Microstructure and mechanical properties of rhenium prepared by electroforming in NaCl-KCl-CsCl-K 2 ReCl 6 molten salts
Source abstract
Abstract
Abstract Rhenium plates of ~ 250 μm thick were prepared by electroforming in NaCl-KCl-CsCl-K2ReCl6 molten salts. The as-deposited rhenium has a near-columnar, fiber-like grain structure and a laminar and twin substructure. The tensile strength and fracture elongation of as-deposited rhenium tested at room temperature were 1040 ± 40 MPa and 8 ± 1.2%, respectively. After annealing at 1000 °C to 1600 °C for 1 h, the grain configuration changed as follows: near-columnar and fiber-like structure → fine equiaxed grain structure → coarse equiaxed grain structure → coarse equiaxed grain mixed with large columnar grain structure. A better combination of strength (744 MPa) and plasticity (18.8%) was obtained by annealing at 1400 °C for 1 h. The grain configuration and substructure, residual stress and oxygen content affect rhenium's mechanical properties with the oxygen content appearing to play a dominant role.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. A rhenium review – from discovery to novel applications,Archives
2. Rhenium a unique rare metal10.1080/10426919408934977 ↗
3. Rhenium and its alloys
4. Properties and applications of rhenium and its alloys
5. Electrodeposition of rhenium and its alloys10.1134/S102319351609010X ↗
6. 2000
7. 1990
8. Induced codeposition of alloys of tungsten, molybdenum and rhenium with transition metals10.1007/978-0-387-49489-0_4 ↗
9. Jones · 2005
10. Pure rhenium metal10.1109/45.481375 ↗
11. Near-net shape powder metallurgy rhenium thruster
12. The effect of manufacturing processes on the mechanical integrity of rhenium
13. Chemical vapor deposition of rhenium on a gourd shaped graphite substrate10.1016/j.surfcoat.2012.05.117 ↗
14. Growth mechanism and mechanical property of laminar iridium coating by electrodeposition10.1016/j.ijrmhm.2015.01.009 ↗
15. Sealing of cracks in the rhenium coating on C/C composites by alloying with cobalt10.1016/j.surfcoat.2014.10.032 ↗
16. Rhenium coating prepared on carbon substrate by chemical vapor deposition10.1016/j.apsusc.2012.08.020 ↗
17. High temperature combustion chambers produced by electroforming
18. NASA in-space advanced chemical propulsion development in recent years
19. Iridium coated rhenium rocket chambers produced by electroforming
20. Properties and enhanced capabilities for EL-Form rhenium
21. Electrodeposition of rhenium from chloride melts-electrochemical nature, structure and applied aspects10.2298/JMMB0302149V ↗
22. Electrodeposition of rhenium onto oriented rhenium foils from salt melts10.1023/A:1013784530337 ↗
23. Epitaxial growth of rhenium on intrinsic and foreign substrates10.1134/S1023193508060086 ↗
24. Electrochemistry of refractory metals in molten salts: application for the creation of new and functional materials10.1351/PAC-CON-08-08-09 ↗
25. Speciation of rhenium in chloride melts: spectroscopic and electrochemical study10.1515/zna-2008-5-618 ↗
26. Kerridge · 2013
27. Black rhenium coating prepared on graphite substrate by electrodeposition in NaCl-KCl-CsCl-K2ReCl6 molten salts10.1016/j.ijrmhm.2017.06.010 ↗
28. Ultrahigh strength and high electrical conductivity in copper10.1126/science.1092905 ↗
29. High temperature rhenium material properties
30. Plastic deformation of platinum metals and rhenium
31. Gottstein · 1999
32. Einfluss von kleinen Beimengungen auf das Rekristallisationsverhalten von Reinstaluminium
33. The effect of variability among grain boundary energies on grain growth in thin film strips10.1557/PROC-317-431 ↗
34. Lucke · 1963 · 171
35. Impurity effects on grain boundary migration10.1088/0965-0393/10/6/201 ↗
36. Structure evolution during processing of polycrystalline films10.1146/annurev.matsci.30.1.159 ↗
37. Mechanisms for microstructure evolution in electroplated copper thin films near room temperature10.1063/1.371086 ↗
38. Recrystallization kinetics of electroplated Cu in damascene trenches at room temperature10.1063/1.368856 ↗
39. Richardson · 1999