Research on the oxidation resistance and ultra-high frequency thermal fatigue shock failure mechanisms of the bilayer and multilayer nano-coatings on cemented carbide tools
Source abstract
Abstract
The multilayer nano-coating shows excellent thermal stability and oxidation resistance which could be attributed to the multielement composition and multilayer structure. It is widely used in the machining of hard-to-cut materials, such as titanium alloy. The formation of serrated chip during cutting process of Ti-6Al-4V would result in the ultra-high frequency thermal fatigue shock on the coating surface, and this could induce the thermal fatigue failure of coating. In this study, the ultra-high frequency (20 kHz) thermal fatigue shock testing was developed to investigate the thermal fatigue failure mechanisms of the bilayer TiSiN/TiAlN coating and multilayer TiSiN/TiAlN nano-coating. It was achieved by using the pulsed laser system to irradiate the coating surface under different shock cycles, which could produce alternating thermal stress on coating surface. This creates a close simulation of the actual working conditions in high-speed machining of Ti-6Al-4V with serrated chip produced. Moreover, the high temperature oxidation experiments were performed to study the oxidation resistance of coating. The failure mechanisms of coating/substrate system under the constant thermal loads and dynamic thermal loads were compared and analyzed. The cutting performance of related coated tools was evaluated after turning Ti-6Al-4V. The correlation between the thermal fatigue shock resistance of coatings at ultra-high frequency and the wear behavior of coated tools was built. It can be concluded that the multilayer TiSiN/TiAlN nano-coating showed better properties of the resistance to thermal fatigue shock in machining Ti-6Al-4V.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Thermal stability of nitride thin films10.1016/S0042-207X(00)00143-3 ↗
2. Microstructures of TiN, TiAlN and TiAlVN coatings on AISI M2 steel deposited by magnetron reactive sputtering10.1016/S1003-6326(14)63383-5 ↗
3. Thermal stability and machining performance of arc evaporated Ti1-xAlxN hard PVD coatings with x=0.5-0.73 ratios using an integrative approach10.1016/j.mtla.2021.101132 ↗
4. Wear and friction of TiAlN/VN coatings against Al2O3 in air at room and elevated temperatures10.1016/j.actamat.2010.01.020 ↗
5. High temperature behavior of nanolayered CrAlTiN coating: thermal stability, oxidation, and tribological properties10.1016/j.surfcoat.2014.07.053 ↗
6. Influence of Si content on the microstructure, thermal stability and oxidation resistance of TiAlSiN/CrAlN multilayers10.1016/j.jallcom.2020.157441 ↗
7. Tribological and cutting performance of TiAlCrN films with different Cr contents deposited with multilayered structure10.1016/j.triboint.2017.11.008 ↗
8. Microstructural, mechanical, thermal stability and oxidation behavior of TiSiN/CrVxN multilayer coatings deposited by D.C. reactive magnetron sputtering10.1016/j.surfcoat.2020.126593 ↗
9. Structure, mechanical properties and thermal stability of CrAlNbN/TiN multilayers10.1016/j.vacuum.2021.110182 ↗
10. Oxidation behavior, microstructure evolution and thermal stability in nanostructured CrN/AlN multilayer hard coatings10.1016/j.jallcom.2009.09.060 ↗
11. Improved properties of TiAlN coatings through the multilayer structure10.1016/j.surfcoat.2013.08.006 ↗
12. Studies on different oxidation behaviors of TiAlN on titanium alloy and stainless steel under thermal cycling10.1016/j.corsci.2021.109865 ↗
13. Crack propagation behavior of TiN coatings by laser thermal shock experiments10.1016/j.apsusc.2012.05.086 ↗
14. Interfacial stability and diffusion barrier ability of Ti1-xZrxN coatings by pulsed laser thermal shock10.1016/j.apsusc.2014.09.134 ↗
15. Local atomic structures and degradation behaviors of Ti1-xZrxN coatings under laser thermal shock10.1016/j.matchar.2017.07.003 ↗
16. Thermal degradation of TiN and TiAlN coatings during rapid laser treatment10.1016/j.surfcoat.2021.127517 ↗
17. Thermal shock behaviors of Ti1-xZrxN coatings by accelerated test based on pulsed laser ablation10.1016/j.ceramint.2015.10.017 ↗
