Microstructure, hardness and mechanical properties of two different unalloyed tantalum wires deposited via wire + arc additive manufacture
Source abstract
Abstract
An innovative way of producing large-scale unalloyed tantalum parts, based on the Wire + Arc Additive Manufacturing process, has been developed in this study. Two different unalloyed tantalum wires have been used to deposit 200-mm-long structures in tantalum. The effect of the wire chemistry on microstructure, hardness, porosity, mechanical properties and strain localisation has been investigated. The deposits showed high integrity and excellent mechanical properties, with yield strength, ultimate tensile strength and elongation as high as 234 MPa, 261 MPa, and 36 %, respectively. Indeed, yield strength was higher than commercially available tantalum, even though, in this study, the grains were large and had a high aspect ratio. Wire + Arc Additive Manufacture has clearly shown the potential to produce tantalum components with relatively low cost and reduced lead time, thus offering a new robust and viable manufacturing route.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. A review of additive manufacturing10.5402/2012/208760 ↗
2. Progress in additive manufacturing10.1007/s11837-015-1323-x ↗
3. Additive manufacturing: technology, applications and research needs10.1007/s11465-013-0248-8 ↗
4. Wire-feed additive manufacturing of metal components: technologies, developments and future interests10.1007/s00170-015-7077-3 ↗
5. Wire + arc additive manufacturing10.1179/1743284715Y.0000000073 ↗
6. Tandem metal inert gas process for high productivity wire arc additive manufacturing in stainless steel10.1016/j.addma.2018.11.022 ↗
7. Microstructure characterization of SS308LSi components manufactured by GTAW-based additive manufacturing: shaped metal deposition using pulsed current arc10.1007/s00170-016-9053-y ↗
8. Microstructural analyses of ATI 718Plus® produced by wire-ARC additive manufacturing process10.1007/s11661-017-4162-2 ↗
9. Microstructure and mechanical properties of wire and arc additive manufactured Ti-6Al-4V10.1007/s11661-012-1444-6 ↗
10. The strengthening effect of inter-layer cold working and post-deposition heat treatment on the additively manufactured Al– 6.3Cu alloy10.1016/j.jmatprotec.2015.11.006 ↗
11. Development of wire + arc additive manufacturing for the production of large-scale unalloyed tungsten components
12. Functionally graded structures of refractory metals by wire arc additive manufacturing
13. Design for Wire + arc additive manufacture: design rules and build orientation selection
14. Tantalum-processing, properties and applications10.1007/BF03220360 ↗
15. New applications for tantalum and tantalum alloys10.1007/s11837-000-0100-6 ↗
16. Tensile properties of annealed tantalum at low temperatures10.1016/0001-6160(55)90060-2 ↗
17. Tantalum and its alloys10.1016/0263-4368(95)94023-R ↗
18. Selective laser melting of pure tantalum: densification, microstructure and mechanical behaviors10.1016/j.msea.2017.09.083 ↗
19. On the solid solution hardening of tantalum by nitrogen and oxygen10.1016/0022-5088(70)90013-5 ↗
20. Strong morphological and crystallographic texture and resulting yield strength anisotropy in selective laser melted tantalum10.1016/j.actamat.2013.04.036 ↗
21. Additively manufactured porous tantalum implants10.1016/j.actbio.2014.12.003 ↗
22. Direct laser processing of a tantalum coating on titanium for bone replacement structures10.1016/j.actbio.2009.11.021 ↗
23. Microstructure of high-strain, high-strain-rate deformed tantalum10.1016/S1359-6454(97)00746-5 ↗
24. Oxidation of Ti-6Al-4V during wire and arc additive manufacture, 3D print
25. Investigation of the benefits of plasma deposition for the additive layer manufacture of Ti-6Al-4V10.1016/j.jmatprotec.2012.02.002 ↗
26. On the origin of microstructural banding in Ti-6Al4V wire-arc based high deposition rate additive manufacturing10.1016/j.actamat.2018.12.038 ↗
27. The chemical state and control of oxygen in powder metallurgy tantalum10.1016/j.msea.2012.01.100 ↗
28. High temperature solid-solubility and phase studies in the system tantalum-oxygen10.1016/0022-5088(72)90062-8 ↗
29. Observation of oxide particles below the apparent oxygen solubility limit in tantalum10.1007/BF02646617 ↗
30. The O-Ta (Oxygen-Tantalum) system10.1007/BF02648373 ↗
31. Effects of oxygen on the mechanical behavior of hydrogenated V, Nb, and ta10.1007/BF02643960 ↗
32. Cyclic plastic deformation of tantalum and niobium at very high numbers of cycles10.1016/S0921-5093(01)01446-0 ↗
33. The cyclic hardening and saturation behaviour of copper single crystals10.1016/0025-5416(78)90174-X ↗
34. Fabrication and mechanical properties of powder metallurgy tantalum prepared by hot isostatic pressing10.1016/j.ijrmhm.2014.09.012 ↗
35. Inverse hall-Petch relationship in nanocrystalline tantalum10.1016/j.msea.2013.05.024 ↗
36. Molecular dynamics simulations of shock compression of nickel: from monocrystals to nanocrystals10.1016/j.actamat.2008.07.052 ↗
37. Additive manufactured Ti-6A1-4V using welding wire: comparison of laser and arc beam deposition and evaluation with respect to aerospace material specifications10.1016/j.phpro.2010.08.087 ↗
38. Microstructure of Ti-6Al-4V specimens produced by shaped metal deposition10.3139/146.110217 ↗