journal article·2012-09

High performance tungsten synthesized by microwave sintering method

Y. Zhou, K. Wang, R. Liu, X.P. Wang, C.S. Liu, Q.F. Fang

Publisher page

Abstract

Abstract The W–Ni alloys with varying amount of Ni (0.1, 0.25, 0.5 and 1.0 wt.%) were microwave sintered at 1450 °C for different holding time 5, 15 and 30 min, and their microstructure, grain size, relative density, thermal conductivity, and Vickers microhardness were characterized. Comparing to the addition of Fe and Cr, the Ni addition can greatly improve the relative density and maintain the high thermal conductivity of W at the same time. It was shown that the addition of 1.0 wt.% Ni into W and microwave sintering at 1450 °C for 5 min would be the best conditions to obtain W–Ni alloys with a relative density close to 100% and an average grain size as small as 15 μm. The Vickers microhardness and thermal conductivity of the sintered W–Ni samples range from 370 to 440 and from 90 to 130 W/m K, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. The mechanical and thermophysical properties of ZrC/W composites at elevated temperature10.1016/S0921-5093(01)01802-0 ↗
2. Lassner · 1999
3. Development of chromia forming Mo–W–Cr alloys: synthesis and characterization10.1023/A:1016191202525 ↗
4. Microstructure and mechanical properties of tungsten composites co-strengthened by dispersed TiC and La2O3 particles10.1016/j.ijrmhm.2007.12.004 ↗
5. Explosive consolidation and its application on preparing of ultra-fine grained tungsten plasma facing material
6. Characterization of novel W alloys produced by HIP10.1016/j.jnucmat.2008.12.217 ↗
7. Spark plasma sintering of tungsten–yttrium oxide composites from chemically synthesized nanopowders and microstructural characterization10.1016/j.jnucmat.2011.03.007 ↗
8. Mechanical properties of Y2O3-doped W–Ti alloys10.1016/j.jnucmat.2010.07.016 ↗
9. Levitt AP. US Patent 5440995; 1995.
10. Effect of temperature gradient in the disk during sintering on microstructure and mechanical properties of ZrCp/W composite10.1016/j.ijrmhm.2008.05.005 ↗
11. Improved mechanical properties and microstructural development of microwave sintered copper and nickel steel PM parts10.1179/003258905X37657 ↗
12. Microwave sintering of W–Ni–Fe alloy10.1016/j.scriptamat.2006.09.010 ↗
13. Full sintering of powdered metal bodies in a microwave field10.1038/21390 ↗
14. Ink-jet printing and microwave sintering of conductive silver tracks10.1002/adma.200502422 ↗
15. Microwave sintering: a new approach to fine-grain tungsten-II
16. Microwave sintering: a new approach to fine-grain tungsten-I
17. Microwave sintering of tungsten10.1016/j.ijrmhm.2008.07.001 ↗
18. Microwave heating of pure copper powder with varying particle size and porosity
19. Microwave sintering W–Cu composites: analyses of densification and microstructural homogenization10.1016/j.jallcom.2008.05.038 ↗
20. Microwave sintering of refractory metals: W, Mo, Re, W–Cu, W–Ni–Cu and W–Ni–Fe alloys10.1080/08327823.2010.11689768 ↗
21. Effect of heating mode and sintering temperature on the consolidation of 90W–7Ni–3Fe alloys10.1016/j.jallcom.2010.09.008 ↗
22. Microwave and conventional sintering of 90W–7Ni–3Cu alloys with premixed and pre-alloyed binder phase10.1016/j.msea.2010.07.074 ↗
23. Effect of heating rate on the microwave sintered W–Ni–Fe heavy alloys10.1016/j.jallcom.2009.03.176 ↗
24. Wang K, Wang XP, Liu R, Hao T, Zhang T, Liu CS, et al. The study on the microwave sintering of tungsten at relatively low temperature. J Nucl Mater in press, doi:10.1016/j.jnucmat.2011.11.012.10.1016/j.jnucmat.2011.11.012 ↗
25. Thermomechanical properties of TiC particle-reinforced tungsten composites for high temperature application10.1016/S0263-4368(02)00105-1 ↗
26. Tensile properties at elevated temperature of W–1%La2O310.1016/0921-5093(96)10377-4 ↗
27. Deformation behavior and strengthening mechanisms at intermediate temperatures in W–La2O310.1016/S0921-5093(97)00420-6 ↗
28. Fabrication and properties of mechanically alloyed oxide-dispersed tungsten heavy alloys10.1016/S0921-5093(03)00641-5 ↗
29. The activated sintering of tungsten with group VIII elements10.1149/1.2425876 ↗
30. On the workability of activated sintered tungsten powder compact
31. The effect of the doping method on the sinterability of nickel-doped tungsten compacts10.1016/0022-5088(84)90318-7 ↗
32. High temperature compressive deformation and fracture characteristics of the activated sintered W–Ni compacts10.1016/S0263-4368(03)00031-3 ↗
33. Brophy · 1961 · 113
34. The thermal conductivity of ceramic dielectrics