Abstract

Microstructure attributes such as solid volume fraction, dihedral angle, initial porosity, and initial pore size are important to densification and distortion control in liquid phase sintering (LPS). In our experiments, these parameters were varied to measure densification and distortion behavior during LPS using W–Ni–Cu alloys. Green compacts were formed using ethylene-bis-stearamide (EBS) as a pore-forming agent with the amount of polymer controlling the initial porosity. Different initial pore sizes were generated by varying the polymer particle size. Dihedral angle was varied by changing the Ni:Cu ratio in the alloys. Finally, the solid:liquid ratio was adjusted via the tungsten content. Dilatometry was employed to measure shrinkage and shrinkage rate during heating. Real time video imaging and quenching experiments isolated the sequence of densification and distortion events in LPS. Distortion was quantified using profiles determined with a coordinate measuring machine (CMM) to calculate a distortion parameter. Sintering results showed that at full densification, initial porosity and pore size have no observable effect on distortion for 80W–16Ni–4Cu alloy while distortion reduces with increasing solid volume fraction and dihedral angle. Microgravity experiments are proposed for further understanding of microstructure effects on densification and distortion in LPS.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. German · 1985
2. Shape distortion in liquid-phase-sintered tungsten heavy alloys10.1007/s11661-998-0235-6 ↗
3. A mathematical model for gravity induced distortion during liquid phase sintering10.1007/BF02663915 ↗
4. German RM. Strength loss and distortion in liquid phase sintering. Adv Powder Metall Particulate Mater 1999, vol. 1. Princeton, NJ: Metal Powder Industries Federation; 1999. p. 3.139–3.151
5. Microstructural effects on distortion and solid–liquid segregation during liquid phase sintering under microgravity conditions10.1007/s11663-998-0145-4 ↗
6. Densification and shape distortion in liquid-phase sintering10.1007/s11661-999-0231-5 ↗
7. Upadhyaya A. A microstructure-based model for shape distortion during liquid phase sintering. Ph.D. Thesis. University Park, PA: The Pennsylvania State University; 1998
8. Densification and structural development in liquid phase sintering10.1007/BF02644699 ↗
9. The effect of porosity on distortion in liquid phase sintered tungsten heavy alloys10.1016/S0263-4368(99)00026-8 ↗
10. German RM. Powder metallurgy science. 2nd ed. Princeton, NJ: Metal Powder Industries Federation; 1994
11. Underwood · 1970
12. Application of percolation theory in predicting shape distortion during liquid phase sintering10.1007/s11661-999-0033-9 ↗
13. The contiguity of liquid phase sintered microstructures10.1007/BF02670329 ↗
14. Riegger H, Pask JA, Exner HE. Sintering processes. New York: Plenum Press; 1980. p. 219–3310.1007/978-1-4899-5301-8_19 ↗
15. Liquid-phase sintering under microgravity conditions10.1007/BF03221459 ↗