Effect of ZrO2 and MgO added in alumina on the physical and mechanical properties of spark plasma sintered nanocomposite

K.L. Meena, D. Benny Karunakar

Publisher page

Abstract

Abstract The aim of the present research work was to investigate the effect on the properties such as density, surface roughness, microhardness, fracture toughness and microstructure added with MgO and ZrO2 in an alumina matrix. The magnesia-zirconia toughened alumina spark plasma sintered nanocomposite samples were developed successfully and found the suppressing grain growth and crack free microstructure. No damage was found due to thermal shock up to 1350 °C. The amount of ZrO2was added with 5 vol%, 10 vol% and 15 vol%, while MgO added with 0.5 vol%, 1 vol% and 2 vol% in an aluminamatrix. Each composition was weighed and mixed together. After that, the powders were pressed under the rapid heating at the sintering temperature of 1250 °C, 1300 °C and 1350 °C and for 5 min holding time under pressure of 60 MPa simultaneously. The optimum properties were found with the compositions of 10 vol% of ZrO2, 1 vol% of MgO in the Al2O3 matrix. It showed highest relative density (99.68%), minimum surface roughness (1.123 μm), highest microhardness (19.46 GPa) and minimum average grain size (0.595 μm). The highest fracture toughness was found to be 6.7 MPa.m1/2 the added with 15 vol% of ZrO2,1 vol% of MgO in the Al2O3 matrix for the holding time 5 min and a sintering temperature of 1300 °C. The X-ray diffraction analyses indicate the presence of major phases were ZrO2, α-Al2O3, MgO, magnesia phase with minor peaks of the secondary phase MgAl2O4. This was found due to chemical reactions between the composite constituents present in the matrix during the sintering. Uniform microstructure was observed using a field emission scanning electron microscope and obtained the sub-micron level of grain size without any significant increases of grain size. The developed compositehas high hardness and toughness to make it more suitable for applications such as ballistic armor and thermal barrier coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Effect of MgO particle size on the microstructure, mechanical properties and wear performance of ZTA-MgO ceramic cutting inserts10.1016/j.ijrmhm.2011.02.002 ↗
2. Automotive and industrial applications of structural ceramics in Japan10.1016/j.jeurceramsoc.2007.09.016 ↗
3. The nanosized microstructure of Al2O3-ZrO2(Y2O3) eutectics fabricated by laser engineered net shaping10.1016/j.scriptamat.2014.09.026 ↗
4. Yttria stabilized Al2O3–ZrO2 eutectic crystal fibers grown by the laser heated pedestal growth (LHPG) method10.1016/j.optmat.2010.02.003 ↗
5. Effect of sintering time on biaxial strength of zirconium dioxide10.1016/j.dental.2008.05.011 ↗
6. Microwave versus conventional sintering: a review of fundamentals, advantages,and applications10.1016/j.jallcom.2010.01.068 ↗
7. Microwave sintering and mechanical properties of Y-TZP/20 wt10.1016/S0921-5093(00)00812-1 ↗
8. Dense nanostructured zirconia by two stage conventional/hybrid microwave sintering10.1016/j.jeurceramsoc.2007.09.002 ↗
9. Improvement of microstructural properties of 3Y-TZP materials by conventional and non-conventional sintering techniques10.1016/j.ceramint.2011.06.035 ↗
10. Processed by different methods
11. Preparation and characterization of an Al2O3-ZrO2 nanocomposite, part I: powder synthesis and transformation behavior during fracture10.1016/j.compositesa.2006.01.005 ↗
12. Two-step sintering of fine alumina-zirconia ceramics10.1016/j.ceramint.2008.08.001 ↗
13. Mechanical properties of zirconia toughened alumina with 10-24vol. % 1Y-TZP reinforcement10.1016/j.jeurceramsoc.2012.06.019 ↗
14. Microstructure and mechanical properties of alumina 5 vol. % zirconia nanocomposites prepared by powder coating and powder mixing routes10.1016/j.ceramint.2012.06.078 ↗
15. Effect of yttria content on the zirconia unit cell parameters10.1111/j.1551-2916.2011.04862.x ↗
16. Rapid densification of yttria-stabilized tetragonal zirconia by electric current-activated/assisted sintering technique10.1111/j.1551-2916.2010.04235.x ↗
17. Thermal conductivity of plasma-sprayed monolithic and multilayer coatings of alumina and Yttria-stabilizedzirconia10.1111/j.1151-2916.1999.tb01816.x ↗
18. Thermal properties of ceria and yttria partially stabilized zirconia thermal barrier coatings10.1016/0257-8972(89)90049-2 ↗
19. Superplastic deformation mechanisms during creep of alumina-zirconia composites10.1016/S1359-6454(97)89771-6 ↗
20. Superplastic behavior of a 20% Al2O3/YTZ ceramic composite10.1016/0036-9748(89)90432-8 ↗
21. Superplastic deformation of Al2O3/Y-TZP particulate composites and laminates10.1016/j.actamat.2004.08.008 ↗
22. Improvement of tensile ductility in high-purity alumina due to magnesia addition10.1016/0956-7151(92)90458-Q ↗
23. High-strain-rate superplasticity in Y2O3- stabilized tetragonal ZrO2dipersed with 30 vol% MgAl2O4 spinel10.1111/j.1151-2916.2002.tb00377.x ↗
24. Characterization of alumina matrix nanocomposite with ZrO2 inclusions densified by spark plasma sintering10.1016/j.msea.2008.10.022 ↗
25. High-strain-rate superplasticity in Y2O3- stabilized tetragonal ZrO2 dispersed with 30 vol. % MgAl2O4 spinel10.1111/j.1151-2916.2002.tb00377.x ↗
26. A high-strain-rate superplastic ceramic10.1038/35095025 ↗
27. Enhanced tensile ductility in ZrO2-Al2O3-spinel composite ceramic10.1016/S1359-6462(02)00300-7 ↗
28. Machinability of hardened steel using alumina-based ceramic cutting tools10.1016/S0263-4368(03)00004-0 ↗
29. Fracture toughness measurements of LPS-SiC: a comparison of the indentation technique and the SEVNB method10.1590/S1516-14392005000200004 ↗
30. Quinn · 2007 · 45
31. Determination of fracture toughness using the area of micro-cracktracks left in brittle materials by Vickers indentation test
32. Maji · 2017 · 2 · 4
33. Microstructural coarsening of zirconia-toughened alumina composites10.1111/j.1551-2916.2005.00374.x ↗
34. Microhardness and fracture toughness of dental materials by indentation method10.1002/jbm.b.30371 ↗
35. Mechanical properties of alumina-zirconia composites for ceramic abutments10.1590/S1516-14392004000400021 ↗
36. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
37. Instrumented and Vickers indentation for the characterization of stiffness, hardness and toughness of zirconia toughened Al2O3 and SiC armor10.1016/j.jmst.2015.06.005 ↗
38. Evaluation of KIc of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
39. Medeiros · 2013 · 17 · 9
40. Taffner · 2004 · vol. 9 · 1057
41. The relationship between microstructure and fracture toughness of zirconia toughened alumina (ZTA) added with MgO and CeO210.1016/j.ijrmhm.2013.07.002 ↗
42. Comparison of the microwave and conventional sintering of alumina: effect of MgO doping and particle size10.1111/jace.12320 ↗
43. Densification of fine-grained alumina ceramics doped by magnesia, yttria and zirconia evaluated by two different sintering models10.1016/j.jeurceramsoc.2014.06.030 ↗