Strengthening and toughening of WC-Ni alloys by adding novel (Ti, Hf, Ta, Nb, Zr)(C, N) high entropy powder
Source abstract
Abstract
A strong and tough WC-11Ni cemented carbide was prepared by adding ultrafine (Ti, Hf, Ta, Nb, Zr)(C, N) high entropy powder with ellipsoidal-like particles of ∼300 nm and a single phase composition via low pressure sintering. WC-11Ni-0.6(Ti, Hf, Ta, Nb, Zr)(C, N) alloy has excellent mechanical properties: bending strength of 2752 MPa, HV30 hardness of 14.76 GPa and toughness of 15.35 MPa·m 1/2, which increase by 22.58%, 20.29% and 20.78% respectively, compared with pure WC-11Ni alloy. (Ti, Hf, Ta, Nb, Zr)(C, N) addition with a small content not only inhibits the abnormal growth of WC grains, but also eliminates the aggregation of Ni binder phase and strengthens Ni binding phase. This work provides a simple route to strengthen and toughen WC-Ni alloys by introducing a novel high entropy inhibitor.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Effects of Ni and cu additions on microstructures, mechanical properties and wear resistances of ultra-coarse grained WC–6Co cemented carbides10.1016/j.ijrmhm.2017.10.009 ↗
2. Performance enhancement of ultra-coarse cemented carbide by boride additives10.1016/j.jallcom.2020.155250 ↗
3. Fabrication and mechanical properties of WC-10Co cemented carbides with plate-like WC grains10.1016/j.jallcom.2019.06.328 ↗
4. Microstructure evolution of WC grains in WC-co-Ni-Al alloys: effect of binder phase composition10.1016/j.jallcom.2017.03.284 ↗
5. Microstructure and properties of ultrafine grained AlCrFeCoNi/WC cemented carbides10.1016/j.ceramint.2018.06.171 ↗
6. Fabrication of WC-co cemented carbides with gradient distribution of WC grain size and co composition by lamination pressing and microwave sintering10.1016/j.ceramint.2018.03.162 ↗
7. Effect of carbon content on microstructure and mechanical properties of WC-10Co cemented carbide with plate-like WC grain10.1016/j.ceramint.2019.09.158 ↗
8. Interface characteristics in cemented carbides with alternative binders10.1016/j.ijrmhm.2020.105306 ↗
9. Corrosion behaviour of WC hardmetals with nickel-based binders10.1016/j.corsci.2018.11.015 ↗
10. High-temperature sliding wear, elastic modulus and bending strength of Ni bonded NbC and WC cermets10.1016/j.ijrmhm.2019.105143 ↗
11. The effects of metallic additives on the microstructure and mechanical properties of WC-co cermets prepared by microwave sintering10.1016/j.ceramint.2020.08.093 ↗
12. Effects of Cr concentration on the microstructure and properties of WC-Ni cemented carbides10.1016/j.jmrt.2019.11.030 ↗
13. Microstructure, mechanical properties, and cutting performances of WC-co cemented carbides with Ru additions10.1016/j.ceramint.2021.06.011 ↗
14. WC grain growth and grain growth inhibition in nickel and iron binder hardmetals10.1016/S0263-4368(01)00070-1 ↗
15. The influence of grain growth inhibitors on the microstructure and properties of submicron, ultrafine and nano-structured hardmetals-a review10.1016/j.ijrmhm.2018.07.003 ↗
16. Long-range migration behavior of rare earth additives in WC–co cemented carbides10.1016/j.ijrmhm.2014.04.020 ↗
17. Microstructure and mechanical properties of 90WC-8Ni-2Mo2C cemented carbide developed by conventional powder metallurgy10.1016/j.ijrmhm.2017.06.009 ↗
18. Spark plasma sintering of ultrafine WC-10Ni-ZrC hardmetals: effects of adding ZrC nano-powder10.1111/ijac.13475 ↗
19. Effects of Nb and NbC additives on microstructure and properties of WC-co-Ni cemented carbides10.1016/j.ijrmhm.2022.105782 ↗
20. Malheiros, The effect of Cr content on the corrosion resistance of WC-Ni-Cr-Mo composites10.1016/j.ijrmhm.2020.105434 ↗
21. Microstructure and properties of in situ La2O3 and SiC co-doped WC-10 wt% Ni cemented carbides prepared by microwave sintering10.1016/j.ceramint.2020.07.296 ↗
22. Microstructure and mechanical properties improvements in cemented carbides by (Cr, Mo, ta)2(C, N) inhibitors10.1007/s12598-019-01343-x ↗
23. VC, Cr3C2 doped ultrafine WC-co cemented carbide prepared by spark plasma sintering10.1016/j.ijrmhm.2010.09.004 ↗
24. Preparation of nanocrystalline gradient cemented carbide by adding gradient former of V (C, N)10.1016/j.ijrmhm.2021.105630 ↗
25. Effects of (Ti, ta, Nb, W)(C, N) on the microstructure, mechanical properties and corrosion behaviors of WC-co cemented carbides10.1016/j.ceramint.2016.09.124 ↗
26. The enhancement of the microstructure and mechanical performances of ultrafine WC-co cemented carbides by optimizing Cr2(C, N) addition and WC particle sizes10.1016/j.ijrmhm.2021.105518 ↗
27. Improved densification and hardness of high-entropy diboride ceramics from fine powders synthesized via borothermal reduction process10.1016/j.ceramint.2020.02.214 ↗
28. Ab Initio prediction of mechanical and electronic properties of ultrahigh temperature high-entropy ceramics (Hf0.2Zr0.2Ta0.2M0.2Ti0.2)B2 (M=Nb, Mo, Cr)10.1002/pssb.201800011 ↗
29. Thermodynamics of formation of simple spinels10.1016/0022-1902(68)80475-0 ↗
30. Investigation into the sintered behavior and properties of nanostructured WC-co-Ni-Fe hard metal alloys10.1016/j.msea.2014.03.096 ↗
31. Study on phase evolution during reaction synthesis of ultrafine (Ti, W, Mo, V)(C, N)-Ni composite powders10.1016/j.matchemphys.2009.07.021 ↗
32. Preparation and properties of the VC/Cr3C2/TaC doped ultrafine WC-co tool material by spark plasma sintering10.1016/j.jallcom.2019.152598 ↗
33. Fabrication of WC-co cemented carbides with gradient distribution of WC grain size and co composition by lamination pressing and microwave sintering10.1016/j.ceramint.2018.03.162 ↗
34. The effects of nitrogen additions to a cobalt-chromium surgical implant alloy10.1007/BF01160770 ↗