18. Mechanical impact test methods for hard coatings of cutting tools: a review10.1007/s00170-021-07219-8 ↗
19. Investigation the fatigue impact behavior and wear mechanisms of bilayer micro-structured and multilayer nano-structured coatings on cemented carbide tools in milling titanium alloy10.1016/j.ijrmhm.2021.105738 ↗
20. Numerical investigation on serrated chip formation during high-speed milling of Ti-6Al-4V alloy10.1016/j.jmapro.2021.09.056 ↗
21. Numerical and experimental investigation on thermo-mechanically induced residual stress in high-speed milling of Ti-6Al-4V alloy10.1016/j.jmapro.2022.02.039 ↗
22. Analytical model of milling forces based on time-variant sculptured shear surface10.1016/j.ijmecsci.2016.06.018 ↗
23. Three-dimensional transient cutting tool temperature field model based on periodic heat transfer for high-speed milling of compacted graphite iron10.1016/j.jclepro.2021.129106 ↗
24. Cutting performance of CrN and Cr-Si-N coated end-mill deposited by hybrid coating system for ultra-high speed micro machining10.1016/j.surfcoat.2008.06.128 ↗
25. Influences of chip serration on micro-topography of machined surface in high-speed cutting10.1016/j.ijmachtools.2014.10.012 ↗
26. Very high speed cutting of Ti-6Al-4V titanium alloy – change in morphology and mechanism of chip formation10.1016/j.ijmachtools.2012.11.004 ↗
27. The relationship between the cutting speed, tool wear, and chip formation during Ti-5553 dry cutting10.1007/s00170-014-6326-1 ↗
28. Evaluation on fracture locus of serrated chip generation with stress triaxiality in high speed machining of Ti6Al4V10.1016/j.matdes.2016.03.012 ↗
29. Investigating the high frequency fatigue failure mechanisms of mono and multilayer PVD coatings by the cyclic impact tests10.1016/j.surfcoat.2018.03.101 ↗
30. Correlation of the fatigue impact resistance of bilayer and nanolayered PVD coatings with their cutting performance in machining Ti-6Al-4V10.1016/j.ceramint.2019.04.193 ↗
31. Research on cutting performance of coated cutting tools by a new impact test method considering contact stress condition caused by segmented chips10.1016/j.jmapro.2021.07.001 ↗
32. An accurate transient model for temperature fluctuation on localized shear band in serrated chip formation10.1016/j.ijmecsci.2021.106588 ↗
33. Characterization of tool–chip interface temperature measurement with thermocouple fabricated directly on the rake face10.1115/1.4044035 ↗
34. Thermomechanical coupling investigation in Ti-6Al-4V orthogonal cutting: experimental and numerical confrontation10.1016/j.ijmecsci.2019.105322 ↗
35. Dynamic constitutive models of Ti-6Al-4V based on isothermal ture stress-strain curves10.1016/j.jmrt.2022.06.164 ↗
36. Wear behavior and thermal stability of HPPMS (Al,Ti,Cr,Si)ON, (Al,Ti,Cr,Si)N and (Ti,Al,Cr,Si)N coatings for cutting tools10.1016/j.surfcoat.2020.125370 ↗
37. Influence of Ti on the mechanical properties, thermal stability and oxidation resistance of Al-Cr-N coatings10.1016/j.vacuum.2015.07.004 ↗
38. Analysis of adiabatic shear banding in orthogonal cutting of Ti alloy10.1016/j.ijmecsci.2013.06.011 ↗
39. Microstructure evolution of adiabatic shear bands and mechanisms of saw-tooth chip formation in machining Ti6Al4V10.1016/j.msea.2011.10.050 ↗
40. Insights into plastic deformation and binder lamella orientation in hardmetal turning inserts10.1016/j.ijrmhm.2022.105779 ↗
41. On the influence of varying the crystallographic texture of alumina CVD coatings on cutting performance in steel turning10.1016/j.ijmachtools.2022.103885 ↗
42. On the mechanism of crater wear in a high strength metastable β titanium alloy10.1016/j.wear.2021.203998 ↗
43. Onset of the degradation of CVD α-Al2O3 coating during turning of ca-treated steels10.1016/j.wear.2021.203785 ↗
44. Quantification of nano-scale interface structures to guide mechanistic modelling of WC grain coarsening inhibition in V-doped hard metals10.1016/j.matdes.2021.109825 ↗
45. Thermodynamic modeling framework for prediction of tool wear and tool protection phenomena in machining10.1016/j.wear.2021.203991 ↗