Effect of Ti Cr filler on microstructure, mechanical properties, and thermal shock resistance of TZM/graphite brazed joints

Dong-Guang Liu, Jin-Xin Zou, Peng Zhang, Si-Wei Zhou, Hui Liu, Ze-Qun Li

Publisher page

Abstract

The objective of this work was to braze titanium zirconium molybdenum(TZM) alloy and graphite with Ti 40Cr filler in order to explore its practical application on computed tomography tube target. The brazed joints` microstructure, mechanical properties, and thermal shock properties were characterized by X-ray diffraction, scanning electron microscopy, and a 3D laser confocal measuring microscope. The results indicated that the interface microstructure of TZM/graphite brazed joints was graphite/Cr 3C 2 /TiC/Ti-Cr(Mo)/Ti-Mo(Cr)/TZM, and the thickness of the brazing seam increases with increasing temperature. In contrast, the thickness of the carbide reaction layer near the graphite side gradually becomes thicker. The shear tests showed that the joint`s strength increased with the temperature increase in a specific temperature range. Maximum shear strength of 26.5 MPa was reached when the joint with groove structure brazed at 1480 °C. The effect of holding time on the joints was similar to that of temperature, but the thickness of the carbide reaction layer did not change with holding time. The optimal brazing process for TZM/Ti-40Cr/graphite brazed joints was to hold for 20 min at 1480 °C. TZM/Ti-40Cr/graphite brazed joints were subjected to a laser thermal shock test. The results indicated that TZM/Ti-40Cr/ graphite brazed joints would not cause serious damage when subjected to 20A laser beam current. When the current rose to 40A, the joints will be broken down by the laser, and the damage depth reached −254.824 μm.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Special computed tomography imaging features of Thymic cyst[J]
2. Computed tomography imaging of iatrogenic esophageal injuries[J]10.1097/RCT.0000000000001283 ↗
3. Computed tomography imaging in oncology[J]10.1016/j.cvsm.2015.12.007 ↗
4. Direct diffusion bonding of immiscible tungsten and copper at temperature close to copper’s melting point10.1016/j.matdes.2017.10.052 ↗
5. Determination of tungsten target parameters for transmission X-ray tube: a simulation study using geant410.1016/j.net.2016.01.006 ↗
6. Molecular dynamics simulations of high-energy radiation damage in W and WeRe alloys10.1016/j.jnucmat.2019.06.027 ↗
7. Effect of target angle and thickness on the heel effect and X-ray intensity characteristics for 70 kV X-ray tube target10.14316/pmp.2016.27.4.272 ↗
8. A beam optics study of a modular multi-source X-ray tube for novel computed tomography applications10.1016/j.nima.2017.06.035 ↗
9. Phase-contrast THz-CT for non-destructive testing[J]10.1364/OE.422961 ↗
10. High temperature fatigue characteristics of P/M and hot forged W-re and TZM for X-ray target of CT scanner10.1016/j.matdes.2017.10.044 ↗
11. Development of rotating anode targets for CT tubes
12. Microstructure, high temperature strength and CO-gas emission of liquid-phase sintered and forged low oxygen TiCZrC-Mo alloy10.2472/jsms.55.558 ↗
13. Effective joining between oxide dispersion strengthened tungsten-based material (ODS-W) and TZM alloy via spark plasma sintering technology[J]
14. High temperature fatigue characteristics of P/M and hot-forged W-re and TZM forc[J]10.1016/j.matdes.2017.10.044 ↗
15. One-step preparation, microstructure and properties of WRe/TZM gradient material for X-ray tube of CT scanner[J]10.1016/j.jmrt.2021.09.109 ↗
16. Analysis of microstructure and mechanical strength of lap joints of TZM alloy welded by a fiber laser10.1016/j.jmapro.2019.02.015 ↗
17. The upgrade of EAST Divertor[J]10.1007/s10894-014-9765-7 ↗
18. Mechanical property and failure mechanism of 3D Carbon–Carbon braided composites bolted joints under unidirectional tensile loading[J]10.1016/j.matdes.2014.08.073 ↗
19. Friction stir extrusion of aluminum AA6061 into isostatically molded graphite[J]10.1016/j.jmapro.2021.07.052 ↗
20. EAST Full Tungsten Divertor Design[J]10.1007/s10894-015-9951-2 ↗
