Microstructure and mechanical properties of liquid–phase sintered W@NiFe composite powders
Source abstract
Abstract
Abstract W–Ni–Fe heavy alloys were obtained by liquid–phase sintering of W@NiFe composite powders. The face–centered cubic NiFe alloys were deposited as a shell on the core of tungsten particle to form W@NiFe composite powders by intermittently electrodeposition. After liquid–phase sintering, W–Ni–Fe heavy alloys had more gradient morphology and shape distortion as the holding time increased. The bending strength and hardness distributed graded at 1470 °C holding for 0.5 h. Top layer of gradient W–Ni–Fe heavy alloys at 1470 °C holding for 0.5 h showed low W W contiguity, no normal growth of W particle size and high sintered density, which led to excellent bending strength (1245 MPa) and hardness (340 HV0.2). The structure and composition of W@NiFe composite powders and the optimization of sintering process parameters were analyzed and discussed. The sintering behavior of W@NiFe composite powders were also investigated in details.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Structure–property correlations of W–Ni–Fe–Mo heavy alloys consolidated using spark plasma sintering10.1088/2053-1591/aae349 ↗
2. GVSN Rao, T K Nandy, effect of alloying addition and microstructural parameters on mechanical properties of 93% tungsten heavy alloys10.1016/j.msea.2015.05.046 ↗
3. Effects of powder mixing technique and tungsten powder size on the properties of tungsten heavy alloys10.1016/S0924-0136(00)00499-4 ↗
4. Microstructure and mechanical properties of mechanically alloyed and solid–state sintered tungsten heavy alloys10.1016/S0921-5093(00)00968-0 ↗
5. Densification behavior of nanocrystalline W–Ni–Fe composite powders prepared by sol–spray drying and hydrogen reduction process10.1016/j.jallcom.2009.09.050 ↗
6. Preparation of W–Ni–Fe heavy alloys by soft chemical method
7. Structure and magnetic properties of electrodeposited Ni87.3Fe11.3W1.4 alloy10.1016/j.powtec.2014.01.017 ↗
8. Microstructural properties of electrochemically prepared NiFe–W powders10.1016/j.matchemphys.2012.04.061 ↗
9. Preparation of fine–grained tungsten heavy alloys by spark plasma sintered W–7Ni–3Fe composite powders with different ball milling time10.1016/j.jallcom.2013.02.014 ↗
10. Zhou · 2015
11. Elaborating the Cu–network structured of the W–Cu composites by sintering intermittently electroplated core–shell powders10.1016/j.jallcom.2018.08.158 ↗
12. Fabrication of W–Ni–Fe alloys with gradient structures10.1016/j.ijrmhm.2012.03.017 ↗
13. Effect of surface carburization on dynamic deformation and fracture of tungsten heavy alloy10.1007/s11661-999-0013-0 ↗
14. Gradient structure induced by molybdenum in 90W–Ni–Fe heavy alloy10.1016/j.ijrmhm.2013.11.017 ↗
15. Structure and properties of electrodeposited Fe–Ni–W alloys with different levels of tungsten content: a comparative study10.1016/j.apsusc.2007.03.068 ↗
16. Electrodeposition and properties of NiW, FeW and FeNiW amorphous alloys: a comparative study10.1016/S0013-4686(00)00437-0 ↗
17. 93W–5.6Ni–1.4Fe heavy alloys with enhanced performance prepared by cyclic spark plasma sintering10.1016/j.msea.2014.01.089 ↗
18. Ni1−xFex (0.1 < x < 0.75) alloy foils prepared from a fluorborate bath using electrochemical deposition10.1016/j.jallcom.2008.06.050 ↗
19. Effect of electrolyte temperature on composition and phase structure of nanocrystalline Fe–Ni alloys prepared by direct current electrodeposition10.1016/j.surfcoat.2012.07.069 ↗
20. Fabrication, characterization, and mechanical properties of 93W–4.9Ni–2.1Fe/95W–2.8Ni–1.2Fe–1Al2O3 heavy alloy composites10.1016/j.msea.2015.04.026 ↗
21. Heating rate effects on microstructural properties of liquid phase sintered tungsten heavy alloys10.1016/j.ijrmhm.2004.01.006 ↗
22. W/NiFe phase interfacial characteristics of liquid–phase sintered W–Ni–Fe alloy10.1016/j.ijrmhm.2006.08.003 ↗
23. Densification behavior of tungsten heavy alloy based on master sintering curve concept10.1007/BF02586116 ↗
24. Gravitational effects on grain coarsening during liquid–phase sintering10.1007/s11661-997-0098-2 ↗
25. Microstructural refinement of W–Ni–Fe heavy alloys by alloying additions10.1007/BF02647738 ↗
26. The effect of contiguity on growth kinetics in liquid–phase sintering10.1007/BF03220917 ↗
27. W–cu composites with homogeneous cu–network structure prepared by spark plasma sintering using core–shell powders10.1016/j.ijrmhm.2019.05.003 ↗
28. Microstructural development and sintering kinetics in ceramic reinforced high speed steel metal matrix composites10.1179/pom.1997.40.2.143 ↗