journal article·2001-07

Densification, mechanical properties and wear behavior of WC–VC–Co–Al hardmetals

F.J Arenas, A Matos, M Cabezas, C Di Rauso, C Grigorescu

Publisher page

Abstract

Abstract The effect of VC and Al additions on the sintering behavior, hardness, toughness, elastic properties and wear characteristics of WC–10 wt% Co has been studied. The amount of VC in the compositions varied up to 18 wt% and the aluminum contents was fixed at 2 wt% with the purpose to promote the in situ formation of the CoAl intermetallic phase. The specimens were prepared by vacuum sintering in the 1350–1500 °C range during 1 h. The sintered samples densification improved both with the temperature and VC contents up to 13 wt%. The heterogeneous microstructure consisting of WC, (W, V)C1−x and intermetallic Al5Co2 phase indicated that the expected reactive sintering induced by the Co and Al could not be properly controlled due to the large Al particle size used, resulting in isolated aluminum enriched pools. Vickers hardness and toughness followed an antagonistic behavior with values ranging from 12.8–17.5 GPa and 7.7–10.5 MPa m1/2, respectively. The sliding wear performance evaluation showed that friction decreases with VC addition but it could not be established a tendency for the wear rate coefficient though values obtained allow to consider these experimental compositions as promising wear resistant materials.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Microstructure and mechanical properties of WC–TiN–10Co and WC–TiN–Mo2C–Co(Ni) cemented carbides10.1016/0272-8842(92)90082-O ↗
2. Investigation into the potential of a composite combining toughness and plastic deformation resistance10.1016/S0263-4368(98)00044-4 ↗
3. Some properties of Ti(C,N)–WC–Ni alloy
4. Microstructure and mechanical properties of a (TiC,Ta,Mo) (CN)–(Co,Ni)-type cermet
5. 1998
6. Phase relations, microstructure and mechanical properties of VC substituted WC–10Co cemented carbide alloys10.1016/S0263-4368(97)00005-X ↗
7. Influence of VC on the microstructure and mechanical properties of WC–Co sintered cemented carbides10.1016/S0263-4368(98)00061-4 ↗
8. Fine grained WC–VC–Co hardmetal10.1179/pom.1996.39.3.210 ↗
9. An atypical microstructure in WC–Co cemented carbides
10. On the preparation of fine V8C7–WC and V4C3–WC powders10.1016/S0263-4368(96)00029-7 ↗
11. Sintering of sub-micron WC–10Co hardmetals containing Ni and Fe10.1016/0025-5416(88)90503-4 ↗
12. Advanced and new grades of WC and binder powder – their properties and application10.1016/S0263-4368(00)00002-0 ↗
13. On the composition of Fe–Ni–Co–WC based cemented carbides10.1016/S0263-4368(96)00023-6 ↗
14. Cemented carbides properties in relation to binder phases
15. Ni3Al bonded WC and TiC hardmetals
16. Ordered intermetallic alloys, part I: nickel and iron aluminides
17. 1985
18. Effect of TiC on the sintering and wear behavior of modified WC/Co hardmetals
19. Indentation fracture toughness of WC–Co cermets10.1007/BF00555296 ↗
20. Upadhyaya · 1996 · 446
21. Physical and chemical nature of cemented carbides
22. Cottrell · 1964 · 5
23. Friction and wear as related to the composition, structure and properties of metals
24. Effects of normal loads on the friction and wear properties of metals and ceramic against cermet in vacuum10.1016/S0043-1648(99)00308-7 ↗
25. Friction and wear of synthetic diamond10.1016/S0263-4368(99)00012-8 ↗