journal article·2012-03

Oxidation behavior of WC–Co hard metal with designed multilayer coatings by CVD

Xiangming Chen, Huiqun Liu, Qinghua Guo, Shunping Sun

Publisher page

Abstract

Abstract Multilayer coatings composed of TiN, TiCN, α-Al 2 O 3 and κ-Al 2 O 3 were designed and then deposited on WC–Co alloy by chemical vapor deposition (CVD) technique, the samples of WC–Co alloy with multilayer coatings were oxidized in the temperature range of 600 °C–950 °C for various times in a Muffle furnace, and weight gain was measured by electronic balance. Phase component and microstructure evolution of coating samples after oxidation were investigated by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results showed that the oxidation resistance of WC–Co alloy was improved markedly after deposition of multilayer coatings. The oxidation kinetics of multilayer coating samples obeyed linear law and diffusion-controlled parabolic law at different oxidation conditions. The oxidation product of coatings was rutile TiO 2 . The sample exhibited excellent oxidation resistance when the outermost layer was α-Al 2 O 3 , which was consistent to the results of apparent activation energy of oxidation reaction. The oxidation resistance of multilayer coatings was improved with the increase of thickness of κ-Al 2 O 3 layer. The κ-Al 2 O 3 transformed into α-Al 2 O 3 over 900 °C. The interface between TiN and TiCN disappeared in the coating sample without α-Al 2 O 3 and κ-Al 2 O 3 layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. 2000
2. Determination of the optimum TiN coating thickness on WC inserts for machining carbon steels10.1016/j.jmatprotec.2004.04.277 ↗
3. Wear mechanism of TiN coated carbide and uncoated cermets tools at high cutting speed applications10.1016/j.jmatprotec.2004.04.352 ↗
4. Abrasive wear behavior of high speed steel and hard metal coated with TiAlN and TiCN10.1016/S0043-1648(01)00638-X ↗
5. Multifunctional multi-component PVD coatings for cutting tools10.1016/j.surfcoat.2005.08.105 ↗
6. Mechanical properties and oxidation behaviour of (Al, Cr)N and (Al, Cr, Si)N coatings for cutting tools deposited by HPPMS10.1016/j.tsf.2008.06.050 ↗
7. Nanoindentation hardness, texture and microstructure of α-Al2O3 and κ-Al2O3 coatings10.1016/j.tsf.2007.10.078 ↗
8. α-Alumina coatings on WC/Co substrates by physical vapor deposition10.1016/j.ijrmhm.2008.10.007 ↗
9. Effect of Si addition on microstructure and mechanical properties of Ti–Al–N coating10.1016/j.ijrmhm.2010.05.001 ↗
10. Nanocrystalline CVD diamond coatings for drilling of WC–Co parts10.1016/j.ijrmhm.2011.04.008 ↗
11. Oxidation behavior of WC–Co10.1016/0921-5093(95)10145-4 ↗
12. Oxidation-induced strength degradation of WC–Co hardmetals10.1016/S0263-4368(01)00033-6 ↗
13. Kinetics inversion in isothermal oxidation of uncoated WC-based carbides between 450 and 800°C10.1016/j.corsci.2008.12.022 ↗
14. Evaluation of wear resistance of AlSiTiN and AlSiCrN nanocomposite coatings for cutting tools10.1016/j.cirp.2008.03.103 ↗
15. Investigation of wear behavior and chip formation for cutting tools with nano-multilayered TiAlCrN/NbN PVD coating10.1016/j.ijmachtools.2007.10.021 ↗
16. Abrasive wear of multilayer κ-Al2O3-Ti(C, N) CVD coatings on cemented carbide10.1016/j.wear.2007.01.113 ↗
17. Abrasive wear behavior of high speed steel and hard metal coated with TiAlN and TiCN10.1016/S0043-1648(01)00638-X ↗
18. Influence of WC replacement by TiC and (Ta, Nb)C on the oxidation resistance of Co-based cemented carbides10.1016/j.ijrmhm.2008.12.009 ↗
19. Liquid phase sintering and oxidation resistance of WC–Ni–Co–Cr cemented carbides10.1016/j.ijrmhm.2010.02.010 ↗
20. Oxidation of WC–Co, WC–Ni and WC–Co–Ni hard metals in the temperature range 500–800°C10.1016/0263-4368(96)00009-1 ↗
21. Microstructural investigation of the κ-Al2O3→α-Al2O3 transformation in multilayer coatings of chemically vapour deposited κ-Al2O310.1016/0040-6090(94)90340-9 ↗
22. Oxidation behavior and flexural strength of AIN exposed to air at elevated temperature10.1111/j.1151-2916.1994.tb07264.x ↗