Abstract
A novel oscillating sinter forging (OSF) was used to prepare ultrafine WC-Co cemented carbides for the first time. The mechanical properties of the resultant samples were characterized and compared with those of cemented carbides prepared by conventional sinter-forging (CSF). The results show that the samples prepared by OSF have higher hardness and fracture toughness. The sample prepared by OSF at 1125 °C has a hardness of 1911 kg/mm 2 and fracture toughness of 17.52 MPa·m 1/2 . These values are much higher than those obtained from the sample prepared by CSF and outperform the general trade-off between hardness and toughness observed in cemented carbides processed by other processes. Microstructural analysis suggests that OSF samples exhibited much better microstructure, such as higher relative density, finer grains, more uniform microstructure, more fcc-structured Co phase, and more ∑2 low-energy grain boundaries. The effects of microstructure on the mechanical properties were discussed. The current study suggests that OSF has excellent synergistic hardening and toughening effects and is a promising technique for preparing high-performance cemented carbides.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Novel WC-Co-Ti3SiC2 cemented carbide with ultrafine WC grains and improved mechanical properties10.1016/j.ceramint.2022.04.239 ↗
2. Low-energy grain boundaries in WC-Co cemented carbides10.1016/j.actamat.2019.06.015 ↗
3. Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide–a review10.1016/j.ijrmhm.2008.07.011 ↗
4. Application of fine grained tungsten carbide based cemented carbides10.1016/0263-4368(95)92672-7 ↗
5. Novel industrial hardmetals for mining, construction and wear applications10.1016/j.ijrmhm.2017.10.021 ↗
6. An experimental study of the sintering of nanocrystalline WC–Co powders10.1016/j.ijrmhm.2005.04.014 ↗
7. Grain growth during the early stage of sintering of nanosized WC-Co powder10.1016/j.ijrmhm.2007.04.006 ↗
8. Study on the mechanical properties, microstructure and corrosion behaviors of nano-WC–Co–Ni–Fe hard materials through HIP and hot-press sintering processes10.1016/j.msea.2014.08.081 ↗
9. Ultrahigh-pressure consolidation and deformation of tantalum carbide at ambient and high temperatures10.1016/j.actamat.2013.03.014 ↗
10. Nanocrystalline cemented tungsten carbide sintered by an ultra-high-pressure rapid hot consolidation process
11. A novel oscillatory pressure-assisted hot pressing for preparation of high-performance ceramics10.1111/jace.12869 ↗
12. Microstructure and mechanical properties of zirconia ceramics consolidated by a novel oscillatory pressure sintering10.1016/j.ceramint.2015.04.026 ↗
13. Enhanced properties of pure alumina ceramics by oscillatory pressure sintering10.1016/j.ceramint.2017.12.133 ↗
14. Oscillatory pressure sintering of high entropy (Zr0.2Ta0.2Nb0.2Hf0.2Mo0.2) B2 ceramic10.1016/j.ceramint.2020.11.108 ↗
15. Oscillating pressure sintering of W-Ni-Fe refractory alloy10.1016/j.jallcom.2019.07.141 ↗
16. Oscillatory pressure sintering: a new method for preparing WC-co cemented carbides10.1016/j.jallcom.2019.152521 ↗
17. Interplay of microstructure and mechanical properties of WC-6Co cemented carbides by hot oscillating pressing method10.1016/j.ceramint.2021.04.063 ↗
18. Densification and grain growth in oscillatory pressure sintering of alumina toughened zirconia ceramic composites10.1016/j.jallcom.2020.155644 ↗
19. Hot oscillatory pressing of B4C ceramics for improving densification and mechanical properties10.1111/jace.18493 ↗
20. Sintering behavior and mechanical properties of alumina ceramics exposed to oscillatory pressure at different sintering stages10.1016/j.ceramint.2021.05.051 ↗
21. Sintering of CdO under low applied stress10.1111/j.1151-2916.1984.tb19665.x ↗
