗
16. Microstructures and properties of titanium alloys Ti–Mo for dental use10.1016/S1003-6326(06)60308-7 ↗
17. Murray · 1987
18. Tsai · 1980 · 455
19. Lutjering · 2007 · 1
20. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗
21. The cleavage strength of polycrystals