journal article·2004-07

Sintering shrinkage of WC–Co and WC–(Ti,W)C–Co materials with different carbon contents

A. Petersson

Publisher page

Abstract

Abstract The sintering of cemented carbides based on WC–Co with different carbon contents and additions of (Ti,W)C has been studied by dilatometry and analysed in terms of a densification model. Shrinkage starts around 1000 °C for WC–Co and in the range 1100–1250 °C for WC–(Ti,W)C–Co. Although a high carbon content initially delays shrinkage in WC–Co it leads eventually to high shrinkage rates and a fully dense material in the shortest time. Practically no difference was found between low and medium carbon contents. For WC–(Ti,W)C–Co, onset of shrinkage depends more strongly on composition and increases with decreasing carbon content. Shrinkage rates are described with a proposed model based on uniaxial viscosity, viscous equivalent of Poisson’s ratio and sintering stress. The three densification stages observed for WC–Co materials reduce to two stages for WC–(Ti,C)C–Co, where higher apparent activation energies also are observed during solid state sintering.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Brookes · 1987
2. A study of the effect of carbon content on the structure and properties of sintered WC–Co alloys
3. Uhrenius B. Phase equilibria and the sintering of cemented carbides. In: Proceedings of powder metallurgy world congress PM’94, vol 2. Les Ulis: Les Editions de Physique; 1994. p. 1443–50
4. A review of parameters influencing some mechanical properties of tungsten carbide-cobalt alloys10.1179/pom.1970.13.25.002 ↗
5. Freytag J, Exner HE. The influence of tungsten and carbon additions on the sintering and the magnetic properties of WC-12Co cemented carbides. In: Hausner HH, Taubenblat PV, editors. Modern developments in powder metallurgy, vol. 10 Ferrous and non-ferrous P/M materials. Princeton: MPIF-APMI; 1977, p. 511–23
6. Sinterverlauf eines WC-12 Gew.% Co Hartmetalls mit unterschiedlicher Bindephasenzusammensetzung
7. The liquid-phase sintering of titanium carbide10.1179/pom.1976.19.3.162 ↗
8. Densification mechanisms in the tungsten carbide-cobalt system10.1179/pom.1976.19.1.38 ↗
9. Wetting of metallic carbides by liquid copper, nickel, cobalt and iron
10. Development of a database for cemented carbides: Thermodynamic modeling and experiments10.1007/s11669-001-0028-8 ↗
11. Modeling of solid state sintering of cemented carbides
12. A general morphological approach of sintering kinetics: Application to WC–Co solid phase sintering10.1016/S1359-6454(98)00055-X ↗
13. Submicron and ultrafine grained hardmetals for microdrills and metal cutting inserts10.1016/S0263-4368(01)00066-X ↗
14. Constitutive Behaviour of WC–Co Materials with different grain size sintered under load10.1016/j.actamat.2003.12.024 ↗
15. Petersson A, Ågren J. Modelling WC–Co sintering shrinkage-effect of carbide grain size and cobalt content. Unpublished manuscript, 2004
16. Charakterisierung der Bindephase von WC–Co Hartmetallen über magnetische Eigenschaften
17. The Thermo-Calc databank system10.1016/0364-5916(85)90021-5 ↗
18. W content in Co binder during sintering of WC–Co10.1016/S1359-6454(97)00459-X ↗
19. M6C formation during sintering of cemented carbides containing (Ti,W)C10.1016/j.ijrmhm.2003.11.001 ↗
20. On constrained sintering—II. Comparison of constitutive models10.1016/0001-6160(88)90190-3 ↗
21. Solid state sintering of cemented carbides––an experimental study
22. Microstructure evolution in the cemented carbides WC–Co I. Effect of the C/W ratio on the morphology and defects of the WC grains10.1002/1521-396X(200209)193:2<271::AID-PSSA271>3.0.CO;2-O ↗
23. Variation of WC grain shape with carbon content in the WC–Co alloys during liquid-phase sintering10.1016/S1359-6462(02)00464-5 ↗