Damage characteristics and material removal mechanisms of CVD-SiC in nanotests: A comparative with sintered SiC
Source abstract
Abstract
High sensitivity to crack and damage of chemical vapor-deposited silicon carbide (CVD- SiC) restricts the high-efficiency and low-damage manufacturing of CVD-SiC components. This paper aims to reveal the damage and material removal mechanisms of CVD-SiC after being scratched by diamond abrasives. The mechanical properties, scratching force, depth of ductile-brittle transition, residual depth and material removal damages of the CVD-SiC were discussed by the indentation, nano-scratching experiments, and compared with sintered silicon carbide (SSiC) ceramics. The results demonstrated that the mechanical properties of CVD-SiC are better than SSiC. In terms of hardness and fracture toughness, CVD-SiC demonstrates a 10– 20% and 20– 30% higher level of performance than SSiC, respectively. SSiC exhibits a brittleness level approximately 30% higher than that of CVD-SiC. SSiC ceramics are prone to crack deflection, intergranular fracture and transgranular fracture during indentation, indicating a higher propensity for brittle fracture in SSiC. The crack propagation in CVD-SiC is relatively regular. Both materials undergo the ductile, ductile-brittle transition and brittle stage, and the fluctuation variability of CVD-SiC material is notably lower than that of SSiC during the brittle stage. Compared with SSiC, the residual depth, groove width and transverse force of CVD-SiC are smaller under the same normal load. The critical depth of ductile-brittle transition of CVD-SiC is about 2 times that of SSiC in experimental and theoretical, indicating that CVD-SiC easily achieves ductile grinding. The mechanical properties, crack system and crystal structure of the CVD-SiC and SSiC materials cause the divergences in brittle removal. The radial-median crack system dominates the material removal of CVD-SiC. The disparity of deformations on the inside and outside of the crystal in the brittle stage leads to significant fluctuation variability of force and depth of SSiC during the scratching.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. High thermal conductivity in wafer-scale cubic silicon carbide crystals10.1038/s41467-022-34943-w ↗
2. Enhancement of oxidation resistance of CVD SiC coated Cf/C-SiC hybrid composite tubes processed through Si-infiltration10.1016/j.jallcom.2020.154107 ↗
3. Fabrication of highly dense three-layer SiC cladding tube by chemical vapor infiltration method10.1111/jace.16552 ↗
4. Impact of nuclear environment on hydrothermal corrosion and silica transport for CVD SiC in light water reactors10.1016/j.jnucmat.2021.153155 ↗
5. Development of SiC ultra light mirror for large space telescope and for extremely huge ground based telescope
6. Materials removal mechanism and multi modes feature for silicon carbide during scratching10.1016/j.ijmecsci.2022.107719 ↗
7. Research on grinding of biological tissue
8. Models of grinding-induced surface and subsurface damages in fused silica considering strain rate and micro shape/geometry of abrasive10.1016/j.ceramint.2021.05.220 ↗
9. A comparative study: surface characteristics of CVD-SiC ground with cast iron bond diamond wheel10.1016/S0890-6955(99)00077-2 ↗
10. Evaluation of surface characteristics of ground CVD-SiC using cast iron bond diamond wheels10.1016/S0141-6359(00)00056-8 ↗
11. Optical polishing and characterization of chemical vapour deposited silicon carbide mirrors for space applications
12. Damage-free finishing of CVD-SiC by a combination of dry plasma etching and plasma-assisted polishing10.1016/j.ijmachtools.2016.11.002 ↗
13. Anisotropy dependence of material removal and deformation mechanisms during nanoscratch of gallium nitride single crystals on (0001) plane10.1016/j.apsusc.2021.152028 ↗
14. Suet to.The material removal and the nanometric surface characteristics formation mechanism of TiC/Ni cermet in ultra-precision grinding10.1016/j.ijrmhm.2021.105494 ↗
15. Grinding mechanism of titanium alloy: research status and prospect10.51393/j.jamst.2020001 ↗
16. Molecular dynamics simulation of the material removal in the scratching of 4H-SiC and 6H-SiC substrates10.1088/2631-7990/abc26c ↗
