Fabrication of 93W–Ni–Fe alloy large-diameter rods by powder extrusion molding
Source abstract
Abstract
Abstract A powder extrusion molding (PEM) process has been used for the manufacturing of tungsten heavy alloy rods with large length to diameter ratio. An improved wax-based multi-component binder was developed for PEM of 93W–Ni–Fe alloy. The miscibility of its components and the characteristics of the binder were evaluated and good thermal–physical properties were obtained. Also, the feedstock rheological properties, extrusion molding and debinding process were studied. The feedstock exhibited a pseudo-plastic flow behavior. The large length to diameter ratio rods, with diameters up to 36 mm were extruded at 65 °C by optimizing the extrusion process. A two-step debinding process was employed to remove the binder in the extruded rods. Solvent debinding was carried out in n-heptane at 45 °C to extract the soluble components. A process of repeated short time immersion and drying of the extruded rods (called short-period solvent debinding) was developed and using this novel technique the binder removed was raised from 45% to 60%. SEM analyses indicated that a large volume of pores was formed in debound rods, but had not created interpenetrating pore channels yet. The rest of the binder could be thermally extracted at a high heating rate without defects.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Influence of specimen geometry on adiabatic shear instability of tungsten heavy alloys10.1016/S0734-743X(02)00022-2 ↗
2. Behind-armor debris from the impact of hypervelocity tungsten penetrators10.1016/j.ijimpeng.2006.09.007 ↗
3. Deformation and fracture of a long-rod projectile induced by an oblique moving plate: experimental tests10.1016/j.ijimpeng.2011.07.002 ↗
4. Extrusion moulding of hard-metal powder using a novel binder system10.1016/S0924-0136(02)01058-0 ↗
5. Powder extrusion moulding of 430L stainless steel thin tubes for porous metal supported SOFCs10.1179/003258909X12502679013693 ↗
6. Fabrication of 8-YSZ thin-wall tubes by powder extrusion moulding for SOFC electrolytes10.1016/j.ceramint.2009.01.008 ↗
7. Cracking defect and porosity evolution during thermal debinding in ceramic injection moldings10.1016/S0272-8842(98)00061-3 ↗
8. Deformation behavior and strength evolution of MIM compacts during thermal debinding10.1016/S1003-6326(08)60049-7 ↗
9. German · 1997
10. Critical thickness in binder removal process for injection molded compacts10.1016/S0921-5093(03)00613-0 ↗
11. Influence of paraffin wax characteristics on the formulation of wax-based binders and their debinding from green molded parts using two comparative techniques10.1016/j.jmatprotec.2009.07.018 ↗
12. MIM of mechanically alloyed nanoscale W–Ni–Fe powder
13. Fabrication of metal matrix composites by metal injection molding—a review10.1016/j.jmatprotec.2007.10.066 ↗
14. Powder injection molding of WC-8%Co tungsten cemented carbide
15. Development of niobium powder injection molding: part I. Feedstock and injection molding10.1016/j.ijrmhm.2005.06.003 ↗
16. Comparative study of pore structure evolution during solvent and thermal debinding of powder injection molded parts10.1007/BF02648403 ↗
17. Ceramic injection moulding: influence of specimen dimensions and temperature on solvent debinding kinetics10.1016/j.jmatprotec.2004.06.008 ↗
18. Effect of solvent debinding variables on the shape maintenance of green molded bodies10.1023/B:JMSC.0000026942.64551.97 ↗
19. The effects of nanoparticle addition on binder removal from injection molded aluminum nitride10.1016/j.ijrmhm.2012.07.003 ↗
20. Production of alumina parts by powder injection molding with a binder system based on high density polyethylene10.1016/j.jeurceramsoc.2007.08.004 ↗
21. In situ dimensional changes of powder injection-molded compacts during solvent debinding10.1016/S1359-6454(98)00093-7 ↗