Effects of lanthanum oxide content on mechanical properties of mechanical alloying Mo–12Si–8.5B (at.%) alloys
Source abstract
Abstract
Abstract Mo–12Si–8.5B alloys with different mass fraction (0 wt.%, 0.3 wt.%, 0.9 wt.%, 1.5 wt.%, 2.5 wt.%) lanthanum oxide (La 2 O 3 ) additive were fabricate by using mechanical alloying and hot pressing sintering techniques. XRD results indicate that the doped Mo–12Si–8.5B alloys are consisted mainly of α-Mo, Mo 3 Si and Mo 5 SiB 2 (T2) phases. It is found that addition of La 2 O 3 has little effect on both the grains and intermetallic sizes. The intermetallic particles are more homogeneously dispersed within α-Mo matrix by increasing the La 2 O 3 content. Compression test and three-point bending test showed that both compression and flexure strength of alloys were obviously improved by the addition of La 2 O 3 . The predominant strengthening mechanisms are fine-grain strengthening and particles dispersion strengthening. In addition, fracture toughness tests showed that the fracture toughness values of all alloys were on the order of 9 MPa·m 1/2 that revealed the addition of La 2 O 3 had little effect on improving the alloys toughness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Processing and mechanical properties of a molybdenum silicide with the composition Mo–12Si–8.5B10.1016/S0966-9795(00)00093-5 ↗
2. Ambient to high temperature fracture toughness and fatigue-crack propagation behavior in a Mo–12Si–8.5B (at.%) intermetallic10.1016/S0966-9795(01)00008-5 ↗
3. Oxidation behavior of Mo5SiB2-based alloy at elevated temperature10.1016/S0966-9795(02)00013-4 ↗
4. Oxidation behavior of extruded Mo5Si3Bx–MoSi2–MoB intermetallics from 600°C–1600°C10.1016/S0966-9795(02)00034-1 ↗
5. Oxidation behavior of αMo–Mo3Si–Mo5SiB2 (T2) three phase system10.1016/S0966-9795(01)00118-2 ↗
6. On the fracture and fatigue properties of Mo–Mo3Si–Mo5SiB2 refractory intermetallic alloys at ambient to elevated temperature (25°C to 1300°C)10.1007/s11661-003-0325-4 ↗
7. Transient oxidation of Mo–Si–B alloys: effect of the microstructure size scale10.1016/j.actamat.2009.06.036 ↗
8. Synthesis of α-Mo–Mo5SiB2–Mo3Si nanocomposite powders by two-step mechanical alloying and subsequent heat treatment10.1016/j.jallcom.2011.05.066 ↗
9. Mechanically alloyed Mo–Si–B alloys with a continuous α-Mo matrix and improved mechanical properties10.1016/j.intermet.2008.04.015 ↗
10. Structural materials: metal–silicon–boron: on the melting behavior of Mo–Si–B alloys10.1016/S0925-8388(02)00676-X ↗
11. Microstructure and mechanical properties of lanthanum oxide-doped Mo–12Si–8.5B(at%) alloys
12. Fracture toughness of sintered Mo–La2O3 alloy and the toughening mechanism10.1016/S0263-4368(99)00030-X ↗
13. Microstructure and oxidation resistance behavior of lanthanum oxide-doped Mo–12Si–8.5B alloys10.1016/j.ijrmhm.2011.06.003 ↗
14. A Mo–Si–B intermetallic alloy with a continuous α-Mo matrix10.1016/S1359-6462(01)01227-1 ↗
15. On the fracture toughness of fine-grained Mo–3Si–1B (wt.%) alloys at ambient to elevated (1300°C) temperatures10.1016/j.intermet.2011.09.003 ↗