Growth mechanism and mechanical property of laminar iridium coating by electrodeposition
Source abstract
Abstract
Abstract Iridium coatings were prepared on rhenium coated graphite by electrodeposition. The Ir coatings were annealed at 1250 °C, 1600 °C and 1950 °C for 7.5 h, respectively. Growth mechanism and mechanical properties of the Ir coatings were investigated. Results showed that the as-received Ir coatings had thickness of about 0.25 mm and characterized as laminar columnar grain structure, which resulted from using higher and lower current densities (− 50 mA/cm 2 and − 20 mA/cm 2 ) alternately. Annealing temperature affected mechanical properties of the Ir coating by changing residual stress, defects and grain size of the coating. The average tensile strength of the as-received, 1250 °C-annealed, 1600 °C-annealed, 1950 °C-annealed (in vacuum) Ir coating and 1950 °C-annealed (in hydrogen) was about 250 MPa, 270 MPa, 234 MPa, 117 MPa and 91 MPa respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Ceramic coatings for carbon–carbon composites
2. The influence of carbon fiber surface treatment on the mechanical properties of carbon/carbon composites10.1016/0008-6223(80)90049-4 ↗
3. MOFFATT · 1981
4. Protective oxide coatings for iridium/rhenium chambers
5. Reed · 1995
6. Thermal cycling of iridium coatings on isotropic graphite10.1007/BF00354413 ↗
7. Moffatt · 1981
8. Lightweight, inexpensive radiation-cooled advanced composite combustion chamber
9. Ceramic Matrix Composite Thermal Protection Systems and Hot Structures for Hypersonic Vehicles
10. Study on inter-diffusion of iridium/rhenium
11. A long duration and high reliability liquid apogee engine for satellites10.1016/j.actaastro.2004.05.030 ↗
12. Sealing of cracks in the rhenium coating on C/C composites by alloying with cobalt10.1016/j.surfcoat.2014.10.032 ↗
13. Chemical vapor deposition of iridium, platinum, rhodium and palladium10.2320/matertrans.44.1717 ↗
14. Thermal stability of iridium coating prepared by MOCVD10.1016/j.ijrmhm.2008.02.001 ↗
15. Deposition effectiveness investigation of ir film prepared by MOCVD10.1016/S1875-5372(10)60081-1 ↗
16. Processing of iridium and iridium alloys: methods from purification to fabrication10.1595/147106708X333827 ↗
17. Iridium thin films deposited by radiofrequency magnetron sputtering10.1116/1.581029 ↗
18. A novel laser technique for oxidation resistant coating of carbon–carbon composite10.1016/S0008-6223(00)00200-1 ↗
19. Oxidation protective iridium and iridium–rhodium coatings produced by electrodeposition from molten salts10.1149/1.2721466 ↗
20. Enhanced oxygen evolution on an electrodeposited ruthenium+iridium coating on titanium10.1016/0022-0728(95)03873-F ↗
21. Iridium coated rhenium rocket chambers produced by electroforming
22. Production of iridium crucibles by electrolysis of molten salts
23. Effects of current reversal on the structure of iridium deposits obtained by molten-chloride electrolysis
24. Electrodeposition of platinum metals and alloys from chloride melts10.2298/JMMB0302201S ↗
25. Effects of catholic current density and temperature on morphology and microstructure of iridium coating prepared by electrodeposition in molten salt under the air atmosphere10.1016/j.apsusc.2012.11.041 ↗
26. Electroforming of near-net shapes of iridium
27. Iridium coating prepared on rhenium substrate by electrodeposition in molten salt in the air atmosphere10.1016/j.surfcoat.2011.08.058 ↗
28. Rhenium used as an interlayer between carbon–carbon composites and iridium coating: adhesion and wettability10.1016/j.surfcoat.2013.07.013 ↗