journal article·2015-11

Conventional sintering of WC with nano-sized Co binder: Characterization and mechanical behavior

Rumman Md. Raihanuzzaman, Seung-Taek Han, Reza Ghomashchi, Hyo-Seob Kim, Soon-Jik Hong

Publisher page

Abstract

Abstract In this study, WC particles of 1–3 μm were blended with two different sizes of Co particles and sintered conventionally at two different temperatures. Compaction of initial powders was carried out using a relatively new dynamic compaction method called Magnetic Pulsed compaction (MPC). The maximum Vickers hardness for the samples found was around 1353 HV (13.27 GPa), while the maximum fracture toughness was observed at 4.6 MPa · m 1/2 . The marked changes in density, hardness, fracture toughness and crack behavior observed in the samples indicate strong correlations among particle size, sintering process and mechanical properties of cemented carbides. In addition, the nature of crack initiation and propagation, which is indicative of the trend in fracture toughness of materials, was observed and analyzed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Analysis of grain-and particle-size distributions in metallic materials10.1179/095066072790137729 ↗
2. Mechanical properties of WC–10Co cemented carbides sintered from nanocrystalline spray conversion processed powders10.1016/S0263-4368(01)00057-9 ↗
3. Nanostructured WC/Co composite powder prepared by high energy ball milling10.1016/j.scriptamat.2003.08.009 ↗
4. Full density processing of complex WC-based cemented carbides10.1016/0924-0136(95)02106-X ↗
5. Consolidation of WC–Co alloys by magnetic pulsed compaction and evaluation of their mechanical properties10.1016/j.powtec.2012.11.032 ↗
6. Powder refinement, consolidation and mechanical properties of cemented carbides—an overview10.1016/j.powtec.2014.04.024 ↗
7. Evaluation of mechanical properties and processing conditions of WCCo alloys fabricated by magnetic pulsed compaction10.1016/j.jallcom.2011.12.108 ↗
8. Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide—a review10.1016/j.ijrmhm.2008.07.011 ↗
9. Design of stable nanocrystalline alloys10.1126/science.1224737 ↗
10. Fabrication and densification behavior analysis of metalizing targets using ZrO2 nanopowders by magnetic pulsed compaction10.2320/matertrans.M2010398 ↗
11. Wear behavior of Al–Fe–Cr–Ti alloys fabricated by magnetic pulsed compaction10.1016/j.powtec.2012.04.018 ↗
12. Effect of magnetic pulsed compaction (MPC) on sintering behavior of materials
13. Microstructural tailoring and characterization of a calcium α‐SiAlON composition10.1111/j.1151-2916.2002.tb00177.x ↗
14. Spark plasma sintering behavior of nanocrystalline WC–10Co cemented carbide powders10.1016/S0921-5093(02)00605-6 ↗
15. Cemented carbides
16. Coromant · 1994
17. Preparation and structure of bulk nanostructured WC–Co alloy by high energy ball-milling10.1023/A:1018525213450 ↗
18. Characterizations of ball-milled nanocrystalline WC–Co composite powders and subsequently rapid hot pressing sintered cermets10.1016/S0167-577X(03)00011-9 ↗
19. Sintering and microstructure of nanophase WC/Co hardmetals10.1016/S0924-0136(96)02748-3 ↗
20. Production of nanometric tungsten carbide powders by planetary milling
21. The fracture toughness of cemented tungsten carbides10.1016/0013-7944(74)90016-2 ↗
22. Materials with ultrafine microstructures: retrospective and perspectives10.1016/0965-9773(92)90045-Y ↗
23. Synthesis and properties of nanophase materials10.1016/0921-5093(93)90726-U ↗
24. Hodson · 2009