journal article·2013-01

Research of surfaces and interfaces increasing during planetary ball milling of nanostructured tungsten carbide/cobalt powder

M.I. Dvornik, A.V. Zaytsev

Publisher page

Abstract

Abstract This work is devoted to researching the kinetics of the formation of particle surfaces and interfaces during the milling of nanostructured tungsten carbide/cobalt (WC–Co) powders in a planetary ball mill. The power consumption of the mill and the energy transferred to the powder are measured. The contents of Co and WC at the surface of the particle, the specific surface areas (SSAs) of the particles, and the SSAs of the WC phase and the WC grains were determined using various methods. The features of the SSA analysis using the laser diffraction method and the Brunauer–Emmett–Teller (BET) gas adsorption method are discussed. The specific interface areas (SIAs) of the WC/WC and WC/Co boundaries were calculated based on the obtained data. The SSA of the powder and the SIA of the WC/WC linearly increased during the beginning of the milling process, the rates of growth subsequently decreased, and the SSA and the SIA approached their limits. The SIA of WC/Co increases linearly without limit. The employed model made it possible to determine the milling rates and the limits of the SSA and the SIA. Based on the obtained results and literature data, the energy that was stored in different surfaces and interfaces was calculated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. A history of fine grained hardmetal10.1016/0263-4368(95)92671-6 ↗
2. Tungsten carbide10.1021/ie50602a018 ↗
3. Microstructural evolution during solid-state sintering of ball-milled nanocomposite WC–10 mass%Co powders
4. Hot isostatic pressing of ultrafine tungsten carbide–cobalt hardmetals10.1023/A:1020048105585 ↗
5. The wear of ultrafine WC–Co hard metals10.1016/S0043-1648(01)00667-6 ↗
6. Submicron and ultrafine grained hardmetals for microdrills and metal cutting inserts10.1016/S0263-4368(01)00066-X ↗
7. Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide — a review10.1016/j.ijrmhm.2008.07.011 ↗
8. General aspects and limits of conventional ultrafine WC powder manufacture and hard metal production10.1016/0263-4368(95)92674-9 ↗
9. Chemical vapor synthesis and characterization of nanosized WC–Co composite powder and post-treatment10.1021/ie800322y ↗
10. Chemical processing of nanostructured cemented carbide10.1023/A:1008665301338 ↗
11. Two step synthesis of nanostructured tungsten carbide–cobalt powders10.1016/S1359-6462(01)00668-6 ↗
12. Production and characterization of ultrafine WC powders10.1016/S0263-4368(01)00067-1 ↗
13. Effect of milling temperature on the synthesis and consolidation of nanocomposite WC–10Co powders10.1016/j.ijrmhm.2008.03.007 ↗
14. Effects of ball milling time on the synthesis and consolidation of nanostructured WC–Co composites10.1016/j.ijrmhm.2009.05.006 ↗
15. Parameters optimization in the planetary ball milling of nanostructured tungsten carbide/cobalt powder10.1016/j.ijrmhm.2007.08.005 ↗
16. Production of nanocrystalline powders by high-energy ball milling: model and experiment10.1088/0957-4484/19/26/265302 ↗
17. Particle size characterization of ultrafine tungsten powder10.1016/S0263-4368(00)00051-2 ↗
18. Nanostructured WC/Co composite powder prepared by high energy ball milling10.1016/j.scriptamat.2003.08.009 ↗
19. Microstructural and mechanical characterization of high energy ball milled and sintered WC–10 wt%Co–xTaC nano powders10.1016/j.ijrmhm.2009.02.001 ↗
20. Characterizations of ball-milled nanocrystalline WC–Co composite powders and subsequently rapid hot pressing sintered cermets10.1016/S0167-577X(03)00011-9 ↗
21. Properties of nanostructured tungsten carbide and their rapid consolidation by pulsed current activated sintering10.1088/0031-8949/2010/T139/014043 ↗
22. Synthesis and characterizations of ball-milled nanocrystalline WC and nanocomposite WC–Co powders and subsequent consolidations10.1016/S0925-8388(00)01155-5 ↗
23. Synthesis and processing of nanostructured WC–Co materials10.1023/A:1016553426227 ↗
24. Synthesis of WC and WC–Co cermets by mechanical alloying and subsequent hot isostatic pressing10.1016/S1359-6462(97)00410-7 ↗
25. Synthesis of nanocrystalline cubic substoichiometric WC1−z powders by mechanochemical technology10.1023/A:1004880221909 ↗
26. Effect of C and milling parameters on the synthesis of WC powders by mechanical alloying10.1016/j.ijrmhm.2009.09.006 ↗
27. Production of nanostructured WC–Co powder by ball milling10.1016/j.ijrmhm.2008.06.005 ↗
28. Nanostructured WC–Co alloy prepared by mechanical alloying10.1016/S0925-8388(96)02678-3 ↗
29. Preparation and structure of bulk nanostructured WC–Co alloy by high energy ball-milling10.1023/A:1018525213450 ↗
30. Structure and properties of bulk nano-structured WC–Co alloy by mechanical alloying10.1016/S0925-8388(97)00252-1 ↗
31. Synthesis of nanocrystalline WC single-phase refractory via mechanical milling
32. Klug · 1974
33. A method of calculating the integral breadths of Debye–Scherrer lines10.1017/S0305004100021988 ↗
34. Power measurements during mechanical milling. An experimental way to investigate the energy transfer phenomena10.1016/1359-6454(95)00226-X ↗
35. A mathematical analysis of milling mechanics in a planetary ball mill10.1016/S0254-0584(00)00289-3 ↗
36. Hodakov · 1972 · 307
37. Material and energy interactions between milling bodies milled particles, and milling environment10.1023/A:1011330024893 ↗
38. The energy efficiency of ball milling in comminution10.1016/S0301-7516(02)00039-X ↗
39. Salman · 2007
40. Evolution of vacancy densities in powder particles during mechanical milling10.1016/S0921-4526(02)01459-X ↗
41. Modelling breakage and reagglomeration during fine dry grinding in ball milling devices10.1016/j.powtec.2009.04.009 ↗
42. Calculation of flocculation and coalescence rates for concentrated dispersions using emulsion stability simulations10.1021/la048433t ↗
43. Co-phase penetration of WC (1010)/WC(1010) grain boundaries from first principles10.1103/PhysRevB.67.115415 ↗
44. Cobalt layers crystallized on the WC(100) surface: spin-polarized ab initio study10.1016/j.ijrmhm.2010.10.005 ↗
45. Surface energies and work functions of the transition metal carbides10.1016/j.susc.2004.03.050 ↗
46. First-principles simulations of metal–ceramic interface adhesion: Co/WC versus Co/TiC10.1103/PhysRevB.65.045408 ↗
47. First principle simulation of the Co layers behavior on a surface of hexagonal tungsten carbide10.1016/j.phpro.2012.01.033 ↗
48. The fracture toughness of WC–Co two-phase alloys — a preliminary model10.1007/BF02700449 ↗
49. Morphology of WC grains in WC–Co alloys: theoretical determination of grain shape10.1016/j.actamat.2006.10.013 ↗
50. Effect of Σ2 grain boundaries on plastic deformation of WC–Co cemented carbides10.1016/j.msea.2005.09.095 ↗
51. Relative grain boundary area and energy distributions in nickel10.1016/j.actamat.2009.06.004 ↗