The effect of increasing V content on structure, mechanical and tribological properties of arc evaporated Ti–Al–V–N coatings

M. Pfeiler, K. Kutschej, M. Penoy, C. Michotte, C. Mitterer, M. Kathrein

Publisher page

Abstract

Abstract In the last years, titanium aluminium vanadium nitride (Ti–Al–V–N) coatings have been introduced as possible candidates for low-friction coatings, based on the formation of vanadium oxide above 550 °C. Here we report on the influence of the V content on the mechanical and tribological properties in the temperature range between room temperature (RT) and 500 °C. An industrial-scale cathodic arc evaporation facility was used to deposit coatings from powder metallurgically produced Ti33−xAl67Vx targets, with x ranging from 0 to 25 at%. X-ray diffraction experiments displayed a dual-phase structure with hexagonal and face-centred cubic phases for all compositions. However, a decreasing effect of V on the fraction of hexagonal phase was observed. Hardness and Young’s modulus increased with increasing V content from 21 to 27.5 GPa and from 250 to 350 GPa, respectively. On the contrary, residual compressive stress decreased with increasing V content from −690 to −330 MPa. Investigations on the wear behaviour at RT revealed decreasing wear coefficients with increasing V content, which is related to reduced tribo-chemical reactions of Ti and the test environment. At 500 °C, wear is generally low but increased with increasing V content due to reduced resistance to oxidation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Single layer and multilayer wear resistant coatings of (Ti,Al)N: a review10.1016/S0921-5093(02)00259-9 ↗
2. On structure and properties of sputtered Ti and Al based hard compound films10.1116/1.573708 ↗
3. (Ti–Al)N advanced films prepared by arc process10.1016/0921-5093(91)90519-S ↗
4. Calorimetric evidence for frictional self-adaptation of TiAlN/VN superlattice coatings10.1016/j.surfcoat.2003.09.024 ↗
5. Influence of oxide phase formation on the tribological behaviour of Ti–Al–V–N coatings10.1016/j.surfcoat.2005.08.044 ↗
6. A new low friction concept for high temperatures: lubricious oxide formation on sputtered VN coatings10.1007/s11249-004-8083-z ↗
7. A new low-friction concept for TiAlN based coatings in high-temperature applications10.1016/j.surfcoat.2004.08.022 ↗
8. Determination of growth induced strain and thermo-elastic properties of coatings by curvature measurements10.1016/S0921-5093(01)01979-7 ↗
9. Prediction of phase change in pseudobinary transition metal aluminium nitrides by band parameters method10.1016/j.surfcoat.2004.07.035 ↗
10. The influence of bias voltage on structure and mechanical/tribological properties of arc evaporated Ti–Al–V–N coatings10.1016/j.surfcoat.2007.07.045 ↗
11. Structure, mechanical and tribological properties of sputtered TiAlN coatings10.1016/j.surfcoat.2004.12.008 ↗
12. Effect of aluminium concentration on friction and wear properties of titanium aluminium nitride films10.1016/S0257-8972(03)00936-8 ↗
13. Microstructure and mechanical properties of cathodic arc ion-plated (Al,Ti)N coatings10.1016/S0257-8972(02)00610-2 ↗
14. Influence of the Al distribution on the structure, elastic properties and phase stability of supersaturated TiAlN10.1063/1.2360778 ↗
15. Influence of the testing parameters on the tribological behaviour of self-mated PVD-coatings10.1016/0043-1648(94)90211-9 ↗
16. Dry sliding wear of TiN based ternary PVD coatings10.1016/0043-1648(93)90370-2 ↗
17. The influence of humidity on the fretting behaviour of PVD TiN coatings10.1016/0043-1648(94)06538-1 ↗
18. Transfer of 319 Al alloy to titanium diboride and titanium nitride based (TiAlN, TiCN, TiN) coatings: effects of sliding speed, temperature and environment10.1016/j.surfcoat.2004.10.008 ↗
19. Hutchings · 1992
20. High-temperature tribological characterization of commercial TiAlN coatings10.1088/0953-8984/18/32/S04 ↗
21. Investigating the correlation between nano-impact fracture resistance and hardness/modulus ratio from nanoindentation at 25–500°C and the fracture resistance and lifetime of cutting tools with TiAlN PVD coatings in milling operations10.1016/j.surfcoat.2006.09.118 ↗
22. Oxidation resistance of (Ti, Al, Si)N coatings in air10.1016/S0257-8972(97)00127-8 ↗
23. The beneficial effect of high-temperature oxidation on the tribological behaviour of V and VN coatings10.1007/s11249-007-9241-x ↗