Enhanced sintering of tungsten
Source abstract
Abstract
W and W-La 2O 3 powders with a range of particle sizes were processed by furnace sintering, direct resistance sintering, and spark plasma sintering to determine the effects of current and pressure on densification and grain size. The results from these experiments are combined with experimental data from literature and compared to a model for densification based on master sintering curve concepts to assess the effectiveness of finer particle sizes, the application of current, and the combined application of current and pressure for achieving sintered densities above 96% of theoretical for pure tungsten and for tungsten containing small amounts of oxides and/or carbides. Experimental results for grain size are also compared to the model predictions for pressureless sintering. The same model is used to assess the effectiveness of transition metal additions, the application of pressure, and the application of electromagnetic radiation on enhancing the sintering of tungsten and refining its grain size.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (95)
Show source-provided references
1. Leichtfried · 2015 · 605
2. Yih · 1979
3. Lassner · 1999
4. Master sintering curve: a practical approach to sintering10.1111/j.1151-2916.1996.tb08097.x ↗
5. Strength predictions for bulk structures fabricated from nanoscale tungsten powders10.1016/j.ijrmhm.2004.10.002 ↗
6. Mapping the compaction and sintering response of tungsten-based materials into the nanoscale range10.1016/j.ijrmhm.2005.03.002 ↗
7. Progress in processing nanoscale refractory and hardmetal powders
8. Activated liquid phase sintering of W–Cu and Mo–Cu10.1016/j.ijrmhm.2015.04.030 ↗
9. Powder injection molding of tungsten components for a He-cooled divertor
10. Study of size-dependent sintering behavior of tungsten powders
11. Sinter-ability of nanocrystalline tungsten powder10.1016/j.ijrmhm.2009.11.003 ↗
12. The relationship between the green density and as-sintered density of nano-tungsten compact10.1016/j.ijrmhm.2015.07.006 ↗
13. The sintering behavior of nanosized tungsten powder prepared by a plasma process10.1016/j.ijrmhm.2008.11.004 ↗
14. Dimension precision of metal injection molded pure tungsten10.1016/j.ijrmhm.2008.10.003 ↗
15. Powder injection molding for mass production of He-cooled divertor parts10.1016/j.jnucmat.2010.12.122 ↗
16. Micro/nano composited tungsten material and its high thermal loading behavior10.1016/j.jnucmat.2014.09.037 ↗
17. The study on low temperature sintering of nanotungsten powders10.1016/j.ijrmhm.2016.10.003 ↗
18. Mechanical and microstructural investigations of tungsten and doped tungsten materials produced via powder injection molding10.1016/j.nme.2015.04.002 ↗
19. Injection molding of tungsten powder treated by jet mill with high powder loading: a solution for fabrication of dense tungsten component at relative low temperature10.1016/j.ijrmhm.2016.10.015 ↗
20. Development of tungsten components for langmuir probes in ITER by metal injection molding
21. Effect of boron on microstructure and fracture of sintered ultrafine-grained tungsten10.1007/s11837-018-3060-4 ↗
22. Preparation of intragranular-oxide-strengthened ultrafine-grained tungsten via low-temperature pressureless sintering10.1016/j.msea.2019.138878 ↗
23. Thermal stability and grain growth kinetics of ultrafine-grained W with various amount of La2O3 addition10.1007/s11661-020-05836-8 ↗
24. Effect of La2O3 addition on the synthesis of tungsten nanopowder via combustion-based method10.1016/j.jmst.2020.03.069 ↗
25. Effect of La2O3 content on the densification, microstructure and mechanical property of W-La2O3 alloy via pressureless sintering10.1016/j.matchar.2021.111092 ↗
26. Spark plasma sintering of tungsten and lanthanated tungsten
27. The effect of Y2O3 on the grain growth and densification of W matrix during low temperature sintering: experiments and modelling10.1016/j.matdes.2019.108080 ↗
