journal article·2013-11

Thermal shock behavior of ZrB2–SiC composite ceramics with added TaSi2

Shubin Wang, Cheng Xu, Yongbin Ding, Xinghong Zhang

Publisher page

Abstract

Abstract The thermal shock behavior of ZrB 2 –SiC composite ceramics was remarkably enhanced by the addition of TaSi 2 particles. TaSi 2 enhanced the residual strength within the temperature range resulting from the crack-healing effect, especially at ~ 1400 °C. Residual fracture toughness increased with increasing TaSi 2 content from 1000 °C to 1600 °C. The addition of soft phase TaSi 2 positively affected the toughening mechanism. Considering the consumption of TaSi 2 at ~ 1400 °C, fracture toughness of the TaSi 2 -containing ZrB 2 –SiC based ceramic decreased with increasing temperature. The formation of a compressive stress zone beneath the surface oxide layer increased fracture toughness at 1600 °C. The cohesive structure of the TaSi 2 -containing ZrB 2 -based material inhibited crack formation and retained higher mechanical properties. Apparent surface changes were observed as a result of oxidation after severe thermal shock test. From the viewpoint of thermodynamics, thermal oxidation resistance improved with the addition of TaSi 2 .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. The oxidation kinetics of zirconium diboride and zirconium carbide at high temperatures10.1149/1.2426263 ↗
2. Development and characterization of metal-diboride-based composites toughened with ultra-fine SiC particulates10.1016/j.solidstatesciences.2005.02.007 ↗
3. Oxidation behavior of ZrB2–SiC–ZrO2 ceramic composites in the temperature range of 800–1200°C10.1016/j.matchemphys.2009.04.044 ↗
4. Thermal shock resistance of ZrB2 and ZrB2–30% SiC10.1016/j.matchemphys.2008.05.048 ↗
5. The addition of lanthanum hexaboride to zirconium diboride for improved oxidation resistance10.1016/j.scriptamat.2007.07.036 ↗
6. Ablation behaviors of ultra-high temperature ceramic composites10.1016/j.msea.2007.02.040 ↗
7. Parameters for measuring the thermal shock of ceramic materials with an indentation-quench method10.1016/S0955-2219(01)00504-0 ↗
8. Microstructure and mechanical properties of hot pressed ZrB2–SiCp–ZrO2 composites10.1016/j.matlet.2007.12.006 ↗
9. Thermal shock stress considering dynamical behavior for ultra high temperature ceramic10.1016/j.solidstatesciences.2010.02.012 ↗
10. Effect of graphite flake on microstructure as well as mechanical properties and thermal shock resistance of ZrB2–SiC matrix ultrahigh temperature ceramics10.1016/j.jallcom.2009.04.109 ↗
11. Mechanical properties of short carbon fiber reinforced ZrB2–SiC ceramic matrix composites10.1016/j.matlet.2008.01.076 ↗
12. Preparation of ZrB2 based hybrid composites reinforced with SiC whiskers and SiC particles by hot-pressing10.1016/j.ijrmhm.2009.01.002 ↗
13. Comparison of ZrB2–ZrO2f ceramics prepared by hot pressing and pressureless sintering10.1016/j.ijrmhm.2012.04.007 ↗
14. Study on in-situ synthesis of ZrB2 whiskers in ZrB2–ZrC matrix powder for ceramic cutting tools10.1016/j.ijrmhm.2012.11.001 ↗
15. Oxidation of ZrB2- and HfB2-based ultra-high temperature ceramics: effect of Ta additions10.1023/B:JMSC.0000041693.32531.d1 ↗
16. Oxidation resistance of fully dense ZrB2 with SiC, TaB2, and TaSi2 additives10.1111/j.1551-2916.2008.02368.x ↗
17. Influence of nanosized SiC particle on the fracture toughness of ZrB2-based nanocomposite ceramic10.1016/j.msea.2010.01.059 ↗
18. Microstructure and mechanical properties of laminated ZrB2–SiC ceramics with ZrO2 interface layers10.1016/j.ijrmhm.2011.08.003 ↗
19. Processing and microstructural characterisation of RBSiC–TaSi2 composites10.1023/A:1004447727931 ↗
20. Effect of graphite flake on the mechanical properties of hot pressed ZrB2–SiC ceramics10.1016/j.matlet.2008.07.027 ↗
21. Effect of surface oxidation on thermal shock resistance of the ZrB2–SiC–ZrC ceramic10.1016/j.compscitech.2011.06.008 ↗
22. Mechanical properties and thermal shock resistance of ZrB2–SiC ceramic toughened with graphite flake and SiC whiskers10.1016/j.scriptamat.2009.07.001 ↗
23. The influence of surface heat transfer conditions on thermal shock behavior of ZrB2–SiC–AlN ceramic composites10.1016/j.scriptamat.2009.06.009 ↗
24. Thermal shock behavior of SiC-whisker-reinforced diboride ultrahigh-temperature ceramics10.1016/j.scriptamat.2008.02.023 ↗
25. Sintering and mechanical properties of ZrB2–TaSi2 and HfB2–TaSi2 ceramic composites10.1111/j.1551-2916.2008.02593.x ↗
26. Microstructure characterization of ZrB2–SiC composite fabricated by spark plasma sintering with TaSi2 additive10.1016/j.jeurceramsoc.2011.08.024 ↗
27. Thermal‐shock resistance and fracture‐strength behavior of two tool carbides10.1111/j.1151-2916.1976.tb09415.x ↗
28. Evolution of structure during the oxidation of zirconium diboride–silicon carbide in air up to 1500°C10.1016/j.jeurceramsoc.2006.10.012 ↗
29. Oxidation characteristics of hafnium and zirconium diboride
30. Synthesis of silicon carbide nanopowder using silica fume10.1111/j.1551-2916.2010.03867.x ↗
31. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
32. Oxidation of TaSi2-containing ZrB2–SiC ultra-high temperature materials10.2174/1874146001003020041 ↗
33. Oxidation behavior of zirconium diboride–silicon carbide at 1800°C10.1016/j.scriptamat.2007.07.009 ↗