Abstract
Abstract WC-Co has excellent mechanical properties at a temperature below 700 °C, but above it, the mechanical properties of WC-Co decrease severely because of the oxidation effect. In the present study, the addition of metal silicide of CrSi2 was considered to enhance the oxidation resistance of cementite carbide. The WC-12Co compacts containing 0, 12.5, and 25 wt% CrSi2 were prepared using mechanical alloying and spark plasma sintering techniques at 1150 °C. According to the results of metallographic characterization, the sintered WC-12Co is composed mainly of WC and Co phases. The addition of CrSi2 leads to the formation of new phases as CrSi, CoSi, Co6W6C, and SiC depending on the compact composition. It is found that the WC-12Co compact with 12.5 wt% CrSi2 content exhibits a lower measured density and higher hardness compared to that of CrSi2-free compact. After the first cycle of exposure at 900 °C, the WC-12Co is severely oxidized, forming porous and crack oxide scales. On the contrary, the addition of 12.5 wt% CrSi2 shows the lowest mass gain and displays the most resistance to oxidation attributed to the formation of mainly SiO2 scales. Further increase in CrSi2 concentration, however, the alloy compact experiences breakaway oxidation after the fifth cycle of exposure. Accordingly, it can be proposed that the addition of 12.5 wt% CrSi2 is the most promising composition to allow the cemented carbide used at high temperatures and oxidizing atmospheres.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Oxidation behaviour of hard and binder phase modified WC-10Co cemented carbides10.1007/BF00729663 ↗
2. Oxidation behavior of WC–Co cemented carbide in elevated temperature10.1088/2053-1591/aad535 ↗
3. Oxidation-induced strength degradation of WC–Co hardmetals10.1016/S0263-4368(01)00033-6 ↗
4. Kinetics and oxidation behavior of laser clad WC-Co and Ni/WC-Co coatings10.1016/j.ceramint.2018.04.087 ↗
5. Kinetics inversion in isothermal oxidation of uncoated WC-based carbides between 450 and 800°C10.1016/j.corsci.2008.12.022 ↗
6. Oxidation of ultrafine-cemented carbide prepared from nanocrystalline WC–10Co composite powder10.1016/j.ceramint.2007.07.029 ↗
7. High-temperature oxidation behaviour of WC-FeAl composite fabricated by spark plasma sintering10.1016/j.ceramint.2018.06.168 ↗
8. Influence of WC replacement by TiC and (Ta,Nb)C on the oxidation resistance of Co-based cemented carbides10.1016/j.ijrmhm.2008.12.009 ↗
9. The selective oxidation behaviour of WC–Co cemented carbides during the early oxidation stage10.1016/j.corsci.2015.02.033 ↗
10. Mechanism of the early stages of oxidation of WC–Co cemented carbides10.1016/j.corsci.2015.11.007 ↗
11. Oxidation behavior of WC-Co10.1016/0921-5093(95)10145-4 ↗
12. Comparison of the oxidation behaviour of WC–Co and WC–Ni–Co–Cr cemented carbides10.1016/j.corsci.2011.05.006 ↗
13. Enhanced mechanical properties and oxidation resistance of tungsten carbide-cobalt cemented carbides with aluminum nitride additions10.1016/j.ceramint.2017.01.145 ↗
14. Oxidation of WC-Co, WC-Ni and WC-Co-Ni hard metals in the temperature range 500–800 °C10.1016/0263-4368(96)00009-1 ↗
15. Liquid phase sintering and oxidation resistance of WC–Ni–Co–Cr cemented carbides10.1016/j.ijrmhm.2010.02.010 ↗
16. Oxidation behavior of tungsten carbide-6% cobalt cemented carbide10.1007/s13632-018-0493-7 ↗
17. Comparison of the wear behavior of WC/(FeAl-B) and WC-Co composites at high temperatures10.1016/j.ijrmhm.2017.05.003 ↗
18. MoSi2 and other Silicides as high temperature structural materials
19. Effect of microstructure on oxidation resistance of MoSi2 fabricated by spark plasma sintering10.1016/j.vacuum.2003.12.081 ↗
20. Classification of oxidation behavior of disilicides10.4028/www.scientific.net/SSP.127.227 ↗
21. Mechanical alloying10.1146/annurev.ms.13.080183.001431 ↗
22. Materials synthesis by mechanical alloying10.1146/annurev.ms.19.080189.001005 ↗
23. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
24. Spark plasma sintering (SPS) method, systems, and applications
25. Spark plasma sintering
26. High temperature cyclic oxidation resistance of 50Cr-50Al coatings mechanically alloyed on low carbon steel10.1016/j.jallcom.2017.10.163 ↗
27. HSC Chemistry Software Version 9.8.1.2 · 2019
28. Experimental investigation and thermodynamic assessment of the C–Co–Fe–Ni–W system10.1016/j.ijrmhm.2015.07.021 ↗
29. Thermodynamics of Cr2O3, FeCr2O4, ZnCr2O4, and CoCr2O410.1016/j.jct.2007.03.001 ↗
30. The influence of chromium oxide on the sintering behavior of silicon nitride10.1111/j.1744-7402.2012.02814.x ↗
31. Electrical conductivity and thermal expansion of spinels at elevated temperatures10.1111/j.1551-2916.2007.01522.x ↗
32. Additivity of the coefficient of thermal expansion in silicate optical fibers10.1364/OL.42.003650 ↗
33. Phase relationships in the system Cr-W-O and thermodynamic properties of CrWO4 and Cr2WO610.1007/BF00552303 ↗
34. Microstructure and cyclic oxidation behavior of W–Cr alloys prepared by sintering of mechanically alloyed nanocrystalline powders10.1016/j.ijrmhm.2012.08.015 ↗