17. Atomistic investigation of machinability of monocrystalline 3C–SiC in elliptical vibration-assisted diamond cutting10.1016/j.ceramint.2020.09.078 ↗
18. Tip-based nanomanufacturing process of single crystal SiC: ductile deformation mechanism and process optimization10.1016/j.apsusc.2019.144039 ↗
19. A material point method based investigation on crack classification and transformation induced by grit geometry during scratching silicon carbide10.1016/j.ijmachtools.2022.103884 ↗
20. Damage formation mechanisms of sintered silicon carbide during single-diamond grinding10.1016/j.ceramint.2021.06.259 ↗
21. Fundamental understanding of the deformation mechanism and corresponding behavior of RB-SiC ceramics subjected to nano-scratch in ambient temperature10.1016/j.apsusc.2018.11.090 ↗
22. Scratching resistance of SiC-rich nano-coatings produced by noble gas ion mixing10.1016/j.surfcoat.2020.125475 ↗
23. Grain size and scratching depth dependent tribological characteristics of CrCoNi medium-entropy alloy coatings: a molecular dynamics simulation study10.1016/j.surfcoat.2023.129772 ↗
24. A quantitative assessment of nanometric machinability of major polytypes of single crystal silicon carbide10.1016/j.jeurceramsoc.2012.04.016 ↗
25. Molecular dynamics simulation of silicon carbide nanoscale material removal behavior10.1016/j.ceramint.2018.03.195 ↗
26. Action mechanism of hydrogen gas on deposition of HfC coating using HfCl4-CH4-H2-Ar system10.1016/j.apsusc.2016.08.169 ↗
27. XRD and XPS studies on surface MMC layer of SiC reinforced Ti–6Al–4V alloy10.1016/S0924-0136(03)00814-8 ↗
28. Comparison of fracture properties of different amorphous carbon coatings using the scratch test and indentation failure method10.1016/j.surfcoat.2022.128247 ↗
29. Synthesis and characterization of monolithic CVD-SiC tubes10.1016/j.jeurceramsoc.2016.02.024 ↗
30. Progress and challenges towards additive manufacturing of SiC ceramic10.1007/s40145-021-0484-z ↗
31. Study on strain rate and heat effect on the removal mechanism of SiC during nano-scratching process by molecular dynamics simulation10.1016/j.ijmecsci.2018.12.022 ↗
32. Grinding of silicon carbide for optical surface fabrication, part 1: surface analysis10.1364/AO.455863 ↗
33. Experimental and FEM based investigation of the influence of the deposition temperature on the mechanical properties of SiC coatings10.1007/s40145-020-0429-y ↗
34. Crack propagation during Vickers indentation of zirconia ceramics10.1016/j.ceramint.2020.05.225 ↗
35. Vickers indentation fracture toughness of Y-TZP dental ceramics10.1016/j.ijrmhm.2016.12.016 ↗
36. High-temperature strength and toughness behaviors for reaction-bonded SiC ceramics below 1400 °C10.1016/j.matlet.2005.01.049 ↗
37. Brittle materials in nano-abrasive fabrication of optical mirror-surfaces10.1016/j.precisioneng.2007.09.001 ↗
38. Assessing hardness and fracture toughness in sintered zinc oxide ceramics through indentation technique10.1016/j.msea.2015.05.107 ↗
39. Evaluation of mechanical hardness and fracture toughness of co and Al co-doped ZnO10.1016/j.msea.2012.08.028 ↗
40. Vickers indentation fracture (VIF) modeling to analyze multi-cracking toughness of titania, alumina and zirconia plasma sprayed coatings10.1016/j.msea.2009.08.058 ↗
41. Characterization of hardness, elastic modulus and fracture toughness of RB-SiC ceramics at elevated temperature by Vickers test10.1016/j.msea.2018.12.044 ↗
42. Crack extension mechanism and scratch stress field model of hard and brittle materials caused by curvature effect10.1016/j.jmatprotec.2023.118058 ↗
43. Ductile-regime grinding: anew technology for machining Brittle materials10.1115/1.2899676 ↗
44. Critique of materials-based models of ductile machining in brittle solids
45. Anisotropic elastic recovery behavior of AlN ceramic during nanoindentation and scratching10.1016/j.wear.2023.204622 ↗
46. Investigation of AlN ceramic anisotropic deformation behavior during scratching10.1016/j.jeurceramsoc.2022.02.001 ↗
47. Hardness anisotropy and active slip systems in a (Hf-ta-Zr-Nb)C high-entropy carbide during nanoindentation10.1016/j.ijrmhm.2021.105646 ↗