The effects of C:N ratio on the aqueous corrosion response of TiC and Ti(C,N) cermets with a Ni 3 Al-based binder
Source abstract
Abstract
Abstract The aqueous corrosion behaviour of TiC and Ti(C,N) based cermets, sintered with 30 vol.% Ni3Al binder, has been investigated. For comparison purposes, the single-phase constituents were prepared using spark plasma sintering (SPS). The potentiodynamic and cyclic polarisation responses of the cermets and single-phase materials have been determined. Post-test corrosion solutions were analysed using inductively coupled plasma optical emission spectrometry, while samples were evaluated using scanning electron microscopy and associated energy dispersive X-ray analysis. Selective attack of the binder occurs, while the extent of corrosion and primary operative mechanism depends on the C:N ratio in the Ti(C,N).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Hardmetals and cermets10.1146/annurev.ms.19.080189.001045 ↗
2. Corrosion behavior in artificial seawater of thermal-sprayed WC-CoCr coatings on mild steel by electrochemical impedance spectroscopy10.1007/s10008-011-1403-y ↗
3. Tribological evaluation of HVOF thermal-spray coatings as a hard chrome replacement10.1002/sia.3721 ↗
4. Titanium carbonitride-based cermets: processes and properties10.1016/0921-5093(93)90588-6 ↗
5. Kreymer · 1974
6. Properties of Ni3Al-bonded titanium carbide ceramics10.1016/S0955-2219(97)00124-6 ↗
7. A comparison of the abrasive wear behaviour of HVOF sprayed titanium carbide- and titanium boride-based cermet coatings10.1016/S0043-1648(01)00702-5 ↗
8. Effect of laser cladding process parameters on clad quality and in-situ formed microstructure of Fe-TiC composite coatings10.1016/j.surfcoat.2010.08.087 ↗
9. Corrosion properties of Co-based cemented carbides in acidic solutions10.1016/S0263-4368(03)00027-1 ↗
10. Electrochemical oxidation of WC in acidic sulphate solution10.1016/S0010-938X(03)00146-X ↗
11. An SFG and ERS investigation of the corrosion of CoW0.013C0.001 alloys and WC-Co cermets in CN−-containing aqueous solutions10.1016/j.corsci.2006.10.038 ↗
12. The corrosion behaviour of WC-VC-Co hardmetals in acidic media10.1016/j.corsci.2010.05.033 ↗
13. Anodic polarization and corrosion of cemented carbides with cobalt and nickel binders10.1007/BF01153988 ↗
14. Anodic polarization and corrosion of WC-Co hardmetals containing small amounts of Cr3C2 and/or VC10.1007/BF01174495 ↗
15. A comparison between cemented carbides containing cobalt and nickel based binders
16. Analytical characterization of the corrosion mechanisms of WC-Co by electrochemical methods and inductively coupled plasma mass spectroscopy10.1016/j.corsci.2006.08.022 ↗
17. ICP-MS, SKPFM, XPS, and microcapillary investigation of the local corrosion mechanisms of WC-Co hardmetal10.1149/1.2929822 ↗
18. Corrosion behavior of thermal sprayed WC cermet coatings having various metallic binders in strong acidic environment10.1016/j.surfcoat.2004.10.142 ↗
19. Electrochemical behaviour of cermet coatings with a bond coat on Al7075: pseudopassivity, localized corrosion and galvanic effect considerations in a saline environment10.1016/j.corsci.2010.04.010 ↗
20. Effects of Cr3C2 addition on the corrosion behavior of Ti(C, N)-based cermets10.1016/j.ijrmhm.2011.10.013 ↗
21. NiTi cladding on stainless steel by TIG surfacing process part II. Corrosion behavior10.1016/S0257-8972(03)00346-3 ↗
22. Corrosion and erosion damage mechanisms during erosion - corrosion of WC-Co-Cr cermet coatings10.1016/S0043-1648(03)00210-2 ↗
23. Aspects of microstructure on the synergy and overall material loss of thermal spray coatings in erosion-corrosion environments10.1016/j.wear.2007.01.071 ↗
24. Method of making ductile intermetallic-bonded ceramic composites
25. An algorithm for least-squares estimation of nonlinear parameters10.1137/0111030 ↗
26. ASTM Standard G59-97 · 2014
27. ASTM Standard G102-89e1 · 2015
28. ASTM Standard G61-86 · 2014
29. Corrosion behaviour of cermet-based coatings with a bond coat in 0.5M H2SO410.1016/j.corsci.2008.09.020 ↗
30. Corrosion behaviour of modified HVOF sprayed WC based cermet coatings on stainless steel
31. The sliding wear of TiC and Ti(C,N) cermets prepared with a stoichiometric Ni3Al binder10.1016/j.wear.2014.06.025 ↗
32. A study on microstructural changes in Ti(CN)-NbC-Ni cermets10.1016/S0921-5093(98)00609-1 ↗
33. Formation of core/rim structures in Ti (C,N)-WC-Ni cermets via a dissolution and reprecipitation process10.1111/j.1151-2916.2000.tb01415.x ↗
34. Effect of boron on the corrosion behavior of polycrystalline Ni3Al10.1007/BF02662413 ↗
35. Evaluation of a Cr3C2(NiCr) coating deposited on s4400 by means of an HVOF process and used for flow plates of PEM fuel10.1016/S1452-3981(23)13396-7 ↗
36. Wear and corrosion behaviour of thermally sprayed cermet coatings10.1016/S0257-8972(00)01141-5 ↗
37. Surface area relationships in polarization and corrosion10.5006/0010-9312-14.7.43 ↗
38. The growth of 2-D pits in thin film aluminum10.1016/0010-938X(90)90199-F ↗
39. Pitting corrosion of titanium - the relationship between pitting potential and competitive anion adsorption at the oxide film/electrolyte interface10.1149/1.1393364 ↗
40. Comparison between open circuit and imposed potential measurements to evaluate the effect of temperature on galvanic corrosion of the pair alloy 31-welded alloy 31 in LiBr solutions10.1016/j.corsci.2008.09.011 ↗
41. Electrolytic corrosion of titanium carbonitride composites10.1023/B:PMMC.0000028273.86448.54 ↗
42. Effects of nitric acid passivation on the pitting resistance of 316 stainless steel10.1016/S0010-938X(00)00052-4 ↗
43. Electrochemical corrosion properties of metal alloys used in orthopaedic implants10.1007/s10800-009-9793-6 ↗
44. Galvanic corrosion of aluminum-matrix composites10.5006/1.3315972 ↗
45. Pourbaix · 1967
46. Effect of Mo and Mo2C on the microstructure and properties of the cermets based on Ti(C,N)
47. Corrosion resistance and biocompatibility of Ti-Ta alloys for biomedical applications10.1016/j.msea.2005.03.032 ↗
48. The corrosion behaviour of Ti-6Al-4V, Ti-6Al-7Nb and Ti-13Nb-13Zr in protein solutions10.1016/S0142-9612(98)00217-8 ↗
49. Pitting corrosion of metals10.1149/1.1838615 ↗
50. ASTM Standard F2129-15 · 2001 · 1
51. Kinetics and mechanism of electrolytic corrosion of titanium-based ceramics in 3% NaCl solution10.1016/j.jeurceramsoc.2004.12.014 ↗