High toughness and strength of Mo-12Si-8.5B-ZrB2 alloy resulting from a bimodal α-Mo grain structure
Source abstract
Abstract
Abstract Designing a bimodal α-Mo grain structure in Mo-12Si-8.5B-ZrB2 alloy was achieved via mechanical alloying followed by hot pressing. This bimodal structure consisted of a major of nano-scaled α-Mo grains and partial micron-scaled α-Mo grains. The effective cooperation of these fine and coarse α-Mo in the Mo-12Si-8.5B-ZrB2 alloy was very beneficial for improving its toughness as well as strength. The high toughness was mainly attributed to the in-situ toughening and crack trapping effects originating from the coarse α-Mo. While the high strength was owing much to the grain boundary strengthening of the fine α-Mo. When the volume fraction ratio of the fine and coarse α-Mo grains was approximately 6:1, the fracture toughness value reached 13.1 MPa·m1/2 in the bimodal alloy, showing a 18% increase compared to an ultrafine-grained alloy. Simultaneously, a high compressive strength with 2998 MPa was also maintained.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Mo-Si-B alloys: developing a revolutionary turbine-engine material10.1557/mrs2003.191 ↗
2. Mo-Si-B alloys for ultrahigh-temperature structural applications10.1002/adma.201200764 ↗
3. High-temperature compression behavior of Mo-Si-B alloys10.1016/j.actamat.2004.08.035 ↗
4. Transient oxidation of Mo-Si-B alloys: effect of microstructure size scale10.1016/j.actamat.2009.06.036 ↗
5. Mechanically alloyed Mo-Si-B alloys with a continuous a-Mo matrix and improved mechanical properties10.1016/j.intermet.2008.04.015 ↗
6. Enhanced oxidation resistance of Mo-12Si-8.5B alloys with ZrB2 addition at 1300 °C10.1016/j.jmst.2017.09.010 ↗
7. Microstructure and mechanical properties of lanthanum oxide-doped Mo-12Si-8.5B (at.%) alloys10.1016/j.jallcom.2013.04.116 ↗
8. Ductility of Mo-12Si-8.5B alloys doped with lanthanum oxide by the liquid-liquid doping method10.1016/j.jallcom.2015.04.047 ↗
9. Ambient to high temperature fracture toughness and fatigue-crack propagation behavior in a Mo-12Si-8.5B (at.%) intermetallic10.1016/S0966-9795(01)00008-5 ↗
10. On the fracture toughness of fine-grained Mo-3Si-1B (wt.%) alloys at ambient to elevated (1300 °C) temperatures10.1016/j.intermet.2011.09.003 ↗
11. Optimization of Mo-Si-B intermetallics10.1007/s11661-005-0166-4 ↗
12. Improved fracture toughness of a Mo-12Si-8.5B-3Zr alloy by grain coarsening and its multiple toughening mechanisms10.1016/j.jallcom.2018.01.398 ↗
13. Microstructure and oxidation resistance of laser-remelted Mo-Si-B alloy10.1016/j.scriptamat.2007.01.025 ↗
14. Enhanced tensile ductility and strength of electrodeposited ultrafine-grained nickel with a desired bimodal microstructure
15. Microstructural evolution of extruded AZ31 alloy with bimodal structure during compression
16. High tensile ductility in a nanostructured metal10.1038/nature01133 ↗
17. A micromechanical model of toughening behavior in the dual-phase composite10.1016/j.ijplas.2010.01.005 ↗
18. Grain growth behavior and hall-Petch strengthening in friction stir processed Al 505910.1007/s11661-014-2492-x ↗
19. The effect of microstructure on fracture toughness and fatigue crack growth behavior in γ-titanium aluminide based intermetallics10.1007/s11661-999-0048-2 ↗
20. Fracture toughness and R-curve behavior of laminated brittle-matrix composites10.1007/s11661-998-0220-0 ↗
21. R-curve behavior of long cracks in alumina10.1111/j.1151-2916.1990.tb05260.x ↗
22. Tensile deformation and fracture mechanism of bulk bimodal ultrafine-grained Al-Mg alloy10.1007/s11661-009-0007-y ↗
23. Effects of lanthanum oxide content on mechanical properties of mechanical alloying Mo-12Si-8.5B (at. %) Alloys10.1016/j.ijrmhm.2013.07.011 ↗
24. Microstructure and improved mechanical properties of ultrafine-grained Mo-12Si-8.5B (at.%) alloys with addition of ZrB210.1016/j.pnsc.2018.04.004 ↗
25. Processing and mechanical properties of a molybdenum silicide with the composition Mo-12Si-8.5B (at.%)10.1016/S0966-9795(00)00093-5 ↗
26. Fractal aspects of ductile and cleavage fracture surfaces10.1016/j.engfracmech.2009.11.009 ↗
27. Flow characteristics of highly constrained metal wires10.1016/0001-6160(89)90069-2 ↗
28. A three-dimensional analysis of crack trapping and bridging by tough particles10.1016/0022-5096(91)90026-K ↗
29. Ambient- to elevated-temperature fracture and fatigue properties of Mo-Si-B alloys: role of microstructure10.1007/s11661-005-0112-5 ↗
30. Microstructural design of toughened ceramics10.1111/j.1151-2916.1991.tb06872.x ↗
31. On the fracture and fatigue properties of Mo-Mo3Si-Mo5SiB2 refractory intermetallic alloys at ambient to elevated temperatures (25 °C to 1300 °C)10.1007/s11661-003-0325-4 ↗
32. Stoichiometry and mechanical properties of Mo3Si10.1016/S0966-9795(00)00058-3 ↗
33. Mechanical properties of Mo5SiB2 single crystals10.1016/S0921-5093(01)01575-1 ↗
34. The multi-scale microstructure and strengthening mechanisms of Mo-12Si-8.5BxZr (at.%) alloys10.1016/j.ijrmhm.2017.06.007 ↗
35. Hall-Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
36. Mechanical behavior and microstructure of a thermally stable bulk nanostructured Al alloy10.1007/s11661-001-0207-6 ↗
37. Strengthening mechanisms in particulate metal matrix composites10.1016/0956-716X(91)90349-6 ↗