journal article·2009-03

Mechanical properties of carbon-derived Si3N4+SiC micro/nano-composite

Lucia Hegedűsová, Monika Kašiarová, Ján Dusza, Miroslav Hnatko, Pavol Šajgalík

Publisher page

Abstract

Abstract In this study the mechanical properties of a recently developed carbon-derived Si 3 N 4 +SiC micro/nano-composite have been investigated with the aim to study the influence of the SiC addition on the room-temperature strength and high-temperature creep behavior. The bending strength values are in the interval from σ 0 = 675 MPa to σ 0 = 832 MPa with the Weibull modulus of 6.4 and 8.6 The contact strength is changing from σ 0R = 1997 MPa to σ 0R = 1167 with m R = 17 and m R = 15. Fracture origins in the specimens tested in bending are clusters of pores and large SiC grains and in the specimens tested in contact mode cone cracks. The composite exhibits high creep resistance thanks to the changed chemical composition and viscosity of the intergranular phase comparing to the monolithic Si 3 N 4 and due to the interlocked silicon nitride grains by the intergranularly located SiC nanoparticles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. High-temperature properties of Yb-containing Si3N4
2. Grain-boundary-phase crystallization and strength of silicon nitride sintered with YSiAlON glass10.1111/j.1151-2916.1990.tb09803.x ↗
3. New design concept of structural ceramics ceramics nanocomposites10.2109/jcersj.99.974 ↗
4. Silicon nitride/silicon carbide nanocomposite materials: I, fabrication and mechanical properties at room temperature10.1111/j.1151-2916.1998.tb02456.x ↗
5. SiC/Si3N4 nano/micro-composite-processing, RT and HT mechanical properties10.1016/S0955-2219(99)00176-4 ↗
6. Silicon nitride/silicon carbide nanocomposite materials: II, hot strength, creep and oxidation resistance10.1111/j.1151-2916.1998.tb02457.x ↗
7. Si3N4/SiCN nano-composites: influence of sic nanoprecipitates on the creep behaviour10.1016/S0955-2219(98)00128-9 ↗
8. SiC/Si3N4 nanocomposites with excellent high-temperature long-term behaviour10.4028/www.scientific.net/KEM.161-163.377 ↗
9. High-temperature strength and microstructural analysis in Si3N4/20-vol%-Sic nanocomposites10.1111/j.1151-2916.1999.tb01863.x ↗
10. Dusza · 1998 · 187
11. Enhanced creep resistant silicon-nitride-based nanocomposite10.1111/j.1551-2916.2005.00289.x ↗
12. Fett · J Mater Sci Lett · 2002 · 21 · 195510.1023/A:1021668932660 ↗
13. Fett · J Test Eval · 2001 · 29 · 110.1520/JTE12385J ↗
14. Mechanical failure of advanced ceramics: the value of fractography10.4028/www.scientific.net/KEM.223.1 ↗
15. Fractography and fracture mechanics property assessment of advanced structural ceramics10.1179/095066099101528270 ↗
16. Morrell R. Fractography of brittle materials. Measurement good practice guide, No. 14, HMSO, National Physical Laboratory, UK, ISSN, 1999.s1368–6550.
17. Besson · J Eur Ceram Soc · 1998 · 18 · 189310.1016/S0955-2219(98)00128-9 ↗
18. Rendtel · J Am Ceram Soc · 1998 · 81 · 110910.1111/j.1151-2916.1998.tb02457.x ↗
19. Rendtel · J Eur Ceram Soc · 2002 · 22 · 251710.1016/S0955-2219(02)00112-7 ↗
20. Wan · J Am Ceram Soc · 2006 · 89 · 27410.1111/j.1551-2916.2005.00702.x ↗