Study on the effectiveness of WS2 and CaF2 on the performances of self-lubricating micro impregnated diamond bits
Source abstract
Abstract
Abstract Self-lubricating micro impregnated diamond bits (IDBs) were manufactured for the first time via hot-pressing powder metallurgy to investigate the effectiveness of two promising solid lubricant additives, WS2 and CaF2, in improving IDBs' self-lubricating and drilling performances through laboratory drilling test and micro analyses. It was found that, with increase in lubricant concentration, the rate of penetration (ROP) of WS2 IDBs increased exponentially, while that of the CaF2 IDBs decreased monotonically from its maximum value at 6 vol% CaF2 concentration. For WS2 IDBs, the increase in ROP was at the sacrifice of substantial deterioration of IDBs' service life, while the service life of CaF2 IDBs gradually increased to surpass that of lubricant-free IDBs at 8 vol% CaF2 addition and continued to grow. Micro analyses, including measurement of diamond protrusion height and micro morphological analysis of IDBs' worn surface, were conducted using a confocal laser scanning microscopy (CLSM). The 10 vol% CaF2 IDBs were found under good protection from either matrix or diamond wear. By contrast, the surface of the 6 vol% WS2 IDBs suffered severe wear. Based on CLSM images, it was inferred that the high ROP and low service life of WS2 IDBs were a result of enhanced three-body abrasive wear by breakaway diamond grits. In general, self-lubricating IDBs with 10 vol% CaF2 addition acquired best overall performances in that they achieved longest service life while having higher ROP than lubricant-free IDBs.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Study on friction and wear properties of self-lubricating impregnated diamond bit cutters10.4028/www.scientific.net/SSP.175.136 ↗
2. Effect of CaF2 and hBN on the mechanical and tribological properties of Fe-based impregnated diamond bit matrix10.1016/j.ijrmhm.2018.04.011 ↗
3. Maximizing BHA durability/reliability: turbodrill/impregnated bit significantly reduces drilling time in granite wash laterals
4. Turbodrilling system and diamond-impregnated bit saved three trips in a hard carbonate reservoir
5. Diamond-impregnated drillbit performance in the lower basalt series offshore the Faroe Islands. A case study based on basalt outcrop testing
6. Innovative impregnated drill-bit design with enhanced durability improves performance in challenging Algerian application
7. Key technologies for well drilling and completion in ultra-deep sour gas reservoirs, Yuanba gasfield, Sichuan basin10.1016/j.ngib.2017.05.011 ↗
8. Gao · 2003 · vol. 27 · 29
9. Development of hot dry rock technology
10. Deep air drilling application to enhance rate of penetration in extremely hard, abrasive and high temperature environment
11. New ideas and technology research on water-saving drilling applied in west droughty area, West China
12. Challenges and methods of drilling on the Moon and Mars
13. Application of solid lubricants in grinding: investigations on graphite sandwiched grinding wheels10.1081/MST-120018959 ↗
14. Self-lubricating behaviors of Al2O3/TiB2 ceramic tools in dry high-speed machining of hardened steel10.1016/j.jeurceramsoc.2004.03.033 ↗
15. Performance of the self-lubricating textured tools in dry cutting of Ti-6Al-4V10.1007/s00170-011-3853-x ↗
16. Influence of granularity of graphite on the properties of self-lubricating impregnated diamond bit
17. Effect of graphite on the friction performance of the diamond bit matrix under low temperature and pressure
18. Effects of MoS2 and WS2 on the matrix performance of WC based impregnated diamond bit10.1016/j.triboint.2018.10.038 ↗
19. Phase reactions and chemical stability of ceramic carbide and solid lubricant particulate additions within sintered high speed steel matrix10.1179/pom.1993.36.4.267 ↗
20. Tribological properties of self-lubricating fluoride-metal composites to 900 Deg C (1650 Deg F)—a review and some new developments10.1115/1.3452648 ↗
21. Self-lubrication of sintered ceramic tools with CaF2 additions in dry cutting10.1016/j.ijmachtools.2005.07.047 ↗
22. Abrasive wear performance of tungsten carbide based self-lubricant cutting tool material10.1016/j.ijrmhm.2015.03.007 ↗
23. WC-Ni-Cr-based self-lubricating composites fabricated by pulsed electric current sintering with addition of WS2 solid lubricant10.1016/j.ijrmhm.2017.03.013 ↗
24. Tribological properties of TiAl matrix self-lubricating composites incorporated with tungsten disulfide and zinc oxide10.1039/C5RA04420K ↗
25. Synergetic lubricating effect of WS2 and Ti3SiC2 on tribological properties of Ni3Al matrix composites at elevated temperatures10.1080/10402004.2014.986353 ↗