21. Effect of temperature and layer thickness on these strengths of carbon bonding for carbon/carbon composites[J]10.1016/j.carbon.2004.09.002 ↗
22. The effects of processing variables on strength of carbon bonding between carbon/carbon composites[J]10.1016/j.msea.2009.01.048 ↗
23. Viability study and mechanical characterisation of copperegraphite electrical contacts produced by adhesive joining[J]10.1016/S0924-0136(03)00476-X ↗
24. The preparation and performance of high-temperature adhesives for graphite bonding[J]10.1016/j.ijadhadh.2005.01.006 ↗
25. Microstructure and performance of graphite/TZM alloy joints with different interfacial structures formed by vacuum diffusion bonding [J]10.1016/j.ijrmhm.2020.105287 ↗
26. Techniques and mechanism of superplasticdiffusionbondingbetween Titaniμm alloy and stainless steel [J]
27. Diffusion bonding W and RAFM-steel with an Fe interlayer by hot isostatic pressing [J]10.1016/j.fusengdes.2020.111796 ↗
28. Characterization of alumina–alumina /graphite/monel superalloy brazed joints [J]10.1016/j.ceramint.2011.07.054 ↗
29. Thermal cycling behavior of alumina−graphite brazed joints in electron tube applications [J]10.1016/S1003-6326(14)63239-8 ↗
30. Brazing graphite to aluminum nitride for thermal dissipation purpose[J]10.1002/adem.201600876 ↗
31. Interface evaluation on the brazed system of AlN-Ticusil-graphite[J]10.1111/ijac.13330 ↗
32. Brazed graphite/refractory metal composites for first-wall protection elements[J]10.1016/0022-3115(91)90053-A ↗
33. The effect of the reactive zone in graphite CFC 222 and TZM molybdenum-alloy brazed joints[J]10.1080/09507110701411924 ↗
34. Brazing a graphite composite to molybdenum alloy TZM using active copper-based filler metals with chromium additive[J]10.2478/v10172-011-0092-y ↗
35. Study of the microstructure and thermomechanical properties of Mo/graphite joint brazed with Ti-Zr-Nb-be powder filler metal[J]10.1007/s10853-021-06015-9 ↗
36. Simulated thermal tests of a molybdenμm/graphite X-ray target manufactured with a novel Ti-Zr-Nb-be powder filler metal: an investigation of the brazed joint evolution under operating conditions[J]10.1016/j.jmapro.2021.07.035 ↗
37. Metallurgical and mechanical examinations of molybdenum/graphite joints by vacuum arc pressure brazing using Ti-Zr filler materials[J]10.1016/j.jmatprotec.2017.06.007 ↗
38. TZM/graphite interface behavior in high-temperature brazing by Ti-based brazing filler materials[J]10.1007/s40194-020-00967-3 ↗
39. Interfacial microstructure and joining properties of titanium–zirconium–molybdenum alloy joints brazed using Ti–28Ni eutectic brazing alloy[J]10.1016/j.msea.2015.12.009 ↗
40. Effect of brazing temperature on microstructure and mechanical properties of graphite/copper joints[J]10.1016/j.msea.2013.11.059 ↗
41. Yang Jia, Tao Li, Xiaoguang Chen, Haitao Xue,et al. Agraphite-reinforced AgCuTi/cu foam composite filler to braze Al2O3 ceramic and 304 stainless steel[J]. Ceram. Int. (in press).
42. Brazing of graphite and stainless steel with ag-cu-Ti filler: effects of brazing process parameters on microstructure and mechanical properties[J]
43. Microstructural characterization of graphite/CuCrZr joints brazed with CuTiH2Ni-based fillers[J]10.1016/j.jallcom.2017.05.019 ↗
44. TZM/graphite interface behavior in high-temperature brazing by Ti-based brazing filler materials[J]10.1007/s40194-020-00967-3 ↗
45. Interfacial microstructure and thermal shock resistance of diffusion bonding ODS-W and molybdenum alloy by spark plasma sintering[J]10.1016/j.ijrmhm.2022.105913 ↗
46. Effect of laser beam thermal shock on the helium ion irradiation damage behavior of W-TiC-Y2O3 composites[J]10.1016/j.jnucmat.2018.06.043 ↗
47. Microstructure and transient laser thermal shock behavior of W–TiC–Y2O3 composites prepared by wet chemical method[J]10.1016/j.jallcom.2018.07.046 ↗
48. Evaluating surface damage behavior of W-(Y0.9La0.1)2O3 composites during spark plasma sintering process improvement[J]10.1016/j.jnucmat.2021.153322 ↗
49. Transient thermal shock and helium ion irradiation damage behaviors of ODS-W/CuCrZr joints[J]10.1016/j.matchar.2021.111710 ↗