28. Microstructure and properties of La2O3 doped W composites prepared by a wet chemical process10.1016/j.ijrmhm.2017.04.004 ↗
29. The influence of modification route on the properties of W-0.3 wt% Y2O3 powder and alloy prepared by nano-in-situ composite method10.1016/j.jallcom.2018.09.163 ↗
30. The activated sintering of tungsten with group VIII elements10.1149/1.2425876 ↗
31. Liquid phase and activated sintering
32. Activated and liquid phase sintering - progress and problems
33. Enhanced sintering through second phase additions10.1179/pom.1985.28.1.7 ↗
34. Enhanced low-temperature sintering of tungsten10.1007/BF02659818 ↗
35. A generalized model for the prediction of periodic trends in the activation of sintering of refractory metals
36. The properties of tungsten processed by chemically activated sintering10.1007/BF02662370 ↗
37. A modified model for the sintering of tungsten with nickel additions10.1016/0022-5088(72)90025-2 ↗
38. The effect of nickel and palladium additions on the activated sintering of tungsten
39. Systematic trends in the chemically activated sintering of tungsten, high temperature
40. Enhanced sintering of tungsten - phase equilibria effects on properties
41. The sintering and strength of coated and co-reduced nickel tungsten powder
42. Activated sintering of tungsten with palladium additions10.1007/BF00774071 ↗
43. Activated sintering of tungsten with nickel additions10.1007/BF00774544 ↗
44. Activation of the sintering of tungsten by the iron-group metals10.1007/BF00778338 ↗
45. Activation of the sintering process of tungsten by the platinum-group metals10.1007/BF00796945 ↗
46. A contribution to the study of the electronic mechanism of the activated sintering of tungsten
47. Theoretical modeling of activated solid-state sintering10.1007/BF02648421 ↗
48. The effect of Ni doping on the mechanical behavior of tungsten10.1016/j.ijrmhm.2020.105281 ↗
49. Investigations of the nickel promotional effect on the reduction and sintering of tungsten compounds10.1016/j.ijrmhm.2018.10.008 ↗
50. New insights into the accelerated sintering of tungsten with trace nickel addition10.1016/j.ijrmhm.2019.105139 ↗
51. 100 years of doped tungsten wire10.1016/j.ijrmhm.2010.05.003 ↗
52. Hot pressing of tungsten and its pseudoalloys10.1007/BF00798021 ↗
53. Thermomechanical properties of TiC particle-reinforced tungsten composites for high temperature applications10.1016/S0263-4368(02)00105-1 ↗
54. Microstructure and mechanical properties of tungsten composites co-strengthened by dispersed TiC and La2O3 particles10.1016/j.ijrmhm.2007.12.004 ↗
55. Microstructure and impact properties of ultra-fine grained tungsten alloys dispersed with TiC10.1016/S0022-3115(98)00753-3 ↗
56. Characterization of novel W alloys produced by HIP10.1016/j.jnucmat.2008.12.217 ↗
57. Development of tungsten and tungsten alloys for DEMO divertor applications via MIM technology10.1016/j.jnucmat.2013.01.004 ↗
58. Tungsten–vanadium–yttria alloys for fusion power reactors (I): microstructural characterization10.1016/j.ijrmhm.2015.07.032 ↗
59. Tungsten–vanadium–yttria alloys for fusion power reactors (II): mechanical characterization10.1016/j.ijrmhm.2015.07.031 ↗
60. In situ oxide dispersion strengthened tungsten alloys with high compressive strength and high strain-to-failure10.1016/j.actamat.2016.09.034 ↗
61. Production of nanocrystalline tungsten using ultra-high-pressure rapid hot consolidation (UPRC)
62. Plasma pressure compaction (P2C) of submicron size tungsten powder
63. Fabrication of high temperature oxides dispersion strengthened tungsten composites by spark plasma sintering process10.1016/j.ijrmhm.2009.03.003 ↗
64. Fabrication and characterization of ultra-fine grained tungsten by resistance sintering under ultra-high pressure10.1016/j.msea.2008.11.012 ↗
65. Multimodal grain size distribution and high hardness in fine grained tungsten fabricated by spark plasma sintering10.1016/j.msea.2011.04.015 ↗
