journal article·2017-12

Microstructure and mechanical properties of hot pressed ZrB2-20SiC composite

Jiten Das, Peddiraju Suraj, Dugyala Shiva Sai Kumar, Laishetti Shekhar, Jamboju Pruthvi, Sweety Kumari, V. Srinivas, J. Janardhana Reddy, V.V. Bhanu Prasad

Publisher page

Abstract

Abstract In this study effort has been made to evaluate micro structural features and corresponding mechanical properties such as bulk hardness, micro hardness, flexural strength and fracture toughness of the ZrB 2 -20 vol% SiC composite before and after infra-red (IR) heating at 1400 and 1500 °C for 600 s. Volume fraction of the ZrB 2 -matrix phase and SiC reinforcing particulate phase of the composite remain same before and after IR heating. The surface of the composite after IR heating at 1400 °C appears to be covered by a thin outer tetragonal SiO 2 layer, and a thin inner monoclinic ZrO 2 layer. Flower like morphology of these oxides is also observed in the oxide scale. Some penetration of oxide product inside the surface defects is also seen. Similar oxide scale is observed for 1500 °C IR heated sample except the absence of flower like oxides morphology in this case. This marginal oxidation on the outer surface of the composite due to IR heating does not affect the mechanical properties of the composite. The mechanical properties such as, bulk hardness, micro hardness, flexural strength and fracture toughness of the composite do not get deteriorated after IR heating of the composite at 1400 and 1500 °C for 600 s rather it appears to improve slightly after IR heating possibly due to healing of the surface defects during IR heating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Thermodynamic analysis of ZrB2-SiC oxidation formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
2. Engineering Conferences International ECI digital archives, Ultra-High Temperature Ceramics: Materials For Extreme Environmental Applications II Proceedings Spring 5-14-2012
3. Oxidation mechanism and resistance of ZrB2-SiC composites10.1016/j.corsci.2009.07.005 ↗
4. Stadelmann · 2015 · 55
5. Influence of silicon carbide particle size on the microstructure and mechanical properties of zirconium diboride–silicon carbide ceramics10.1016/j.jeurceramsoc.2006.07.003 ↗
6. Oxidation behavior of zirconium diboride–silicon carbide at 1800°C10.1016/j.scriptamat.2007.07.009 ↗
7. Fracture Toughness of Advanced Ceramics at Room Temperature10.6028/jres.097.026 ↗
8. Oxidation behavior of ZrB2-SiC composites at low pressures10.1111/jace.13281 ↗
9. Thermogravimetric Study of the oxidation of ZrB2in the temperature range of 800°C to 1500°C10.1149/1.2408279 ↗
10. Effect of an SiC addition of the oxidation of ZrB2
11. Oxidation of ZrB2-SiC10.1002/9780470294680.ch27 ↗
12. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C10.1016/j.jeurceramsoc.2006.10.012 ↗
13. ZrB2 -SiC composites prepared by reactive pulsed electric current sintering10.1016/j.jeurceramsoc.2010.05.012 ↗
14. High-strength zirconium diboride-based ceramics10.1111/j.1551-2916.2004.01170.x ↗
15. Strength of hot pressed ZrB2 -SiC composite after exposure to high temperatures (1000–1700°C)10.1016/j.jeurceramsoc.2012.06.025 ↗
16. Densification, microstructure, and mechanical properties of zirconium diboride based ultra-high temperature ceramics
17. Mechanical properties of ZrB2 –SiC(ZrSi2) ceramics10.1016/j.jeurceramsoc.2010.03.022 ↗
18. Influence of SiCnp content on the microstructure and mechanical properties of ZrB2-SiC nanocomposite10.1016/j.scriptamat.2010.06.005 ↗
19. Characterization of zirconium diboride-molybdenum disilicide ceramics
20. Characterization of zirconium diboride for thermal protection systems10.4028/www.scientific.net/KEM.264-268.493 ↗