Effect of diamond additions on the microstructure, physical and mechanical properties of WC- TiC- Co/Ni Nano-composite
Source abstract
Abstract
Abstract WC- TiC- Co- Ni/diamond composites have been prepared by powder metallurgy technique. 2.5%, 5%, 7.5% and 10 wt% diamond were added. WC- TiC- Co/diamond was coated with 12 wt% nickel by the electro-less deposition process. All the samples were compressed at 700 MPa then sintered at 1450 for 1 h. XRD, EDAX, and microstructure were investigated. Density, electrical resistivity, thermal conductivity, magnetic properties, the coefficient of thermal expansion, fracture toughness and hardness were studied. The results of XRD and EDAX analysis show that new phases were formed. It also revealed that the diamond content has a positive effect on the thermal properties of composites. Presence of Ni content improves the Fracture toughness of the composites but decreases the hardness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Mechanical properties of WC–10Co cemented carbides sintered from Nano-crystalline spray conversion processed powders10.1016/S0263-4368(01)00057-9 ↗
2. Microstructures of cemented carbides10.1016/S0261-3069(01)00006-1 ↗
3. Sandvik, Understanding cemented carbide. Sandvik Hard Materials.
4. A research on the grain growth of WC–Co cemented carbide10.1016/j.ijrmhm.2006.03.002 ↗
5. Microstructure and mechanical properties of Nano-crystalline WC–12Co consolidated by spark plasma sintering10.1016/j.ijrmhm.2006.03.008 ↗
6. Growth behavior of rounded (Ti,W)C and faceted WC grains in a Co matrix during liquid phase sintering10.1016/j.actamat.2005.06.021 ↗
7. Microstructures of binder-less tungsten carbides sintered by spark plasma sintering process10.1016/S0921-5093(03)00151-5 ↗
8. Tribological wear behavior of diamond reinforced composite coating10.1016/j.msea.2005.12.004 ↗
9. Gill · 2004
10. Spark plasma sintering of diamond binder-less WC composites
11. Microstructural characterization and wear behaviour of diamond composite materials
12. Wear mechanisms of diamond-containing hardmetals in comparison with diamond-based materials10.1016/j.ijrmhm.2017.10.013 ↗
13. Microstructure and physical properties of blended and coated (Ta, Nb) C/Ni cermets
14. Microstructure, physical properties and hardness of alumina short fibres/nickel matrix composites fabricated by powder technology10.1177/0021998313513203 ↗
15. Room-temperature thermal conductivity of cemented transition-metal carbides10.1111/j.1151-2916.1988.tb05804.x ↗
16. Grain coarsening in Fe-Ni-Cr alloys and the influence of second-phase particles10.1016/0001-6160(82)90149-3 ↗
17. Grain size distribution in Al2O3-ZrO2 generated by high-temperature annealing10.1111/j.1151-2916.1991.tb06849.x ↗
18. Fracture toughness of steels with nickel content in respect of carbide morphology10.1179/1743284715Y.0000000023 ↗
19. The effect of nickel on fracture toughness at low temperature for hydrogen pre-charged steel samples
20. Hardness, toughness, brittleness and cracking systems in an iron-based bulk metallic glass by indentation