66. Chemically produced nanostructured ODS–lanthanum oxide–tungsten composites sintered by spark plasma10.1016/j.jnucmat.2010.10.060 ↗
67. Sintering of tungsten powder with and without tungsten carbide additive by field assisted sintering technology10.1016/j.ijrmhm.2011.09.014 ↗
68. Kinetics of densification and grain growth of pure tungsten during spark plasma sintering10.1007/s11663-012-9704-9 ↗
69. Basic characterization of oxide dispersion strengthened fine-grained tungsten based materials fabricated by mechanical alloying and spark plasma sintering10.1016/j.jnucmat.2011.11.039 ↗
70. The effect of HfC content on mechanical properties HfC–W composites10.1016/j.ijrmhm.2014.01.012 ↗
71. Microstructure and mechanical properties of W-Ta and W-Ta-TiC alloys sintered by field assisted sintering technique
72. Room and ultrahigh temperature structure-mechanical property relationships of tungsten alloys formed by field assisted sintering technique (FAST)10.1016/j.msea.2016.06.006 ↗
73. Grain growth behavior and mechanical properties of zirconium micro-alloyed and nano-size zirconium carbide dispersion strengthened tungsten alloys10.1016/j.ijrmhm.2015.03.019 ↗
74. Effect of hot rolling and annealing on the mechanical properties and thermal conductivity of W-0.5 wt.% TaC alloys10.1016/j.ijrmhm.2015.12.004 ↗
75. Recent progress on the R&D of W-ZrC alloys for plasma facing components in fusion devices10.1016/j.nme.2018.07.002 ↗
76. Densification mechanism and mechanical properties of tungsten powder consolidated by spark plasma sintering10.1016/j.ijrmhm.2016.07.023 ↗
77. Toughness and microstructure of tungsten fibre net-reinforced tungsten composite produced by spark plasma sintering10.1016/j.msea.2016.02.034 ↗
78. Fabrication of sintered tungsten by spark plasma sintering and investigation of thermal stability10.1016/j.ijrmhm.2017.08.013 ↗
79. Spark plasma sintering of pure tungsten powder: densification kinetics and grain growth10.1016/j.powtec.2017.01.050 ↗
80. Electromigration-enhanced densification kinetics during spark plasma sintering of tungsten powder10.1007/s11661-019-05201-4 ↗
81. The effect of particle size on the densification kinetics of tungsten powder during spark plasma sintering10.1016/j.ijrmhm.2020.105358 ↗
82. Microstructural and compositional effects of transition metal carbide additions on dispersion-strengthened tungsten fabricated via spark plasma sintering10.1016/j.ijrmhm.2018.04.015 ↗
83. Effect of ZrO2 content on microstructure and mechanical properties of W alloys fabricated by spark plasma sintering10.1016/j.ijrmhm.2018.11.006 ↗
84. Assessment of mechanical properties of SPS-produced tungsten including effect of neutron irradiation10.1016/j.ijrmhm.2020.105207 ↗
85. Spark plasma sintering of tungsten–yttrium oxide composites from chemically synthesized nanopowders and microstructural characterization10.1016/j.jnucmat.2011.03.007 ↗
86. Microstructure and helium irradiation performance of W–ZrC/Sc2O3 composites prepared spark plasma sintering10.1016/j.ijrmhm.2018.01.011 ↗
87. Densification and microstructure evolution of W-TiC-Y2O3 during spark plasma sintering10.1016/j.ijrmhm.2018.11.014 ↗
88. Microwave sintering: a new approach to fine-grain tungsten - I
89. Microwave sintering: a new approach to fine-grain tungsten - II
90. Microwave sintering of tungsten10.1016/j.ijrmhm.2008.07.001 ↗
91. The study on the microwave sintering of tungsten at relatively low temperature10.1016/j.jnucmat.2011.11.012 ↗
92. High performance tungsten synthesized by microwave sintering method10.1016/j.ijrmhm.2012.02.016 ↗
93. Balling phenomena in selective laser melted tungsten10.1016/j.jmatprotec.2015.02.032 ↗
94. Effect of process parameters on the selective laser melting (SLM) of tungsten10.1016/j.ijrmhm.2017.11.035 ↗
95. Selective laser melting of tungsten and tungsten alloys10.1016/j.ijrmhm.2017.12.005 ↗