journal article·2026-12

Effect of the binder phase composition and volume fraction on the sintering behavior of extra-coarse WC-based hardmetals

Irene Salto Talaya, Lucía Muñoz-Ortuño, José M. Sánchez-Moreno, Unai Galech, Federico Ibarreta-López, Roberto Martínez-Pampliega, Adrián Durán Benito, Tomás Soria-Biurrun

Publisher page

Abstract

This work investigates the sintering behavior and microstructural evolution of extra-coarse WC hardmetals using conventional Co and FeNiCo (40/40/20) (wt.%) binder phases. Four compositions containing 15 and 20 wt.% metallic binder were produced by powder metallurgy and consolidated by SinterHIP at 1475 °C. Dilatometry and DSC analyses showed that replacing Co with FeNiCo significantly reduces sinterability, shifting densification to higher temperatures despite similar calculated liquid-phase fractions. This behavior is attributed to the lower solubility of WC in FeNiCo liquids compared with liquid Co. Microstructural characterization revealed complete densification and the elimination of W₂C after sintering. WC grain growth was strongly affected by binder chemistry. FeNiCo-bonded alloys exhibited more pronounced changes in grain size distribution with increasing binder content and developed more rounded WC morphologies than WC–Co grades. Hardness measurements confirmed a significant softening associated with FeNiCo substitution, mainly due to the intrinsically lower hardness of Ni-rich metallic matrices.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Wear damage of cemented carbides with different combinations of WC mean grain size and Co content, part II: laboratory performance tests on rock cutting and drilling10.1016/j.ijrmhm.2005.03.007 ↗
2. A new view of the deterioration and wear of WC/Co cemented carbides rock rill buttons10.1016/j.wear.2007.01.030 ↗
3. On a wear test for rock drill inserts10.1016/j.wear.2012.10.023 ↗
4. Pitting mechanism of cemented carbide tool in the early stage of rock drilling10.1016/j.ijrmhm.2013.08.009 ↗
5. Modes of failure of cemented tungsten carbide tool bits (WC/Co): a study of wear parts10.1016/j.ijrmhm.2015.06.018 ↗
6. The wear of WC-Co bits during rotary-percussive drilling of reinforced concrete10.1016/j.ijrmhm.2016.08.006 ↗
7. Examination of wear damage to rock-mining hardmetal drill bits10.1016/j.ijrmhm.2017.01.013 ↗
8. Influence of cemented carbide binder type on wear initiation in rock drilling investigated in sliding wear against magnetite rock10.1016/j.ijrmhm.2019.105035 ↗
9. Wear phenomena in different cemented carbides during rotary-percussive drilling in reinforced concrete10.1016/j.ijrmhm.2022.105941 ↗
10. Effects of ultrafine WC on the densification behavior and microstructural evolution of coarse-grained WC-5Co cemented carbides10.1016/j.ceramint.2020.01.113 ↗
11. Effect of ultrafine WC contents on the microstructures, mechanical properties and wear resistances of regenerated coarse grained WC-10Co cemented carbides10.1016/j.ijrmhm.2021.105516 ↗
12. Effects of nano WC and Cr3C2 on grain growth, microstructure and mechanical properties of ultra-coarse cemented carbides10.1016/j.ijrmhm.2022.106022 ↗
13. Novel ultra-coarse hardmetal grades with reinforced binder for mining and construction10.1016/j.ijrmhm.2005.03.007 ↗
14. Effect of WC grain size on mechanical properties and microstructures of cemented carbide with medium entropy alloy Co-Ni-Fe binder10.1007/s11771-020-4355-5 ↗
15. Effect of milling conditions and binder phase content on liquid phase sintering of heat treatable WC-Ni-Co-Cr-Al-Ti cemented carbides10.1016/j.ijrmhm.2020.105202 ↗
16. Influence of TiB2 and Ni addition on microstructure and mechanical properties of WC–10Co ultra–coarse grain cemented carbides10.1016/j.jallcom.2025.183179 ↗
17. Grohol · 2023
18. Aspects of sintering of cemented carbides with Fe-based binders10.1016/j.ijrmhm.2014.07.028 ↗
19. Effect of chromium and carbon contents on the sintering of WC-Fe-Ni-Co-Cr multicomponent alloys10.1016/j.ijrmhm.2020.105317 ↗
20. Experimental and theoretical study of WC-40Fe-20Co-40Ni10.1016/j.ijrmhm.2021.105719 ↗
21. Densification of WC-Fe-Ni-Co-Cr cemented carbides processed by HIP after sintering: effect of WC powder particle size10.1016/j.ijrmhm.2022.105994 ↗
22. Experimental investigation and thermodynamic modelling of WC-Fe-Ni-Co-Cr cemented carbides10.1016/j.ijrmhm.2024.106824 ↗
23. The preparation, preparation mechanism and properties of extra coarse-grained WC-Co hardmetals10.1016/j.mprp.2017.01.001 ↗
24. Controlled porosity by an extreme Kirkendall effect10.1016/0001-6160(74)90059-5 ↗
25. Modelling WC-co sintering shrinkage-effect of carbide grain size and cobalt content10.1016/j.msea.2006.10.157 ↗
26. Upadhyaya · 1983 · 41
27. Wetting of surfaces and grain boundaries in cemented carbides and the effect from local chemistry
28. Sintering of submicron WC–10 wt.% Co hard metals containing nickel and iron10.1016/0025-5416(88)90503-4 ↗
29. Cemented carbide microstructures: a review10.1016/j.ijrmhm.2018.12.004 ↗
30. Novel binders for WC-based cemented carbides with high Cr contents10.1016/j.ijrmhm.2019.105063 ↗
31. On the three-dimensional structure of WC grains in cemented carbides10.1016/j.actamat.2013.05.008 ↗
32. Evolution of the WC grain shape in WC-Co alloys during sintering: effect of C content10.1016/j.ijrmhm.2008.06.001 ↗
33. Faceting/roughening of WC/binder interfaces in cemented carbides: a review10.3390/ma16103696 ↗
34. Carbide grain growth in cemented carbides sintered with alternative binders10.1016/j.ijrmhm.2019.105088 ↗
35. Global trends in the hard metals industry
36. New scientific approaches to development of tool materials10.1179/imr.1988.33.1.151 ↗
37. A new hardness model for materials design in cemented carbides10.1016/j.ijrmhm.2018.04.004 ↗