22. Effect of shear stress on sintering10.1111/j.1151-2916.1986.tb04693.x ↗
23. Shear deformation and densification of powder compacts10.1111/j.1151-2916.1986.tb07452.x ↗
24. Enhancement of strength through sinter forging10.1111/j.1151-2916.1987.tb05686.x ↗
25. Transparent MgAl2O4 spinel ceramics prepared via sinter-forging10.1016/j.jeurceramsoc.2021.02.017 ↗
26. Improvement of mechanical properties of zirconia-toughened alumina by sinter forging10.1007/BF00366869 ↗
27. Indentation fracture of WC-co cermets10.1007/BF00555296 ↗
28. Mechanical test discriminability for WC hardmetals10.1016/0263-4368(92)90055-7 ↗
29. Formation mechanisms of microstructure imperfections and their effects on strength in submicron cemented carbide Int10.1016/j.ijrmhm.2013.02.016 ↗
30. Study of the growth kinetics of in situ WC grains in tungsten carbide layers produced by a diffusion-controlled reaction10.1016/j.ceramint.2022.08.131 ↗
31. Oscillatory pressure sintering of WC-Fe-Ni cemented carbides10.1016/j.ceramint.2020.02.040 ↗
32. A new hardness model for materials design in cemented carbides10.1016/j.ijrmhm.2018.04.004 ↗
33. The enhancement of the microstructure and mechanical performances of ultrafine WC-Co cemented carbides by optimizing Cr2(C, N) addition and WC particle sizes10.1016/j.ijrmhm.2021.105518 ↗
34. High-energy ball milling of WC-10Co: effect of the milling medium and speed on the mechanical properties10.1016/j.ijrmhm.2021.105774 ↗
35. Microstructure and properties of ultrafine WC-0.6 VC-10Co hardmetals densified by pressure-assisted critical liquid phase sintering10.1016/j.jallcom.2004.04.070 ↗
36. The effect of NbC on mechanical properties and fracture behavior of WC-10Co cemented carbides10.1016/j.ijrmhm.2014.11.006 ↗
37. Preparation and performance of ultrafine grained WC-10Co alloys with added La2O310.1016/j.ceramint.2018.11.071 ↗
38. Complexions in WC-Co cemented carbides10.1016/j.actamat.2018.02.018 ↗
39. Effects of WC particle size on densification and properties of spark plasma sintered WC-Co cermet10.1016/j.ijrmhm.2009.07.017 ↗
40. Quantitative characterization of the microstructure and properties of nanocrystalline WC-Co bulk10.1016/j.scriptamat.2012.02.029 ↗
41. Phase size distribution in WC/Co10.1016/0026-0800(86)90005-4 ↗
42. Microstructure, hardness and toughness of nanostructured and conventional WC-Co composites10.1016/S0965-9773(98)00123-8 ↗
43. Stress–strain behaviors of cermets with various binder contents and residual thermal stress states10.1016/j.msea.2022.143101 ↗
44. Toughening cemented carbides by phase transformation of zirconia
45. The effects of fine WC contents and temperature on the microstructure and mechanical properties of inhomogeneous WC-(fine WC-Co) cemented carbides10.1016/j.ceramint.2016.08.119 ↗
46. The influence of composition, phase transformation and varying the relative FCC and HCP phase contents on the properties of dilute Co-W-C alloys[J]10.1016/0025-5416(84)90179-4 ↗
47. Residual stress evolution enhanced martensite phase transition and texture development in cryogenic-tempered WC-Co ultra-coarse grained cemented carbide10.1016/j.msea.2022.142592 ↗
48. The role of tungsten in the Co binder: effects on WC grain size and hcp–fcc co in the binder phase10.1016/j.ijrmhm.2014.09.028 ↗
49. Binder phase strengthening of WC–Co alloy through post-sintering treatment10.1016/j.ijrmhm.2014.09.031 ↗
50. EBSD characterization of carbide-carbide boundaries in WC-Co composites10.1111/j.0022-2720.2004.01313.x ↗
51. Microstructure and mechanical properties improvements in cemented carbides by (Cr, Mo, Ta)2 (C, N) inhibitors10.1007/s12598-019-01343-x ↗
52. Co-phase penetration of WC (10−10)/WC (10-10) grain boundaries from first principles10.1103/PhysRevB.67.115415 ↗