Abstract

The W-0.25 wt%Al 2O 3 alloy was fabricated by a powder metallurgy processing route, including hydrogen reduction, induction sintering and hot swaging. Al 2O 3 particles are absorbed on the surface of W particles with size ranging from 50 to 1000 nm. The microstructure of sintered alloy presents equiaxed grains with an average size of 8.6 μm and TEM result shows that a semi-coherent relationship exists in between W and Al 2O 3. After swaging, the swaged W-0.25 wt%Al 2O 3 alloy with fully dense was obtained. EBSD result indicates most of grains are obviously elongated and the average aspect ratio of W grains is 2.3:1. There is an obvious transition layer with a thickness of approximately 20 nm between W and Al 2O 3 . The interface displays an amorphous feature because of uncoordinated deformation occurred in swaging process. 3-point bend tests show that the ductile-to-brittle transition temperature of sintered alloy is in the range of 350–400 °C. Moreover, the swaged alloy begins to exhibit obvious ductile behavior at 100–200 °C and the bending strength increases with increasing temperature, which reaches a maximum value of 1762 MPa at 400 °C.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Achieving high strength/ductility in bulk W-Zr-Y2O3 alloy plate with hybrid microstructure10.1016/j.matdes.2016.06.012 ↗
2. Development of a helium-cooled divertor concept: design-related requirements on materials and fabrication technology10.1016/j.jnucmat.2004.04.137 ↗
3. Structure evolution of Y2O3 and consequent effects on mechanical properties of W–Y2O3 alloy prepared by ball milling and SPS10.1016/j.msea.2021.142448 ↗
4. Assessment of tungsten for use in the ITER plasma facing components10.1016/S0022-3115(98)00285-2 ↗
5. Hierarchical microstructures enabled excellent low-temperature strength-ductility synergy in bulk pure tungsten10.1016/j.actamat.2022.117765 ↗
6. Solute-induced solid-solution softening and hardening in bcc tungsten10.1016/j.actamat.2017.09.019 ↗
7. Effect of NbC content on microstructure and mechanical properties of W-NbC composites10.1016/j.ijrmhm.2017.09.008 ↗
8. Determination of the DBTT of nanoscale ZrC doped W alloys through amplitude-dependent internal friction technique10.1016/j.msea.2018.01.055 ↗
9. Recrystallization behavior and thermal shock resistance of the W-1.0 wt% TaC alloy10.1016/j.jnucmat.2018.01.042 ↗
10. Thermomechanical properties of TiC particle-reinforced tungsten composites for high temperature applications10.1016/S0263-4368(02)00105-1 ↗
11. Microstructural evolution in single tungsten fiber-reinforced tungsten composites during annealing: recrystallization and abnormal grain growth10.1016/j.jnucmat.2020.152579 ↗
12. Microwave synthesis and properties of fine-grained oxides dispersion strengthened tungsten10.1016/j.jnucmat.2012.03.008 ↗
13. Mechanical properties of a tungsten-23.4 percent rhenium-0.27 percent hafnium-carbon alloy10.1016/0022-5088(71)90028-2 ↗
14. Dilatometric analysis of sintering of tungsten and tungsten with ceria and hafnia dispersions10.1016/0263-4368(93)90074-P ↗
15. W-Y2O3 composites obtained by mechanical alloying and sintering10.1016/j.apt.2020.12.017 ↗
16. Effect of ZrC particle size on microstructure and room temperature mechanical properties of ZrCp/W composites10.1016/j.msea.2010.03.008 ↗
17. Effects of doping route on microstructure and mechanical properties of W-1.0wt.%La2O3 alloys10.1016/S1003-6326(20)65462-0 ↗
18. W-2 wt.%Y2O3 composite: microstructure and mechanical properties10.1016/j.msea.2012.01.011 ↗
19. Microstructure and preparation of an ultra-fine-grained W-Al2O3 composite via hydrothermal synthesis and spark plasma sintering10.1016/j.ijrmhm.2017.12.022 ↗
20. Strengthening mechanism and effect of Al2O3 particle on high-temperature tensile properties and microstructure evolution of W–Al2O3 alloys10.1016/j.msea.2022.142678 ↗
21. Accelerated sintering of high-performance oxide dispersion strengthened alloy at low temperature10.1016/j.actamat.2021.117309 ↗
22. Achieving high strength and ductility in ODS-W alloy by employing oxide@W core-shell nanopowder as precursor10.1038/s41467-021-25283-2 ↗
23. Adhesion strength and bonding mechanism of γ-Fe (111)/α-Al2O3 (0001) interfaces with different terminations10.1016/j.jallcom.2021.159529 ↗
24. Preparation of equiaxed α-Al2O3 by adding oxalic acid10.1016/j.ceramint.2021.08.029 ↗
25. Processing of fine-grained W materials without detrimental phases and their mechanical properties at 200-432 K10.1016/j.msea.2007.03.079 ↗
26. Mechanical properties of tungsten in the transition temperature range10.1016/j.jnucmat.2013.11.019 ↗