The effect of consolidation parameters on the mechanical properties of binderless tungsten carbide
Source abstract
Abstract
Abstract This paper discusses the effect of the process parameters on the mechanical properties of binderless pure tungsten carbide during a GPS (gas protection sintering) process. The result of experiments reveal that the mechanical properties of the material increases with raising the sintering temperature and extending the retention time; however a decreased hardness was observed as a result of abnormal grain growth under higher sintering temperatures. The results of XRD and EDS analyses confirmed the absence of brittle phases such as W 2 C or impurity phases in the microstructure. The optimized process parameters for GPS process are identified as: a mean particle size of 1.03 μm, a sintering temperature of 1860 °C and a retention time of 60 min; the resulting mechanical properties are: a relative density of 95.1%, a micro-hardness of 1718 kgf/mm 2 and a fracture toughness of 5.97 MPa m 1/2 . The width of particles size distribution has a significant effect on the density and hardness of the sintered material however the width of particles size distribution is dependent on the original particle size. Finally, ultra-fine particles increase the chance of conglomeration and sub-micron structures. The conglomeration of ultra-fine particles hinders the filling of porosities during sintering and lowers the density and hardness of the material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Consolidation and properties of binderless sub-micron tungsten carbide by field-activated sintering10.1016/j.ijrmhm.2004.08.003 ↗
2. Consolidation of ultrafine binderless cemented carbide by spark plasma sintering10.1016/S1006-706X(08)60056-4 ↗
3. Properties of ultra-fine grain binderless cemented carbide ‘RCCFN’10.1016/0263-4368(95)92676-B ↗
4. Properties and microstructure of WC–TiC–Co and WC–TiC–Mo2C–Co(Ni) cemented carbide
5. An investigation of the influence of powder particle size on microstructure and hardness of bulk samples of tungsten carbide10.1016/S0032-5910(01)00391-6 ↗
6. Influence of processing parameters on the formation of WC–Co nanocomposite powder using a polymer as carbon source
7. Structure and properties of bulk nano-structured WC–CO alloy by mechanical alloying10.1016/S0925-8388(97)00252-1 ↗
8. On the formation of very large WC crystals during sintering of ultrafine WC–Co alloys10.1016/S0263-4368(01)00069-5 ↗
9. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
10. Sparking plasma sintering of nanometric tungsten carbide10.1016/j.ijrmhm.2008.06.004 ↗
11. Effects of lower cobalt binder concentrations in sintering of tungsten carbide10.1016/j.msea.2006.05.118 ↗
12. Introduction to powder metallurgy
13. Powder metallurgy technology
14. Bulk ultrafine binderless WC prepared by spark plasma sintering10.1016/j.scriptamat.2005.10.014 ↗
15. Chemical processing of nanophase WC–Co composite powder10.1179/mst.1990.6.10.953 ↗
16. Tribological study of WC produced by plasma pressure compaction10.1016/j.ijrmhm.2005.06.006 ↗
17. Consolidation of ultra fine WC and WC–Co hard materials by pulsed current activated sintering and its mechanical properties10.1016/j.ijrmhm.2005.11.004 ↗
18. Lin YY. A study of fabrication and cutting of tungsten carbide materials. N Chin-Yi Univers Techn, Master thesis, 2005.
19. Microstructures of binderless tungsten carbides sintered by spark plasma sintering process10.1016/S0921-5093(03)00151-5 ↗
20. Properties and rapid consolidation of ultra-hard tungsten carbide10.1016/j.jallcom.2009.09.040 ↗